    Abstract: The method for producing a friction material is characterized by defiberizing 10-45 % kraft pulp and 5-15 % linter pulp in the beater to be 400-500 freeness, adding an coagulating agent to the mixed slurry of the pulps, 5-30 % diatom earth, 1-15 % silica, 1- 15 % zeolite, 10-45 % cashew nut shell oil and 1-10 % cardolite, molding the mixt. under the condition of 30 dg/cm2 surface pressure and 50-60 deg.C temp., blanking it to be a fixed size, and heat-hardening it. The friction material for brakes and clutches has a good porosity and durability.

    Abstract translation: 摩擦材料的制造方法的特征在于,将打浆机中的10-45%牛皮纸浆和5-15%的棉绒纸浆分解为400-500的游离度,向纸浆的混合浆料中加入凝结剂,5-30% 硅藻土,1-15%二氧化硅,1-15%沸石,10-45%腰果壳油和1-10%腰果,成型混合物。 在30dg / cm2的表面压力和50-60℃的温度条件下,将其冲裁成固定尺寸,并加热硬化。 制动器和离合器的摩擦材料具有良好的孔隙率和耐久性。