알루미늄 실리케이트계 형광체 및 이의 제조방법
    1.
    发明公开
    알루미늄 실리케이트계 형광체 및 이의 제조방법 有权
    硅酸铝磷酸盐的新组合物和制备方法

    公开(公告)号:KR1020130090127A

    公开(公告)日:2013-08-13

    申请号:KR1020120011222

    申请日:2012-02-03

    CPC classification number: Y02B20/181

    Abstract: PURPOSE: An aluminum silicate phosphor is provided to be excited by the ultraviolet ray and a wavelength of 250-500 nm which a blue light emitting diode shows, and to show a light emitting wavelength spectrum of 350-800 nm region. CONSTITUTION: An aluminum silicate phosphor is represented by Chemical formula (1): M_xN_(1-x)Al_(2-x)Si_(2+x)O_8:Q_y. Wherein M is any one selected from Li, Na, K, Rb and Cs, N is any one selected from Be, Mg, Ca, Sr and Ba, Q is at least one activator or co-activator selected from europium (Eu), manganese (Mn), iron (Fe), chrome (Cr), calcium (Ca), zinc (Zn), cobalt (Co), nickel (Ni), copper (Cu), yttrium (Y), lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), samarium (Sm), gadolinium (Gd), terbium (Tb), dysprosium (Dy), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), gallium (Ga), germanium (Ge) and indium (In), x is 0

    Abstract translation: 目的:提供由紫外线激发的硅酸铝荧光体,蓝色发光二极管显示的250-500nm的波长,并显示350-800nm区域的发光波长光谱。 构成:铝酸钙荧光体由化学式(1)表示:M_xN_(1-x)Al_(2-x)Si_(2 + x)O_8:Q_y。 其中M为选自Li,Na,K,Rb和Cs中的任一种,N为选自Be,Mg,Ca,Sr和Ba中的任一种,Q为选自铕(Eu), 锰(Mn),铁(Fe),铬(Cr),钙(Ca),锌(Zn),钴(Co),镍(Ni),铜(Cu),钇(Y),镧(La) 铈(镨),镨(Pr),钕(Nd),钐(Sm),钆(Gd),铽(Tb),镝(Dy),铒(Er),ium(Tm),镱(Yb) 镥(Lu),镓(Ga),锗(Ge)和铟(In),x为0

    형광체 및 형광체 제조방법
    2.
    发明公开
    형광체 및 형광체 제조방법 审中-实审
    磷光体及其制备方法

    公开(公告)号:KR1020130063412A

    公开(公告)日:2013-06-14

    申请号:KR1020110129915

    申请日:2011-12-06

    CPC classification number: C09K11/7734 H01L33/502

    Abstract: PURPOSE: An aluminum silicate-based phosphor is excited by UV and blue light emitting diodes, and to have a light-emitting spectrum within 400-800 nm. CONSTITUTION: An aluminum silicate-based phosphor is represented by chemical formula: (M_(1-x)N_x)_4(Si_(1-y)Al_y)_8O_(16±δ):Eu^(2+)_z. In the chemical formula, each of M and N is one or more elements selected from an alkali earth metal group including Li, Na, K, Rb, and Cs; 0

    Abstract translation: 目的:铝硅酸盐系磷光体由紫外和蓝色发光二极管激发,发光光谱范围在400〜800nm之间。 构成:硅酸铝基磷光体由化学式表示:(M_(1-x)N_x)_4(Si_(1-y)Al_y)_8O_(16±δ):Eu ^(2 +)_ z。 在该化学式中,M和N中的一个是选自包括Li,Na,K,Rb和Cs的碱土金属组中的一种或多种元素; 0 <= x <= 1,0,0

    알루미늄 실리케이트계 형광체 및 이의 제조방법
    4.
    发明授权
    알루미늄 실리케이트계 형광체 및 이의 제조방법 有权
    硅酸铝粉末的新组成及其制备方法

    公开(公告)号:KR101405596B1

    公开(公告)日:2014-06-10

    申请号:KR1020120026405

    申请日:2012-03-15

    Abstract: 본 발명은 알루미늄 실리케이트계 형광체 및 이의 제조방법에 관한 것으로서 보다 상세하게는 250∼500nm의 파장에서 여기하고 400∼800nm의 파장에서 발광 특성을 지니며, 하기 화학식(1)로 표시되는 알루미늄 실리케이트계 형광체, 이의 제조방법 및 하기 화학식(1)로 표시되는 알루미늄 실리케이트계 형광체를 포함하는 발광소자에 관한 것이다.
    M
    1+xy Al
    1+x Si
    2-x O
    6 :Q
    y ......화학식(1)
    상기 화학식(1)에서 M은 Li, Na, K, Rb, Cs 중에서 선택된 어느 하나의 알칼리금속이고; Q는 유로피움(Eu), 망간(Mn), 철(Fe), 크롬(Cr), 칼슘(Ca), 아연(Zn), 코발트(Co), 니켈(Ni), 구리(Cu), 이트륨(Y), 란탄(La), 세륨(Ce), 프라세듐(Pr), 네오디뮴(Nd), 사마륨(Sm), 가돌륨(Gd), 터븀(Tb), 디스프로슘(Dy), 어븀(Er), 튤륨(Tm), 이터븀(Yb), 루테튬(Lu), 갈륨(Ga), 게르마늄(Ge), 인듐(In) 중에서 선택된 한 개 이상의 활성제 또는 부활성제이고; x는 0 ≤ x ≤ 1; y는 0

    압력 조절을 통한 양자점 합성방법 및 합성조절방법
    5.
    发明公开
    압력 조절을 통한 양자점 합성방법 및 합성조절방법 有权
    压力控制合成方法及其分析方法

    公开(公告)号:KR1020120137924A

    公开(公告)日:2012-12-24

    申请号:KR1020110057101

    申请日:2011-06-13

    Abstract: PURPOSE: A synthetic method quantum dots and synthesis are provided to control pressure at high temperature without limiting the volume of a reactor, to control the condition of a whole specimen regardless of the volume of a reactor. CONSTITUTION: A synthetic method quantum dots and synthesis comprises: a step of injecting a cation compound, an anion compound, a surfactant and a solvent into a high-pressure reactor, and mixing the materials, and increasing the temperature and pressure of the mixture; a step of temporarily generating nucleus; and a step of growing quantum dots in order. The amount of the cation compound, anion compound and the surfactant are 0.001-10 mmol, 0.001-10 mmol and 0.001-100, respectively. [Reference numerals] (AA) Heating reaction solution; (BB) Suddenly decreasing pressure; (CC) Quantum dot nucleation/growth; (DD) Sudden increase/decrease of pressure; (EE) Completion of quantum dot growth

    Abstract translation: 目的:提供合成方法量子点和合成来控制高温下的压力而不限制反应器的体积,以控制整个样品的状态,而与反应器的体积无关。 构成:合成方法量子点和合成包括:将阳离子化合物,阴离子化合物,表面活性剂和溶剂注入高压反应器中,并混合该材料并提高混合物的温度和压力的步骤; 暂时产生核的一个步骤; 以及顺序生长量子点的步骤。 阳离子化合物,阴离子化合物和表面活性剂的量分别为0.001-10mmol,0.001-10mmol和0.001-100。 (标号)(AA)加热反应溶液; (BB)突然减压; (CC)量子点成核/生长; (DD)压力突然增加/减少; (EE)完成量子点增长

    알루미늄 실리케이트계 형광체 및 이의 제조방법
    6.
    发明公开
    알루미늄 실리케이트계 형광체 및 이의 제조방법 有权
    硅酸铝磷酸盐的新组合物及其制备方法

    公开(公告)号:KR1020130104688A

    公开(公告)日:2013-09-25

    申请号:KR1020120026405

    申请日:2012-03-15

    Abstract: PURPOSE: An aluminum silicate-based phosphor is provided to be excited by the wavelength of 250-500 nm which ultraviolet ray and blue light emitting diode show, and to have the emission spectrum of 400-800 nm. CONSTITUTION: An aluminum silicate-based phosphor is represented by the following chemical formula (1): M1+x-yAl1+xSi2-xO6:Qy In the above chemical formula (1), M is one of alkali metal selected from Li, Na, K, Rb, and Cs, and Q is one or more activators or co-activators selected from europium (Eu), manganese (Mn), iron (Fe), chrome (Cr), calcium (Ca), zinc (Zn), cobalt (Co), nickel (Ni), copper (Cu), yttrium (Y), lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), samarium (Sm), gadolinium (Gd), terbium (Tb), dysprosium (Dy), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), gallium (Ga), germanium (Ge), and indium (In). X is 0

    Abstract translation: 目的:提供紫外线和蓝色发光二极管显示的250-500nm波长激发的硅酸铝基荧光体,并具有400-800nm的发射光谱。 构成:铝硅酸盐系荧光体由以下化学式(1)表示:M1 + x-yAl1 + xSi2-xO6:Qy在上述化学式(1)中,M是选自Li,Na ,K,Rb和Cs,Q是一种或多种选自铕(Eu),锰(Mn),铁(Fe),铬(Cr),钙(Ca),锌(Zn) ,钴(Co),镍(Ni),铜(Cu),钇(Y),镧(La),铈(Ce),镨(Pr),钕(Nd),钐(Sm),钆(Gd) ,铽(Tb),镝(Dy),铒(Er),ium(Tm),镱(Yb),镥(Lu),镓(Ga),锗(Ge)和铟(In)。 X为0 <= x <=,Y为0

    알루미늄 실리케이트계 형광체 및 이의 제조방법
    9.
    发明授权
    알루미늄 실리케이트계 형광체 및 이의 제조방법 有权
    新型硅酸铝粉组合物及其制备方法

    公开(公告)号:KR101356098B1

    公开(公告)日:2014-01-29

    申请号:KR1020120011222

    申请日:2012-02-03

    CPC classification number: Y02B20/181

    Abstract: 본 발명은 알루미늄 실리케이트계 형광체 및 이의 제조방법에 관한 것으로서 보다 상세하게는 250∼500nm의 파장에서 여기하고 350∼800nm의 파장에서 발광 특성을 지니며, 하기 화학식(1)로 표시되는 알루미늄 실리케이트계 형광체, 이의 제조방법 및 상기의 알루미늄 실리케이트계 형광체를 포함하는 발광소자에 관한 것이다.
    M
    x N
    1-xy Al
    2-x Si
    2+x O
    8 :Q
    y ......화학식(1)
    상기 화학식(1)에서 M은 Li, Na, K, Rb, Cs 중에서 선택된 어느 하나의 알칼리금속이고, N은 Be, Mg, Ca, Sr, Ba 중에서 선택된 어느 하나의 알칼리토금속이고, Q는 유로피움(Eu), 망간(Mn), 철(Fe), 크롬(Cr), 코발트(Co), 니켈(Ni), 구리(Cu), 이트륨(Y), 란탄(La), 세륨(Ce), 프라세듐(Pr), 네오디뮴(Nd), 사마륨(Sm), 가돌륨(Gd), 터븀(Tb), 디스프로슘(Dy), 어븀(Er), 튤륨(Tm), 이터븀(Yb) 및 루테튬(Lu) 중에서 선택된 한 개 이상의 활성제 또는 부활성제이고, x는 0

Patent Agency Ranking