술포닐아민이미드-함유 양이온 중합개시제 및 이를 함유한 양이온 중합조성물
    1.
    发明公开
    술포닐아민이미드-함유 양이온 중합개시제 및 이를 함유한 양이온 중합조성물 失效
    含有磺酰胺酰胺的阳离子聚合引发剂和含有它的阳离子聚合组合物

    公开(公告)号:KR1020010016765A

    公开(公告)日:2001-03-05

    申请号:KR1019990031853

    申请日:1999-08-03

    Abstract: PURPOSE: Provided are cationic polymerization initiator containing sulfonyl amine amide, which dose not have ion structure of salt in molecular structure thereof, and a cationic polymerization composition containing the same, which can increase selectivity of oligomer synthesis. CONSTITUTION: The cationic polymerization initiator containing the sulfonyl amine amide is represented by the formula 1. And the cation polymerization composition contains 0.1-10 mol%(based on cation polymerization organic material) of the cation polymerization initiator(formula 1) containing the sulfonyl amine amide. In the formula, R1 is C1-C4 alkyl, substituted or unsubstituted phenyl, wherein phenyl is substituted by 1-4 substituent selected from the group consisting of C1-C4 alkyl, C1-C4 alkoxy, halogen atom, R2 is C1-C5 alkyl, allyl, substituted or unsubstituted benzyl, wherein the benzyl is substituted by 1-5 substituent selected from the group consisting of C1-C5 alkyl, C1-C5 alkoxy, nitro, and halogen atom.

    Abstract translation: 目的:提供含有磺酰胺酰胺的阳离子聚合引发剂,其不具有其分子结构中的盐的离子结构,以及含有该磺酰胺酰胺的阳离子聚合引发剂,其可提高低聚物合成的选择性。 构成:含有磺酰胺酰胺的阳离子聚合引发剂由式1表示。阳离子聚合组合物含有含有磺酰胺的阳离子聚合引发剂(式1)的0.1-10摩尔%(基于阳离子聚合有机材料) 酰胺。 在该式中,R 1是C 1 -C 4烷基,取代或未取代的苯基,其中苯基被选自C1-C4烷基,C1-C4烷氧基,卤素原子的1-4个取代基取代,R2是C1-C5烷基 ,烯丙基,取代或未取代的苄基,其中苄基被1-5个选自C1-C5烷基,C1-C5烷氧基,硝基和卤素原子的取代基取代。

    탄화수소 제조용 철 혼성촉매
    2.
    发明授权
    탄화수소 제조용 철 혼성촉매 失效
    用于制备碳氢化合物的铁催化剂

    公开(公告)号:KR100224472B1

    公开(公告)日:1999-10-15

    申请号:KR1019970031733

    申请日:1997-07-09

    Abstract: 본 발명은 철 혼성촉매를 이용한 탄화수소의 제조방법에 관한 것으로서, 더욱 상세하게는 담지체 없이 주촉매로서 철(Fe)과, 조촉매로서 아연(Zn), 바나듐(V), 크롬(Cr) 및 망간(Mn) 중에서 선택된 1종 이상이 특정 조성비로 공침되어 있는 철 혼성촉매를 이산화탄소의 수소화 반응에 의한 탄화수소의 제조공정에서 촉매로 사용하여 이산화탄소의 전환율과 C
    2+ 탄화수소의 선택도를 향상시키게 되는 철 혼성촉매를 이용한 탄화수소의 제조방법에 관한 것이다.

    페놀함유 폐수처리제
    5.
    发明授权
    페놀함유 폐수처리제 失效
    用于处理包括废水的酚醛的试剂

    公开(公告)号:KR100146502B1

    公开(公告)日:1998-08-17

    申请号:KR1019950023625

    申请日:1995-08-01

    Abstract: 본 발명은 페놀함유 폐수처리제에 관한 것으로서, 더욱 상세하게는 페놀의 분해반응에서 강력한 활성을 나타내는 철(iron) 등의 금속을 무기담체 또는 고분자담체에 담지시켜 폐수중에 함유된 페놀 및 페놀유도체를 효과적으로 처리할 수 있는 폐수처리제에 관한 것이다.

    열중합용 양이온 중합성 조성물, 중합촉매 및 중합방법
    6.
    发明授权
    열중합용 양이온 중합성 조성물, 중합촉매 및 중합방법 失效
    热聚合阳离子单体的组成,催化剂和聚合方法

    公开(公告)号:KR100131137B1

    公开(公告)日:1998-04-13

    申请号:KR1019940000310

    申请日:1994-01-10

    Abstract: The cation polymeric composition is prepared by containing more than 1 or 2 materials of cation polymerization initiator, a positive ion polymeric material combined and selected from more than 1 or 2 species of compound among a group of structural formulas(1), (2) and (3) and positive ion polymerization initiator for the thermal polymerization. In the formula, R is hydrogen atom, alkyl or alkoxy group and X is antimony hexafluoride, arsenic hexafluoride, phosphorous hexafluoride and boron tetrafluoride.

    Abstract translation: 阳离子聚合物组合物通过含有多于1种或2种阳离子聚合引发剂的材料来制备,阳离子聚合引发剂,结合式(1),(2)和 (3)和用于热聚合的正离子聚合引发剂。 式中,R为氢原子,烷基或烷氧基,X为六氟化锑,六氟化砷,六氟化磷,四氟化硼。

    이산화탄소로 부터 합성가스의 제조방법
    8.
    发明授权
    이산화탄소로 부터 합성가스의 제조방법 失效
    二氧化碳合成气的制备工艺

    公开(公告)号:KR1019960009892B1

    公开(公告)日:1996-07-24

    申请号:KR1019930016885

    申请日:1993-08-25

    CPC classification number: B01J23/78 C01B3/40 C01B2203/1052 Y02P20/52

    Abstract: Synthetic gas is prepared by continuously reacting carbon dioxide with low grade hydrocarbon or natural gas containing methane and oxygen or steam in a mole ratio of 2:1-5:1 in the presence of a catalyst that comprises nickel, alkali and alkali earth metals supported on silicone such as zeolite, silica, silicate or silica-alumina at 600-1,000deg.C and 0.5-20 atms and a space velocity of 1,000-500,000. The ratio of carbon monoxide to hydrogen in the synthetic gas is 1:2-2:1.

    Abstract translation: 在催化剂存在下,使二氧化碳与含有甲烷和氧气或蒸汽的摩尔比为2:1-5:1的低级烃或天然气连续反应制备合成气体,所述催化剂包含负载的镍,碱和碱土金属 在600-1000℃,0.5-20atms,空间速度为1000-500,000的硅氧烷如沸石,二氧化硅,硅酸盐或二氧化硅 - 氧化铝上。 合成气中一氧化碳与氢的比例为1:2.2:1。

    폐수처리용 불균일 촉매 및 그 제조방법
    9.
    发明公开
    폐수처리용 불균일 촉매 및 그 제조방법 失效
    用于废水处理的非均相催化剂及其生产方法

    公开(公告)号:KR1019960003789A

    公开(公告)日:1996-02-23

    申请号:KR1019940016445

    申请日:1994-07-08

    Abstract: 본 발명은 폐수중에 함유된 H
    2 S가스 및 암모니아 가스 산화용 불균일 고체 촉매를 제공한다. 본 발명의 고체 촉매는 비닐피리딘 고분자 100중량%에 대하여 철염 또는 철염 착물 1-20중량%를 지지시켜 제조한다. 철염은 바람직하게는 FeCl
    2 이며 철염착물로는 Na
    2 EDTA가 바람직하다. 본 발명의 촉매는 폐수중의 악취가스 특히 H
    2 S가스 및 NH
    3 가스를 제거하는데 매우 유용하다.

    열중합용 양이온 중합성 조성물, 중합촉매 및 중합방법
    10.
    发明公开
    열중합용 양이온 중합성 조성물, 중합촉매 및 중합방법 失效
    用于热聚合的阳离子聚合性组合物,聚合催化剂和聚合方法

    公开(公告)号:KR1019950023660A

    公开(公告)日:1995-08-18

    申请号:KR1019940000310

    申请日:1994-01-10

    Abstract: 본 발명은, 양이온 중합성 물질을 열에 의해 단시간에 중합시켜 양호한 물성을 갖는 경화물이나 실용성 있는 양이온 중합성 화합물의 올리고머를 얻기 위한 중합조성물과 이를 중합하기 위한 중합촉매 및 중합방법에 관한 것으로서, 다음의 일반식(Ⅰ), (Ⅱ), (Ⅲ)으로 나타내어지는 화합물의 1종 또는 2종 이상 조합되어 선택되어지는 양이온 중합개시제 및 양이온 중합성 물질의 하나 또는 둘 이상과, 상기의 양이온 중합개시제를 포함하는 중합조성물임.

    (여기에 있어서, R은 수소원자, 알킬기 X=SbF
    6 , AsF
    6 , PF
    6 , BF
    4 또는 알콕시기이다.)

Patent Agency Ranking