Abstract:
A radiation tuned optical fiber comprises an optical fiber that includes a substantially circular core and a cladding containing an asymmetric stress zone. The substantially circular core has an initial birefringence. A length of the optical fiber has at least one radiation-tuned portion wherein the substantially circular core has a tuned birefringence to provide the radiation tuned optical fiber in which the tuned birefringence differs from the initial birefringence.
Abstract:
An optical article including a core; at least one cladding layer; and a narrow fluorine reservoir between the core and the cladding layer. The fluorine reservoir has a higher concentration of fluorine than either the cladding layer or the core. One particular embodiment includes a core including a halide-doped silicate glass that comprises approximately the following in cation-plus-halide mole percent 0.25-5 mol% Al2O3, 0.05-1.5 mol% La2O3, 0.0005-0.75 mol% Er2O3, 0.5-6 mol% F, 0-1 mol% Cl.
Abstract:
An optical article including a core; at least one cladding layer; and a narrow fluorine reservoir between the core and the cladding layer. The fluorine reservoir has a higher concentration of fluorine than either the cladding layer or the core. One particular embodiment includes a core including a halide-doped silicate glass that comprises approximately the following in cation-plus-halide mole percent 0.25-5 mol% Al2O3, 0.05-1.5 mol% La2O3, 0.0005-0.75 mol% Er2O3, 0.5-6 mol% F, 0-1 mol% Cl.
Abstract translation:一种包括芯的光学物品; 至少一个包覆层; 以及纤芯和包层之间的窄氟储层。 氟储层的氟浓度高于包层或核心。 一个具体的实施方式包括包含掺杂卤化物的硅酸盐玻璃的核心,所述玻璃在阳离子加卤化物中包含约0.25-5摩尔%的Al 2 O 3,0.05-1.5摩尔%的La 2 O 3,0.0005-0.75摩尔%的Er 2 O 3,0.5-6 摩尔%F,0-1摩尔%Cl。
Abstract:
A fusion splice including a first optical fiber having a first MFD and a first MFD expansion rate. The splice further includes a second fiber (100) having a second MFD and a second MFD expansion rate, wherein the second MFD is lower than the first MFD. The second fiber comprises a core (110), a cladding (130) radially surrounding the core, and a zone (120) of high-concentration of fluorine between the core and the cladding. The rate of MFD expansion of the first fiber is less than the rate of MFD expansion of the second fiber during the fusion splicing operation.