Abstract:
A patch for a device in an electronic housing including an aluminum layer having a threshold thickness, a non-conductive layer on a first side of the aluminum layer, and a radio-frequency (RF) transparent layer on a second side of the aluminum layer is provided. A method for manufacturing an antenna window including a patch as above is also provided, the method including determining a thickness of the aluminum layer adjacent to an anodized aluminum layer. A method for manufacturing an antenna window including coating an aluminum layer having a threshold thickness on a radio-frequency (RF) transparent layer to form an RF transparent laminate is also provided. A method for manufacturing an antenna window including removing a thickness of aluminum is also provided. A method for manufacturing an antenna window including disposing a mask on an aluminum substrate and anodizing the aluminum substrate to a selected thickness is also provided.
Abstract:
The disclosure is directed to treated titanium alloys comprising a titanium substrate coated with an oxidized surface coating or an oxide-interdiffused titanium substrate. By creating an oxidized surface coating or oxide-interdiffused titanium substrate at the titanium substrate surface, the resulting treated titanium alloy has a dark color (e.g., grey to black).
Abstract:
The embodiments described herein relate to anodic films and methods for forming anodic films. The methods described can be used to form anodic films that have a white appearance. Methods involve positioning reflective particles on or within a substrate prior to or during an anodizing process. The reflective particles are positioned within the metal oxide of the resultant anodic film but substantially outside the pores of the anodic film. The reflective particles scatter incident light giving the resultant anodic film a white appearance.
Abstract:
An electronic device may include conductive structures with a light-reflecting coating. The coating may have a two or four-layer thin-film interference filter. The two-layer filter may have a CrN layer and an SiCrN layer. The four-layer filter may have two CrN layers and two SiCrN layers. The two-layer filter may be used to coat relatively small conductive components. The four-layer filter may be used to coat a conductive housing sidewall. Both types of interference filter may produce a relatively uniform light blue color despite variations in coating thickness produced on account of the geometry of the underlying conductive structure.
Abstract:
An electronic device such as a wristwatch may include a conductive housing. A corrosion-resistant coating may be deposited on the conductive housing. The coating may include transition layers and an uppermost alloy layer. The transition layers may include a chromium seed layer on the conductive housing and a chromium nitride layer on the chromium seed layer. The uppermost alloy layer may include TiCrCN or other alloys and may provide the coating with desired optical reflection and absorption characteristics. The transition layers may include a minimal number of coating defects, thereby eliminating potential sites at which visible defects could form when exposed to salt water. This may allow the electronic device to exhibit a desired color and to be submerged in salt water without producing undesirable visible defects on the conductive housing structures.
Abstract:
A patch for a device in an electronic housing including an aluminum layer having a threshold thickness, a non-conductive layer on a first side of the aluminum layer, and a radio-frequency (RF) transparent layer on a second side of the aluminum layer is provided. A method for manufacturing an antenna window including a patch as above is also provided, the method including determining a thickness of the aluminum layer adjacent to an anodized aluminum layer. A method for manufacturing an antenna window including coating an aluminum layer having a threshold thickness on a radio-frequency (RF) transparent layer to form an RF transparent laminate is also provided. A method for manufacturing an antenna window including removing a thickness of aluminum is also provided. A method for manufacturing an antenna window including disposing a mask on an aluminum substrate and anodizing the aluminum substrate to a selected thickness is also provided.
Abstract:
An electronic device may include conductive structures having a visible-light-reflecting coating. The coating may include a seed layer, transition layers, a neutral-color base layer, and an uppermost layer that forms a single-layer interference film. The neutral-color base layer may be opaque to visible light. The interference film may include silicon and may have an absorption coefficient between 0 and 1. The interference film may include, for example, CrSiCN or CrSiC. The composition of the interference film, the thickness of the interference film, and/or the composition of the base layer may be selected to provide the coating with a desired color in the visible spectrum (e.g., at blue or purple wavelengths). The color may be relatively stable even if the thickness of the coating varies across its area.
Abstract:
An electronic device may include conductive structures having a visible-light-reflecting coating. The coating may include a seed layer, transition layers, a neutral-color base layer, and an uppermost layer that forms a single-layer interference film. The neutral-color base layer may be opaque to visible light. The interference film may include silicon and may have an absorption coefficient between 0 and 1. The interference film may include, for example, CrSiN or CrSiCN. The composition of the interference film, the thickness of the interference film, and/or the composition of the base layer may be selected to provide the coating with a desired color near the middle of the visible spectrum (e.g., at green wavelengths). The color may be relatively stable even if the thickness of the coating varies across its area.
Abstract:
An electronic device such as a wristwatch may include a conductive housing. A corrosion-resistant coating may be deposited on the conductive housing. The coating may include transition layers and an uppermost alloy layer. The transition layers may include a chromium seed layer on the conductive housing and a chromium nitride layer on the chromium seed layer. The uppermost alloy layer may include TiCrCN or other alloys and may provide the coating with desired optical reflection and absorption characteristics. The transition layers may include a minimal number of coating defects, thereby eliminating potential sites at which visible defects could form when exposed to salt water. This may allow the electronic device to exhibit a desired color and to be submerged in salt water without producing undesirable visible defects on the conductive housing structures.