PROCESS FOR THE PREPARATION OF POROUS PROPYLENE POLYMERS
    3.
    发明申请
    PROCESS FOR THE PREPARATION OF POROUS PROPYLENE POLYMERS 审中-公开
    制备多孔丙烯聚合物的方法

    公开(公告)号:WO2015059117A1

    公开(公告)日:2015-04-30

    申请号:PCT/EP2014/072501

    申请日:2014-10-21

    Abstract: Process for the preparation of a porous propylene carried out in the presence of a catalyst system comprising (a) a Ziegler-Natta catalyst containing at least two electron donor compounds one of which being present in an amount from 50 to 90% by mol with respect to the total amount of donors and selected from succinates and the other being selected from 1,3 diethers, (b) an aluminum alkyl and comprising the following steps: i) contacting the catalyst components (a) and (b) for a period of time ranging from 1 to 60 minutes, at a temperature ranging from 35 to 55°C; optionally, ii) pre-polymerizing with one or more olefins of formula CH 2 =CHR, where R is H or a C 1 -C 10 hydrocarbon group, up to forming amounts of polymer from about 0.1 up to about 1000 g per gram of solid catalyst component (a); and iii) polymerizing propylene in the optional presence of minor amounts of ethylene and/or C 4 -C 10 alpha olefins producing said porous propylene (co)polymer.

    Abstract translation: 在催化剂体系存在下进行的多孔丙烯的制备方法,该催化剂体系包含(a)含有至少两种电子给体化合物的齐格勒 - 纳塔催化剂,其中一种催化剂体系以50至90摩尔%的量存在, 相对于供体的总量,选自琥珀酸盐,另一种选自1,3-二醚,(b)烷基铝,包括以下步骤:i)使催化剂组分(a)和(b)接触一段时间 时间为1至60分钟,温度范围为35至55℃; 任选地,ii)使用一种或多种式CH 2 = CHR的烯烃进行预聚合,其中R是H或C1-C10烃基,直至每克固体催化剂组分约0.1至约1000g的聚合物的形成量 (一个); 和iii)在少量乙烯和/或C 4 -C 10α-烯烃的任选存在下聚合丙烯,生产所述多孔丙烯(共)聚合物。

    PROCESS FOR THE PREPARATION OF POROUS PROPYLENE POLYMERS
    6.
    发明公开
    PROCESS FOR THE PREPARATION OF POROUS PROPYLENE POLYMERS 有权
    VERFAHREN ZUR HERSTELLEN VONPORÖSENPROPYLENPOLYMEREN

    公开(公告)号:EP3060588A1

    公开(公告)日:2016-08-31

    申请号:EP14786901.0

    申请日:2014-10-21

    Abstract: Process for the preparation of a porous propylene carried out in the presence of a catalyst system comprising (a) a Ziegler-Natta catalyst containing at least two electron donor compounds one of which being present in an amount from 50 to 90% by mol with respect to the total amount of donors and selected from succinates and the other being selected from 1,3 diethers, (b) an aluminum alkyl and comprising the following steps: i) contacting the catalyst components (a) and (b) for a period of time ranging from 1 to 60 minutes, at a temperature ranging from 35 to 55°C; optionally, ii) pre-polymerizing with one or more olefins of formula CH2=CHR, where R is H or a C1-C10 hydrocarbon group, up to forming amounts of polymer from about 0.1 up to about 1000 g per gram of solid catalyst component (a); and iii) polymerizing propylene in the optional presence of minor amounts of ethylene and/or C4-C10 alpha olefins producing said porous propylene (co)polymer.

    Abstract translation: 在催化剂体系存在下进行的多孔丙烯的制备方法,包括(a)含有至少两种电子给体化合物的齐格勒 - 纳塔催化剂,其中一种以50-90% 相对于供体的总量,选自琥珀酸盐,另一种选自1,3-二醚,(b)烷基铝,包括以下步骤:i)使催化剂组分(a)和(b)接触一段时间 时间为1至60分钟,温度范围为35至55℃; 任选地,ii)使用一种或多种式CH 2 = CHR的烯烃进行预聚合,其中R是H或C1-C10烃基,直到每克固体催化剂组分约0.1至约1000g的聚合物的形成量 (一个); 和iii)在少量乙烯和/或C 4 -C 10α-烯烃的任选存在下聚合丙烯,生产所述多孔丙烯(共)聚合物。