公开(公告)号:CA2479994A1
公开(公告)日:2004-04-01
申请号:CA2479994
申请日:2003-08-28
Applicant: BASELL POLIOLEFINE SPA
Inventor: GOBERTI PAOLO , ZUCCHELLI UGO , CREDALI UMBERTO
Abstract: Polyolefin compositions filled with high amounts of inorganic fillers comprising, by weight: (I) 20 to 60% by weight of an heterophasic polyolefin composition comprising: A) from 8 to 25% by weight of a crystalline polymer fraction selected from propylene homopolymer, propylene copolymers and mixtu re there; and B) from 75 to 92% by weight of an elastomeric fraction comprising at least an elastomeric copolymer of propylene or ethylene with 15 to 45% of at least one alpha-olefin, having solubility in xylene at room temperature greater than 50% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from 3.0 to 6.5 dl/g; and (II) 40 to 80% by weight of an inorganic filler selected from flame-retardant inorganic fillers and inorgan ic oxides or salts.
-
公开(公告)号:AU2003207898A1
公开(公告)日:2003-09-22
申请号:AU2003207898
申请日:2003-03-06
Applicant: BASELL POLIOLEFINE SPA
Inventor: BUTALA ROBERT G , HAN CHOONG Y , ENNIS GERALD JOHN , GOBERTI PAOLO , GLOGOVSKY TODD
Abstract: A polyolefin composition suitable for preparing single ply roofing membranes, comprising: (A) from about 15 to about 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H2C=CHR , where R is H or a C2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity of the xylene soluble fraction being higher than about 3.0 dl/g up to about 6.0 dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H2C=CHR , where R is a C2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0 dl/g; the (1)/(2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least three stages, has tensile strength at break >=25 MPa, elongation at break >=700 MPa and toughness >=150 MPa.
-
公开(公告)号:DE60017842T2
公开(公告)日:2006-01-12
申请号:DE60017842
申请日:2000-03-13
Applicant: BASELL POLIOLEFINE SPA
Inventor: RIGOSI LUIGI , GOBERTI PAOLO
Abstract: A process for effecting a coupling between a plastic material and a metal surface comprising the steps of applying a powder of an adhesive polymer composition to the metal surface; then overmoulding the metal surface with a plastic material by injection moulding; and finally applying heat to the metal surface.
-
4.
公开(公告)号:AR041267A1
公开(公告)日:2005-05-11
申请号:ARP030103346
申请日:2003-09-16
Applicant: BASELL POLIOLEFINE SPA
Inventor: GOBERTI PAOLO , CREDALI UMBERTO , ZUCCHELLI UGO
-
公开(公告)号:ES2235850T3
公开(公告)日:2005-07-16
申请号:ES00918792
申请日:2000-03-13
Applicant: BASELL POLIOLEFINE SPA
Inventor: RIGOSI GIAN LUIGI , GOBERTI PAOLO
Abstract: Un procedimiento para efectuar un acoplamiento entre un material plástico y una superficie metálica que comprende las etapas de: a) aplicar un polvo de una composición polimérica adhesiva a la superficie de metal; b) sobremoldear la superficie de metal con material plástico mediante moldeo por inyección; y c) aplicar calor a la superficie de metal.
-
公开(公告)号:DE60017842D1
公开(公告)日:2005-03-10
申请号:DE60017842
申请日:2000-03-13
Applicant: BASELL POLIOLEFINE SPA
Inventor: RIGOSI LUIGI , GOBERTI PAOLO
Abstract: A process for effecting a coupling between a plastic material and a metal surface comprising the steps of applying a powder of an adhesive polymer composition to the metal surface; then overmoulding the metal surface with a plastic material by injection moulding; and finally applying heat to the metal surface.
-
公开(公告)号:AT288457T
公开(公告)日:2005-02-15
申请号:AT00918792
申请日:2000-03-13
Applicant: BASELL POLIOLEFINE SPA
Inventor: RIGOSI GIAN LUIGI , GOBERTI PAOLO
Abstract: A process for effecting a coupling between a plastic material and a metal surface comprising the steps of applying a powder of an adhesive polymer composition to the metal surface; then overmoulding the metal surface with a plastic material by injection moulding; and finally applying heat to the metal surface.
-
公开(公告)号:CA2448581A1
公开(公告)日:2003-09-18
申请号:CA2448581
申请日:2003-03-06
Applicant: BASELL POLIOLEFINE SPA
Inventor: BUTALA ROBERT G , ENNIS GERALD JOHN , GOBERTI PAOLO , HAN CHOONG Y , GLOGOVSKY TODD
Abstract: A polyolefin composition suitable for preparing single ply roofing membranes , comprising: (A) from about 15 to 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H2C=CHR1, where R1 is H or a C2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity o f the xylene soluble fraction being higher than about 3.0dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H2C=CHR2, where R2 is a C2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0dl/g; the (1) (2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least thre e stages, has tensile strength at break >= 25 Mpa, elongation at break > = 700 Mpa and toughness >= 150 Mpa.
-
公开(公告)号:CA2448581C
公开(公告)日:2008-07-08
申请号:CA2448581
申请日:2003-03-06
Applicant: BASELL POLIOLEFINE SPA
Inventor: ENNIS GERALD JOHN , GOBERTI PAOLO , GLOGOVSKY TODD , HAN CHOONG Y , BUTALA ROBERT G
Abstract: A polyolefin composition suitable for preparing single ply roofing membranes, comprising: (A) from about 15 to 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H2C=CHR1, where R1 is H or a C2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity of the xylene soluble fraction being higher than about 3.0dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H2C=CHR2, where R2 is a C2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0dl/g; the (1) (2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least three stages, has tensile strength at break >= 25 Mpa, elongation at break >= 700 Mpa and toughness >= 150 Mpa.
-
公开(公告)号:BR0303374A
公开(公告)日:2004-12-28
申请号:BR0303374
申请日:2003-03-06
Applicant: BASELL POLIOLEFINE SPA
Inventor: GLOGOVSKY TODD , BUTALA ROBERT G , HAN CHOONG Y , ENNIS GERALD JOHN , GOBERTI PAOLO
Abstract: A polyolefin composition suitable for preparing single ply roofing membranes, comprising: (A) from about 15 to about 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H2C=CHR , where R is H or a C2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity of the xylene soluble fraction being higher than about 3.0 dl/g up to about 6.0 dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H2C=CHR , where R is a C2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0 dl/g; the (1)/(2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least three stages, has tensile strength at break >=25 MPa, elongation at break >=700 MPa and toughness >=150 MPa.
-
-
-
-
-
-
-
-
-