公开(公告)号:JPH02229810A
公开(公告)日:1990-09-12
申请号:JP33674689
申请日:1989-12-27
Applicant: BASF AG
Inventor: REHMER GERD , BOETTCHER ANDREAS , AUCHTER GERHARD
IPC: C08F212/08 , C08F2/46 , C08F20/10 , C08F20/26 , C08F20/52 , C08F212/00 , C08F220/18 , C08F220/30 , C08F220/58 , C08F290/00 , C08F290/06 , C08F299/00 , C09D4/00 , C09D133/04 , C09J4/00 , C09J133/04
-
公开(公告)号:AT366759T
公开(公告)日:2007-08-15
申请号:AT03755108
申请日:2003-05-21
Applicant: BASF AG
Inventor: WULFF DIRK , FELDTHUSEN JENSEN JESPER , AUCHTER GERHARD , WILDBURG GERALD , FINK RALF
IPC: C08F285/00 , C08F2/22 , C08F257/02 , C08F265/04 , C08F291/00 , C08L51/00 , C09J151/00
Abstract: The invention relates to a method for producing an aqueous polymer dispersion having a polymer solids content of >=50% by weight by carrying out the radically initiated aqueous emulsion polymerization of ethylenically unsaturated compounds (monomers). The inventive method is characterized in that: a) a mixture is provided in a polymerization vessel and contains a partial quantity 1 consisting of: deionized water, 0.001 to 0.5 parts by weight of a polymer with a weighted average particle diameter of =80% [polymerization step A], and; b) afterwards, a monomer emulsion containing partial quantity 2, which consists of deionized water, 0.1 to 5 parts by weight of dispersants and 90 to 99.5 parts by weight of monomers, is fed under polymerization conditions to the obtained reaction mixture [polymerization step B], whereby; c) the total amount of the monomers used for the polymerization is equal to 100 parts by weight, and the total amount of deionized water is
-
公开(公告)号:DE10223615A1
公开(公告)日:2003-12-11
申请号:DE10223615
申请日:2002-05-27
Applicant: BASF AG
Inventor: WULFF DIRK , FELDTHUSEN JENSEN JESPER , AUCHTER GERHARD , WILDBURG GERALD , FINK RALF
IPC: C08F2/22 , C08F257/02 , C08F265/04 , C08F285/00 , C08F291/00 , C08L51/00 , C09J151/00 , C08F220/18 , C08F212/08 , C08F236/06 , C08F214/04 , C08F210/02 , C08F218/04 , C04B24/26 , C09D5/02 , C09D5/12 , C09J133/10
Abstract: The invention relates to a method for producing an aqueous polymer dispersion having a polymer solids content of >=50% by weight by carrying out the radically initiated aqueous emulsion polymerization of ethylenically unsaturated compounds (monomers). The inventive method is characterized in that: a) a mixture is provided in a polymerization vessel and contains a partial quantity 1 consisting of: deionized water, 0.001 to 0.5 parts by weight of a polymer with a weighted average particle diameter of =80% [polymerization step A], and; b) afterwards, a monomer emulsion containing partial quantity 2, which consists of deionized water, 0.1 to 5 parts by weight of dispersants and 90 to 99.5 parts by weight of monomers, is fed under polymerization conditions to the obtained reaction mixture [polymerization step B], whereby; c) the total amount of the monomers used for the polymerization is equal to 100 parts by weight, and the total amount of deionized water is
-
公开(公告)号:DE10208039A1
公开(公告)日:2003-09-04
申请号:DE10208039
申请日:2002-02-26
Applicant: BASF AG
Inventor: DIEHL HEIKO , AYDIN ORAL , AUCHTER GERHARD , HARTZ OLIVER , DRAGON ANDREE
IPC: C08L23/06 , C08L57/00 , C09J7/02 , C09J133/06 , G09F3/10 , C09D5/02 , C09J4/02 , C09J123/06
-
公开(公告)号:ES2181026T3
公开(公告)日:2003-02-16
申请号:ES97941951
申请日:1997-08-21
Applicant: BASF AG
Inventor: REHMER GERD , STANGER BERND , AUCHTER GERHARD , TURK JOHANNES , AYDIN ORAL , FUSSL RUDIGER
IPC: C08F2/22 , C08F2/16 , C08F2/24 , C08F220/06 , C08F220/12 , C08F220/18 , C09J7/04 , C09J133/04 , C09J133/06
Abstract: Readily filterable and deodorizable aqueous dispersions of pressure-sensitive adhesive, especially for self-adhesive labels, having solids contents of more than 65%, can be prepared with readily reproducible properties by copolymerizing esters of acrylic and/or methacrylic acid in the presence of less than 50 ppm of inhibitor and, preferably, in the presence of from 0.01 to 5% by weight of reducing agent by a special emulsion technique. The highly concentrated pressure-sensitive adhesive dispersion, subsequently deodorized with steam, is free from coagulum and seediness.
-
公开(公告)号:BR9711330A
公开(公告)日:1999-08-17
申请号:BR9711330
申请日:1997-08-21
Applicant: BASF AG
Inventor: REHMER GERD , STANGER BERND , AUCHTER GERHARD , TUERK JOHANNES , AYDIN ORAL , FUESSL RUEDIGER
IPC: C08F2/22 , C08F2/16 , C08F2/24 , C08F220/06 , C08F220/12 , C08F220/18 , C09J7/04 , C09J133/04 , C09J133/06
Abstract: Readily filterable and deodorizable aqueous dispersions of pressure-sensitive adhesive, especially for self-adhesive labels, having solids contents of more than 65%, can be prepared with readily reproducible properties by copolymerizing esters of acrylic and/or methacrylic acid in the presence of less than 50 ppm of inhibitor and, preferably, in the presence of from 0.01 to 5% by weight of reducing agent by a special emulsion technique. The highly concentrated pressure-sensitive adhesive dispersion, subsequently deodorized with steam, is free from coagulum and seediness.
-
公开(公告)号:BR9711043A
公开(公告)日:1999-08-17
申请号:BR9711043
申请日:1997-07-29
Applicant: BASF AG
Inventor: SCHULER BERNHARD , AUCHTER GERHARD , TUERK JOHANNES , NOORDIJK RIK , DOBBELAAR JOHANNES , BAECHER REINHARD , HUEMMER WOLFGANG
IPC: C08L33/06 , C08F212/00 , C08F220/00 , C08F220/12 , C08F220/18 , C09J7/02 , C09J7/04 , C09J133/06 , G09F3/10 , C07F220/12
Abstract: A polymer which is composed offrom 50 to 99.98% by weight of a C1-C12 alkyl (meth)acrylate a),from 0.02 to 1.8% by weight of a vinyl-aromatic compound b),from 0 to 10% by weight of an ethylenically unsaturated acid or an ethylenically unsaturated acid anhydride c), andfrom 0 to 40% by weight of other monomers d), the percentages by weight being based on the polymer.
-
公开(公告)号:NO990567L
公开(公告)日:1999-02-08
申请号:NO990567
申请日:1999-02-08
Applicant: BASF AG
Inventor: SCHULER BERNHARD , AUCHTER GERHARD , T RK JOHNNES , NOORDIJK RIK , DOBBELAAR JOHANNES , BOCNER REINHARD , H MMER WOLFGANG
IPC: C08F212/00 , C08L33/06 , C08F220/00 , C08F220/12 , C08F220/18 , C09J7/02 , C09J7/04 , C09J133/06 , G09F3/10 , C08F
Abstract: A polymer which is composed offrom 50 to 99.98% by weight of a C1-C12 alkyl (meth)acrylate a),from 0.02 to 1.8% by weight of a vinyl-aromatic compound b),from 0 to 10% by weight of an ethylenically unsaturated acid or an ethylenically unsaturated acid anhydride c), andfrom 0 to 40% by weight of other monomers d), the percentages by weight being based on the polymer.
-
公开(公告)号:NO990567D0
公开(公告)日:1999-02-08
申请号:NO990567
申请日:1999-02-08
Applicant: BASF AG
Inventor: SCHULER BERNHARD , AUCHTER GERHARD , TUERK JOHNNES , NOORDIJK RIK , DOBBELAAR JOHANNES , BOCNER REINHARD , HUEMMER WOLFGANG
IPC: C08F212/00 , C08L33/06 , C08F220/00 , C08F220/12 , C08F220/18 , C09J7/02 , C09J7/04 , C09J133/06 , G09F3/10 , C08F
Abstract: A polymer which is composed offrom 50 to 99.98% by weight of a C1-C12 alkyl (meth)acrylate a),from 0.02 to 1.8% by weight of a vinyl-aromatic compound b),from 0 to 10% by weight of an ethylenically unsaturated acid or an ethylenically unsaturated acid anhydride c), andfrom 0 to 40% by weight of other monomers d), the percentages by weight being based on the polymer.
-
公开(公告)号:CA2263948A1
公开(公告)日:1998-02-26
申请号:CA2263948
申请日:1997-08-21
Applicant: BASF AG
Inventor: STANGER BERND , FUESSL RUEDIGER , REHMER GERD , AUCHTER GERHARD , AYDIN ORAL , TUERK JOHANNES
IPC: C08F2/22 , C08F2/16 , C08F2/24 , C08F220/06 , C08F220/12 , C08F220/18 , C09J7/04 , C09J133/04 , C09J133/06
Abstract: Aqueous solutions of adhesive materials which can be easily filtered and deodorized, particularly for self-adhesive labels, with a solids content of over 65 % can be produced with good reproducibility of characteristics through copolymerization of esters of acrylic and/or methacrylic acid in the presence of less than 50 ppm inhibitor and preferably in the presence of 0.01 to 5 % by weight of reducing agents, according to a special emulsion process. The highly concentrated and steam-deodorized adhesive material dispersion is free of coagulants and specks.
-
-
-
-
-
-
-
-
-