公开(公告)号:DE3333679A1
公开(公告)日:1985-04-04
申请号:DE3333679
申请日:1983-09-17
Applicant: BASF AG
Inventor: GEIERHAAS HERBERT DR , NETH NORBERT DR , ADLKOFER JUERGEN DR
Abstract: In the oxidation of hydrogen sulphide contained in exhaust gases and/or organic sulphur compounds, catalysts are used which contain a) cobalt oxide and b) tungsten oxide and/or molybdenum oxide as active components and which are applied to a support of silicic acid which has an internal surface area (according to BET) of 50 to 200 m /g and a water uptake capacity of 60 to 120 ml/100 g.
-
公开(公告)号:DE3732932A1
公开(公告)日:1989-04-13
申请号:DE3732932
申请日:1987-09-30
Applicant: BASF AG
-
公开(公告)号:DE3869033D1
公开(公告)日:1992-04-16
申请号:DE3869033
申请日:1988-09-22
Applicant: BASF AG
Inventor: BECKER HANS-JUERGEN DR , GEIERHAAS HERBERT DR , IRGANG MATTHIAS DR , SPRAGUE MICHAEL JOLYON DR
Abstract: A zine oxide contg desulphurisation material is claimed, contg 20-80 wt% high surface-area Zn0 and 20-80 wt% basic zinc carbonate, mixed with water to form, dried and calcined. The surface area of the zinc oxide is min 10 m2/g, pref over 30 m2/g; technical grade zinc carbonate is used, of formula 5Zno.2C02.3H20 The oxide and carbonate are blended with water (10-60 wt%, pref 20-50%, taken as proportion of total content), blending time 1-10h, usually 1-5h. The mixt is formed, and dried, and calcined.
-
公开(公告)号:DE4000609A1
公开(公告)日:1991-07-18
申请号:DE4000609
申请日:1990-01-11
Applicant: BASF AG
Inventor: MEISSNER RUPRECHT , GEIERHAAS HERBERT DR , ADLKOFER JUERGEN DR , LEBERT ULRICH DR
Abstract: Catalyst for oxidn. of SO2 to SO3 consists of a SiO2 support activated with V and alkali metal cpds. The support: has a pore vol. fraction of 10-30% pores with dia. up to 15nm, 25-60% pores with dia. 15-200 nm and 10-60% pores with a dia. of over 200nm. The catalyst is produced by mixing SiO2 of the specified pore dia. with enough liquid (water and/or H2SO4) to give a mouldable mixt., moulding, drying and calcining the moulding (at 450-650 deg.C), impregnating the calcined material with activators and drying. USE/ADVANTAGE - The catalyst has very good mechanical properties (hardness and attrition in both the fresh and aged state), high activity over a wide temp. range (ca. 380-420 deg.C) and very low pressure drop. The high activity at relatively low temp. makes it possible to reduce operating costs by using a lower temp. than usual and also reduces SO2 emissions at low temp.
-
公开(公告)号:DE1618130B
公开(公告)日:1971-05-19
申请号:DE1618130D
申请日:1967-04-03
Applicant: BASF AG
Inventor: GEIERHAAS HERBERT DR , WINTERSBERGER KARL DR , WUNSCH GERD DR
-
公开(公告)号:DE2301016A1
公开(公告)日:1974-07-18
申请号:DE2301016
申请日:1973-01-10
Applicant: BASF AG
Inventor: BUECHNER OSKAR DR , GEIERHAAS HERBERT DR , GIERTH VOLKER DR , MUELLER SIEGFRIED , ZACHER WIELAND DR
-
公开(公告)号:DE2260696A1
公开(公告)日:1974-07-04
申请号:DE2260696
申请日:1972-12-12
Applicant: BASF AG
Inventor: HEISS JUERGEN DR , SCHULZ GERHARD DR , BECK FRITZ DR , GEIERHAAS HERBERT DR , ZIRKER GUENTER DR
Abstract: Salts of 1-10C aliphatic mono- or di-carboxylic acids with metals of normal potential >=0.5V are prepd by reactn. of the metal with the acid, opt. with water in the presence of 0.1-10% nitrate ions in the media. The process partic. for 1-4C acids is pref. carried out at 50-200 degrees C in the presence of nitrate ions from the nitrate of the metal employed, ammonium nitrate or nitric acid. Partic. for Co. Ni, Cu in catalyst prepn.
-
公开(公告)号:DE1618130B1
公开(公告)日:1971-05-19
申请号:DE1618130D
申请日:1967-04-03
Applicant: BASF AG
Inventor: GEIERHAAS HERBERT DR , WINTERSBERGER KARL DR , WUNSCH GERD DR
-
公开(公告)号:CH478846A
公开(公告)日:1969-09-30
申请号:CH1016267
申请日:1967-07-17
Applicant: BASF AG
Inventor: WUNSCH GERD DR , WINTERSBERGER KARL DR , GEIERHAAS HERBERT DR
-
-
-
-
-
-
-
-