公开(公告)号:AT63755T
公开(公告)日:1991-06-15
申请号:AT88102524
申请日:1988-02-20
Applicant: BASF AG
Inventor: HERNER MARTIN DR , KELLER RUDOLF , KOEHNLEIN ERNST DR
-
公开(公告)号:DE3853770D1
公开(公告)日:1995-06-14
申请号:DE3853770
申请日:1988-12-10
Applicant: BASF AG
Inventor: SCHLAG JOHANNES DR , KOEHNLEIN ERNST DR , BAUER PETER , HERNER MARTIN DR , HUB HANS-HENNING DR
-
公开(公告)号:AT91820T
公开(公告)日:1993-08-15
申请号:AT89115872
申请日:1989-08-29
Applicant: BASF AG
-
公开(公告)号:AT122494T
公开(公告)日:1995-05-15
申请号:AT88120670
申请日:1988-12-10
Applicant: BASF AG
Inventor: SCHLAG JOHANNES DR , KOEHNLEIN ERNST DR , BAUER PETER , HERNER MARTIN DR , HUB HANS-HENNING DR
-
公开(公告)号:DE3862878D1
公开(公告)日:1991-06-27
申请号:DE3862878
申请日:1988-02-20
Applicant: BASF AG
Inventor: HERNER MARTIN DR , KELLER RUDOLF , KOEHNLEIN ERNST DR
Abstract: The invention relates to a method of making a crosslinkable ethylene polymer sheet by taking a film of carboxyl-containing ethylene polymer, which is preferably an ethylene-acrylic acid-alkyl acrylate terpolymer or a graft copolymer of ethylene polymer and carboxyl-containing monomer, and applying to it at from room temperature to +45 DEG C, preferably with the aid of pressure systems, a liquid organic peroxide in a uniform manner in amounts of from 0.3 to 3.0 % by weight and allowing the peroxide to diffuse into the film, and to the use of the crosslinkable ethylene copolymer sheet for making a layered material by placing the adhesive sheet between two cover sheets and heating while employing a small amount of pressure.
-
公开(公告)号:DE3830008A1
公开(公告)日:1990-03-15
申请号:DE3830008
申请日:1988-09-03
Applicant: BASF AG
-
公开(公告)号:DE3300749A1
公开(公告)日:1984-07-12
申请号:DE3300749
申请日:1983-01-12
Applicant: BASF AG
Inventor: KOEHNLEIN ERNST DR , BAUER PETER
-
公开(公告)号:DE3816397A1
公开(公告)日:1989-11-23
申请号:DE3816397
申请日:1988-05-13
Applicant: BASF AG
Inventor: KOEHNLEIN ERNST DR , SCHLAG JOHANNES DR , VOGT HEINZ DR , BAUER PETER , HAUSS ALFRED FRIEDRICH DR
Abstract: The invention relates to an electrical high-voltage cable of 1 to 500 kV, the cable insulation being resistant towards the formation or growth of water trees and consists of 70 to 99 parts by weight of an ethylenepolymer (I) and 1 to 30 parts by weight of an ethylenecopolymer (II) which consists of 80 to 92 parts by weight of ethylene and 8 to 20 parts by weight of C4-C10- alpha -olefins with a density of 0.890 to 0.915 g/cm and a crystalline melting point of 90 to 125 DEG C.
-
公开(公告)号:DE3705784A1
公开(公告)日:1988-09-01
申请号:DE3705784
申请日:1987-02-24
Applicant: BASF AG
Inventor: HERNER MARTIN DR , KELLER RUDOLF , KOEHNLEIN ERNST DR
Abstract: The invention relates to a method of making a crosslinkable ethylene polymer sheet by taking a film of carboxyl-containing ethylene polymer, which is preferably an ethylene-acrylic acid-alkyl acrylate terpolymer or a graft copolymer of ethylene polymer and carboxyl-containing monomer, and applying to it at from room temperature to +45 DEG C, preferably with the aid of pressure systems, a liquid organic peroxide in a uniform manner in amounts of from 0.3 to 3.0 % by weight and allowing the peroxide to diffuse into the film, and to the use of the crosslinkable ethylene copolymer sheet for making a layered material by placing the adhesive sheet between two cover sheets and heating while employing a small amount of pressure.
-
公开(公告)号:DE3607757A1
公开(公告)日:1987-09-10
申请号:DE3607757
申请日:1986-03-08
Applicant: BASF AG
Inventor: SCHLAG JOHANNES DR , KOEHNLEIN ERNST DR , BAUER PETER , KOESSLER LUDWIG , HAUSS ALFRED FRIEDRICH DR
-
-
-
-
-
-
-
-
-