公开(公告)号:DE3906524A1
公开(公告)日:1990-09-13
申请号:DE3906524
申请日:1989-03-02
Applicant: BASF AG
Inventor: NINTZ ECKHARD DR , WEBER HEINZ DR
-
公开(公告)号:DE3925740A1
公开(公告)日:1991-02-07
申请号:DE3925740
申请日:1989-08-03
Applicant: BASF AG
Inventor: WEBER HEINZ DR , EHRMANN GERD DR , DIETZEN FRANZ-JOSEF DR , NINTZ ECKHARD DR , ZETTLER HANS DIETER
-
公开(公告)号:DE59009709D1
公开(公告)日:1995-11-02
申请号:DE59009709
申请日:1990-07-24
Applicant: BASF AG
Inventor: WEBER HEINZ DR , EHRMANN GERD DR , DIETZEN FRANZ-JOSEF DR , NINTZ ECKHARD DR , ZETTLER HANS DIETER
-
公开(公告)号:ES2052808T3
公开(公告)日:1994-07-16
申请号:ES89108685
申请日:1989-05-13
Applicant: BASF AG
Inventor: WEBER HEINZ DR , NINTZ ECKHARD DR , WALTER MANFRED DR , BALLWEBER DIETER , OSTERMAYER BERTRAM DR
Abstract: Expandable polymers in particle form for the preparation of foams having high heat distortion resistance contain from 20 to 94.9% by weight of a styrene polymer, from 0.1 to 75% by weight of a polyphenylene ether and from 5 to 20% by weight of a blowing agent mixture of aliphatic or cycloaliphatic hydrocarbons on the one hand and aromatic hydrocarbons, alcohols, ketones, ethers, esters and/or chlorohydrocarbons on the other hand.
-
公开(公告)号:DE58902323D1
公开(公告)日:1992-10-29
申请号:DE58902323
申请日:1989-05-13
Applicant: BASF AG
Inventor: WEBER HEINZ DR , NINTZ ECKHARD DR , WALTER MANFRED DR , BALLWEBER DIETER , OSTERMAYER BERTRAM DR
Abstract: Expandable polymers in particle form for the preparation of foams having high heat distortion resistance contain from 20 to 94.9% by weight of a styrene polymer, from 0.1 to 75% by weight of a polyphenylene ether and from 5 to 20% by weight of a blowing agent mixture of aliphatic or cycloaliphatic hydrocarbons on the one hand and aromatic hydrocarbons, alcohols, ketones, ethers, esters and/or chlorohydrocarbons on the other hand.
-
公开(公告)号:DE3918583A1
公开(公告)日:1990-12-13
申请号:DE3918583
申请日:1989-06-07
Applicant: BASF AG
Inventor: NINTZ ECKHARD DR , WEBER HEINZ DR , NICKOLAUS WILHELM DR
IPC: C08J9/08
Abstract: Foams having a density of from 0.1 to 1.0 g/cm and based on aromatic polyether ketones and other thermoplastic polymers having a high melting point are obtained by melting an intimate mixture of the polymer and from 0.5 to 10% by weight of an aliphatic or aromatic di- or polycarboxylic acid which undergoes a weight loss of at least 50% on heating to from 130 to 300 DEG C with elimination of gaseous decomposition products, and cooling the product with simultaneous shaping.
-
公开(公告)号:DE3817631A1
公开(公告)日:1989-11-30
申请号:DE3817631
申请日:1988-05-25
Applicant: BASF AG
Inventor: WEBER HEINZ DR , NINTZ ECKHARD DR , WALTER MANFRED DR , BALLWEBER DIETER , OSTERMAYER BERTRAM DR
Abstract: Expandable polymers in particle form for the preparation of foams having high heat distortion resistance contain from 20 to 94.9% by weight of a styrene polymer, from 0.1 to 75% by weight of a polyphenylene ether and from 5 to 20% by weight of a blowing agent mixture of aliphatic or cycloaliphatic hydrocarbons on the one hand and aromatic hydrocarbons, alcohols, ketones, ethers, esters and/or chlorohydrocarbons on the other hand.
-
-
-
-
-
-