公开(公告)号:FI961679A
公开(公告)日:1996-04-17
申请号:FI961679
申请日:1996-04-17
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58 , D21H , C08L
Abstract: PCT No. PCT/EP94/02034 Sec. 371 Date Mar. 29, 1996 Sec. 102(e) Date Mar. 29, 1996 PCT Filed Jun. 22, 1994 PCT Pub. No. WO95/11342 PCT Pub. Date Apr. 27, 1995Papers which are coated with a paper coating slip based on a binder containing A) from 1 to 49% by weight of polymers based on esters of acrylic acid or of methacrylic acid with a C4-C12-alkanol, having a glass transition temperature of from -80 DEG to +25 DEG C., and B) from 51 to 99% by weight of polymers based on butadiene, the stated weights being based on the sum A)+B), are used for offset printing.
-
公开(公告)号:AT171492T
公开(公告)日:1998-10-15
申请号:AT94922859
申请日:1994-06-22
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58
Abstract: PCT No. PCT/EP94/02034 Sec. 371 Date Mar. 29, 1996 Sec. 102(e) Date Mar. 29, 1996 PCT Filed Jun. 22, 1994 PCT Pub. No. WO95/11342 PCT Pub. Date Apr. 27, 1995Papers which are coated with a paper coating slip based on a binder containing A) from 1 to 49% by weight of polymers based on esters of acrylic acid or of methacrylic acid with a C4-C12-alkanol, having a glass transition temperature of from -80 DEG to +25 DEG C., and B) from 51 to 99% by weight of polymers based on butadiene, the stated weights being based on the sum A)+B), are used for offset printing.
-
公开(公告)号:ES2121219T3
公开(公告)日:1998-11-16
申请号:ES94922859
申请日:1994-06-22
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58
Abstract: PCT No. PCT/EP94/02034 Sec. 371 Date Mar. 29, 1996 Sec. 102(e) Date Mar. 29, 1996 PCT Filed Jun. 22, 1994 PCT Pub. No. WO95/11342 PCT Pub. Date Apr. 27, 1995Papers which are coated with a paper coating slip based on a binder containing A) from 1 to 49% by weight of polymers based on esters of acrylic acid or of methacrylic acid with a C4-C12-alkanol, having a glass transition temperature of from -80 DEG to +25 DEG C., and B) from 51 to 99% by weight of polymers based on butadiene, the stated weights being based on the sum A)+B), are used for offset printing.
-
公开(公告)号:AU1808095A
公开(公告)日:1995-05-08
申请号:AU1808095
申请日:1994-06-22
Applicant: BASF AG
Inventor: WIRTH THOMAS , SCHULER BERNHARD , LAWRENZ DIRK , STURM BERTHOLD , NISSLER HARALD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58
Abstract: PCT No. PCT/EP94/02034 Sec. 371 Date Mar. 29, 1996 Sec. 102(e) Date Mar. 29, 1996 PCT Filed Jun. 22, 1994 PCT Pub. No. WO95/11342 PCT Pub. Date Apr. 27, 1995Papers which are coated with a paper coating slip based on a binder containing A) from 1 to 49% by weight of polymers based on esters of acrylic acid or of methacrylic acid with a C4-C12-alkanol, having a glass transition temperature of from -80 DEG to +25 DEG C., and B) from 51 to 99% by weight of polymers based on butadiene, the stated weights being based on the sum A)+B), are used for offset printing.
-
公开(公告)号:CA2174233A1
公开(公告)日:1995-04-27
申请号:CA2174233
申请日:1994-06-22
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58 , B41M1/36
Abstract: The invention concerns the use, for offset printing, of paper coated with a binder-based coating compound containing A) 1 to 49 % by wt. of polymers made from esters of acrylic or methacrylic acid with C4-C12 alkanols and having a glass transition temperature of -80 to +25 ~C, and B) 51 to 99 % by wt. of butadiene polymers, the weights being relative to the total of A and B.
-
公开(公告)号:CA2174233C
公开(公告)日:2004-03-30
申请号:CA2174233
申请日:1994-06-22
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58 , B41M1/36
Abstract: The invention concerns the use, for offset printing, of paper coated with a binder-based coating compound containing A) 1 to 49 % by wt. of polymers mad e from esters of acrylic or methacrylic acid with C4-C12 alkanols and having a glass transition temperature of -80 to +25 ~C, and B) 51 to 99 % by wt. of butadiene polymers, the weights being relative to the total of A and B.
-
公开(公告)号:DE59406985D1
公开(公告)日:1998-10-29
申请号:DE59406985
申请日:1994-06-22
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58
Abstract: PCT No. PCT/EP94/02034 Sec. 371 Date Mar. 29, 1996 Sec. 102(e) Date Mar. 29, 1996 PCT Filed Jun. 22, 1994 PCT Pub. No. WO95/11342 PCT Pub. Date Apr. 27, 1995Papers which are coated with a paper coating slip based on a binder containing A) from 1 to 49% by weight of polymers based on esters of acrylic acid or of methacrylic acid with a C4-C12-alkanol, having a glass transition temperature of from -80 DEG to +25 DEG C., and B) from 51 to 99% by weight of polymers based on butadiene, the stated weights being based on the sum A)+B), are used for offset printing.
-
公开(公告)号:FI961679A0
公开(公告)日:1996-04-17
申请号:FI961679
申请日:1996-04-17
Applicant: BASF AG
Inventor: WIRTH THOMAS , NISSLER HARALD , STURM BERTHOLD , LAWRENZ DIRK , SCHULER BERNHARD
IPC: C09D109/00 , C09D109/10 , C09D113/02 , C09D121/00 , C09D133/04 , C09D133/06 , D21H19/44 , D21H19/58 , D21H , C08L
Abstract: PCT No. PCT/EP94/02034 Sec. 371 Date Mar. 29, 1996 Sec. 102(e) Date Mar. 29, 1996 PCT Filed Jun. 22, 1994 PCT Pub. No. WO95/11342 PCT Pub. Date Apr. 27, 1995Papers which are coated with a paper coating slip based on a binder containing A) from 1 to 49% by weight of polymers based on esters of acrylic acid or of methacrylic acid with a C4-C12-alkanol, having a glass transition temperature of from -80 DEG to +25 DEG C., and B) from 51 to 99% by weight of polymers based on butadiene, the stated weights being based on the sum A)+B), are used for offset printing.
-
-
-
-
-
-
-