公开(公告)号:NO952887D0
公开(公告)日:1995-07-20
申请号:NO952887
申请日:1995-07-20
Applicant: BASF AG
Inventor: FETZNER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
IPC: B01D53/56 , B01D53/86 , B01D53/94 , B01J21/04 , B01J23/00 , B01J23/72 , B01J23/76 , B01J23/78 , B01J23/80 , B01J35/10 , C07C51/487
Abstract: PCT No. PCT/EP94/00081 Sec. 371 Date Mar. 24, 1995 Sec. 102(e) Date Mar. 24, 1995 PCT Filed Jan. 13, 1994 PCT Pub. No. WO94/16798 PCT Pub. Date Aug. 4, 1994A process for the catalytic decomposition of dinitrogen monoxide in a gas stream by contacting the gas stream at temperatures of 200 DEG -900 DEG C. and pressures of 0.1 to 20 bar with a catalyst free of noble metals, the catalyst being prepared by combining a spinel CuAl2O3 with another spinel-forming metal component selected from the group consisting of tin, lead, zinc, magnesium, calcium, strontium and barium or mixtures thereof in elemental form or as an oxide or salt, and calcining at temperatures of 300 DEG -1300 DEG C. and under pressures of 0.1-200 bar in order to at least partially liberate the copper from the spinel by replacement with the other metal component.
-
公开(公告)号:AU5882794A
公开(公告)日:1994-08-15
申请号:AU5882794
申请日:1994-01-13
Applicant: BASF AG
Inventor: FETZER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
IPC: B01D53/56 , B01D53/86 , B01D53/94 , B01J21/04 , B01J23/00 , B01J23/72 , B01J23/76 , B01J23/78 , B01J23/80 , B01J35/10 , C07C51/487 , B01D53/36
Abstract: PCT No. PCT/EP94/00081 Sec. 371 Date Mar. 24, 1995 Sec. 102(e) Date Mar. 24, 1995 PCT Filed Jan. 13, 1994 PCT Pub. No. WO94/16798 PCT Pub. Date Aug. 4, 1994A process for the catalytic decomposition of dinitrogen monoxide in a gas stream by contacting the gas stream at temperatures of 200 DEG -900 DEG C. and pressures of 0.1 to 20 bar with a catalyst free of noble metals, the catalyst being prepared by combining a spinel CuAl2O3 with another spinel-forming metal component selected from the group consisting of tin, lead, zinc, magnesium, calcium, strontium and barium or mixtures thereof in elemental form or as an oxide or salt, and calcining at temperatures of 300 DEG -1300 DEG C. and under pressures of 0.1-200 bar in order to at least partially liberate the copper from the spinel by replacement with the other metal component.
-
公开(公告)号:IN182764B
公开(公告)日:1999-07-17
申请号:IN28MA1994
申请日:1994-01-19
Applicant: BASF AG
Inventor: FETZER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
-
公开(公告)号:DE59402378D1
公开(公告)日:1997-05-15
申请号:DE59402378
申请日:1994-01-13
Applicant: BASF AG
Inventor: FETZER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
IPC: B01D53/56 , B01D53/86 , B01D53/94 , B01J21/04 , B01J23/00 , B01J23/72 , B01J23/76 , B01J23/78 , B01J23/80 , B01J35/10 , C07C51/487
Abstract: PCT No. PCT/EP94/00081 Sec. 371 Date Mar. 24, 1995 Sec. 102(e) Date Mar. 24, 1995 PCT Filed Jan. 13, 1994 PCT Pub. No. WO94/16798 PCT Pub. Date Aug. 4, 1994A process for the catalytic decomposition of dinitrogen monoxide in a gas stream by contacting the gas stream at temperatures of 200 DEG -900 DEG C. and pressures of 0.1 to 20 bar with a catalyst free of noble metals, the catalyst being prepared by combining a spinel CuAl2O3 with another spinel-forming metal component selected from the group consisting of tin, lead, zinc, magnesium, calcium, strontium and barium or mixtures thereof in elemental form or as an oxide or salt, and calcining at temperatures of 300 DEG -1300 DEG C. and under pressures of 0.1-200 bar in order to at least partially liberate the copper from the spinel by replacement with the other metal component.
-
公开(公告)号:AU4177496A
公开(公告)日:1996-07-03
申请号:AU4177496
申请日:1995-12-01
Applicant: BASF AG
Inventor: KOPIETZ MICHAEL , HANDERMAN ALAN , JONES SIMON , KALCK ULRICH , PRIESTER CLAUS-ULRICH , AUER HEINZ , RITZ JOSEF , FUCHS HUGO , PIJL PAUL
IPC: B01J8/10 , C07D201/12 , C08G69/14 , C08J11/16
Abstract: Caprolactam is obtained from caprolactam-containing polymers in the presence of a base under reduced pressure by depolymerizing polymers which contain the repeating unit -[-N(H)-(CH2)5-C(O)-] or mixtures consisting essentially of from 50 to 99.99% by weight of a polymer containing the repeating unit -[-N(H)-(CH2)5-C(O)-]- from 0.01 to 50% by weight of additives selected from the group consisting of inorganic fillers, organic and inorganic pigments and dyes, from 0 to 10% by weight of organic and/or inorganic additives, from 0 to 40% by weight of non-polyamide-containing polymers and from 0 to 20% by weight of polyamides, with the exception of polycaprolactam and copolyamides prepared from caprolactam, in at least two depolymerization reactors connected in series.
-
公开(公告)号:NO952887L
公开(公告)日:1995-07-20
申请号:NO952887
申请日:1995-07-20
Applicant: BASF AG
Inventor: FETZNER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
IPC: B01D53/56 , B01D53/86 , B01D53/94 , B01J21/04 , B01J23/00 , B01J23/72 , B01J23/76 , B01J23/78 , B01J23/80 , B01J35/10 , C07C51/487
Abstract: PCT No. PCT/EP94/00081 Sec. 371 Date Mar. 24, 1995 Sec. 102(e) Date Mar. 24, 1995 PCT Filed Jan. 13, 1994 PCT Pub. No. WO94/16798 PCT Pub. Date Aug. 4, 1994A process for the catalytic decomposition of dinitrogen monoxide in a gas stream by contacting the gas stream at temperatures of 200 DEG -900 DEG C. and pressures of 0.1 to 20 bar with a catalyst free of noble metals, the catalyst being prepared by combining a spinel CuAl2O3 with another spinel-forming metal component selected from the group consisting of tin, lead, zinc, magnesium, calcium, strontium and barium or mixtures thereof in elemental form or as an oxide or salt, and calcining at temperatures of 300 DEG -1300 DEG C. and under pressures of 0.1-200 bar in order to at least partially liberate the copper from the spinel by replacement with the other metal component.
-
公开(公告)号:UA42712C2
公开(公告)日:2001-11-15
申请号:UA95083847
申请日:1994-01-13
Applicant: BASF AG
Inventor: FETZER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
IPC: B01D53/56 , B01D53/86 , B01D53/94 , B01J21/04 , B01J23/00 , B01J23/72 , B01J23/76 , B01J23/78 , B01J23/80 , B01J35/10 , C07C51/487
Abstract: Спосібкаталітичногорозкладузакисуазотувключаєпроведенняобробкинакаталізаторі, якийотриманошляхомоб’єднання CuAl2O4, принаймні, зоднимметалом, вибранимізгрупи, якавключаєолово, свинецьтаелементІІ-їголовноїабопобічноїгрупиперіодичноїсистемиелементіву виглядіоксидуабосоліабов елементарномувигляді, такальцинаціїпритемпературах 300 - 1300 ºСтатиску 0,1 - 200 бар.
-
公开(公告)号:AT151309T
公开(公告)日:1997-04-15
申请号:AT94905047
申请日:1994-01-13
Applicant: BASF AG
Inventor: FETZER THOMAS , BUECHELE WOLFGANG , WISTUBA HERMANN , OTTO BERNHARD , BUERGER GERT , PIJL PAUL
IPC: B01D53/56 , B01D53/86 , B01D53/94 , B01J21/04 , B01J23/00 , B01J23/72 , B01J23/76 , B01J23/78 , B01J23/80 , B01J35/10 , C07C51/487
Abstract: PCT No. PCT/EP94/00081 Sec. 371 Date Mar. 24, 1995 Sec. 102(e) Date Mar. 24, 1995 PCT Filed Jan. 13, 1994 PCT Pub. No. WO94/16798 PCT Pub. Date Aug. 4, 1994A process for the catalytic decomposition of dinitrogen monoxide in a gas stream by contacting the gas stream at temperatures of 200 DEG -900 DEG C. and pressures of 0.1 to 20 bar with a catalyst free of noble metals, the catalyst being prepared by combining a spinel CuAl2O3 with another spinel-forming metal component selected from the group consisting of tin, lead, zinc, magnesium, calcium, strontium and barium or mixtures thereof in elemental form or as an oxide or salt, and calcining at temperatures of 300 DEG -1300 DEG C. and under pressures of 0.1-200 bar in order to at least partially liberate the copper from the spinel by replacement with the other metal component.
-
公开(公告)号:DE2960562D1
公开(公告)日:1981-11-05
申请号:DE2960562
申请日:1979-05-03
Applicant: BASF AG
Inventor: DECKER EMILE DE , NEUBAUER GERALD DR , PIJL PAUL , WAUWE GERARD VAN
-
-
-
-
-
-
-
-
-