1.
    发明专利
    未知

    公开(公告)号:NO975601L

    公开(公告)日:1998-06-05

    申请号:NO975601

    申请日:1997-12-03

    Applicant: BASF AG

    Abstract: Modification of the cross-flow resistance of a diaphragm based on fibrous material comprises treating the diaphragm, during or after manufacture, with a dispersion of a component (I) containing fluorine and optionally a solution containing a zirconium dioxide (ZrO2) precursor. Preferably treatment is carried out during electrolysis. The amount of (I) used is 0.1-30 wt.% w.r.t. the fibrous material of the diaphragm and the amount applied is 30-500 g/m diaphragm surface area.

    3.
    发明专利
    未知

    公开(公告)号:NO984888L

    公开(公告)日:1999-04-22

    申请号:NO984888

    申请日:1998-10-20

    Applicant: BASF AG

    Abstract: Composite fibers (I) are prepared by heating a mixture of a PTFE or PTFE-copolymer-dispersion or powder with a fine particulate inorganic material and a fiber forming material with stirring such that the PTFE or PTFE copolymer becomes capable of flow but does not decompose and the dispersing agent is removed (in the case of a dispersion) and shearing the mixture in a mixer having a Froude number of more than 1. An Independent claim is included for a process for the production of a diaphragm by addition of (I) to a solution containing water and a thickening agent; filtering of the mixture with suction over a porous support to layer the composite fiber (I); drying of the coated porous support and heating at 90-390 degrees C.

    5.
    发明专利
    未知

    公开(公告)号:NO984888D0

    公开(公告)日:1998-10-20

    申请号:NO984888

    申请日:1998-10-20

    Applicant: BASF AG

    Abstract: Composite fibers (I) are prepared by heating a mixture of a PTFE or PTFE-copolymer-dispersion or powder with a fine particulate inorganic material and a fiber forming material with stirring such that the PTFE or PTFE copolymer becomes capable of flow but does not decompose and the dispersing agent is removed (in the case of a dispersion) and shearing the mixture in a mixer having a Froude number of more than 1. An Independent claim is included for a process for the production of a diaphragm by addition of (I) to a solution containing water and a thickening agent; filtering of the mixture with suction over a porous support to layer the composite fiber (I); drying of the coated porous support and heating at 90-390 degrees C.