公开(公告)号:AT239045T
公开(公告)日:2003-05-15
申请号:AT00954599
申请日:2000-08-08
Applicant: BASF AG
Inventor: KRECH RUEDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF
Abstract: A thermoplastic polyurethane (I) has: (a) a Shore A hardness of 45-80; (b) a tensile strength (DIN53504) of greater than 15 MPa; (c) a tear strength (DIN53515) of greater than 30 N/mm and an abrasion resistance (DIN 53516) of less than 250 mm . Independent claims are included for: (1) the production of (I) by mixing a thermoplastic polyurethane with a diol having a mol. wt. of 62-700 g/mol, followed by the addition of an isocyanate and optionally an isocyanate reactive compound, having a mol. wt. of 701-8000, diols having a mol. wt. of 62-700, catalyst and/or additive and/or pressing aids; and (2) The production of film, molded articles, rolls, fibers or cladding in automobiles, ducting, cable connectors, bellows, cable sheathing, sealant, or dampening elements containing the thermoplastic polyurethane (I).
-
公开(公告)号:ES2198344T3
公开(公告)日:2004-02-01
申请号:ES00954599
申请日:2000-08-08
Applicant: BASF AG
Inventor: KRECH RUEDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF
Abstract: A thermoplastic polyurethane (I) has: (a) a Shore A hardness of 45-80; (b) a tensile strength (DIN53504) of greater than 15 MPa; (c) a tear strength (DIN53515) of greater than 30 N/mm and an abrasion resistance (DIN 53516) of less than 250 mm . Independent claims are included for: (1) the production of (I) by mixing a thermoplastic polyurethane with a diol having a mol. wt. of 62-700 g/mol, followed by the addition of an isocyanate and optionally an isocyanate reactive compound, having a mol. wt. of 701-8000, diols having a mol. wt. of 62-700, catalyst and/or additive and/or pressing aids; and (2) The production of film, molded articles, rolls, fibers or cladding in automobiles, ducting, cable connectors, bellows, cable sheathing, sealant, or dampening elements containing the thermoplastic polyurethane (I).
-
公开(公告)号:AT373030T
公开(公告)日:2007-09-15
申请号:AT02019574
申请日:2000-08-08
Applicant: BASF AG
Inventor: KRECH RUEDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF
Abstract: A thermoplastic polyurethane (I) has: (a) a Shore A hardness of 45-80; (b) a tensile strength (DIN53504) of greater than 15 MPa; (c) a tear strength (DIN53515) of greater than 30 N/mm and an abrasion resistance (DIN 53516) of less than 250 mm . Independent claims are included for: (1) the production of (I) by mixing a thermoplastic polyurethane with a diol having a mol. wt. of 62-700 g/mol, followed by the addition of an isocyanate and optionally an isocyanate reactive compound, having a mol. wt. of 701-8000, diols having a mol. wt. of 62-700, catalyst and/or additive and/or pressing aids; and (2) The production of film, molded articles, rolls, fibers or cladding in automobiles, ducting, cable connectors, bellows, cable sheathing, sealant, or dampening elements containing the thermoplastic polyurethane (I).
-
公开(公告)号:DE50014660D1
公开(公告)日:2007-10-25
申请号:DE50014660
申请日:2000-08-08
Applicant: BASF AG
Inventor: KRECH RUEDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF DR
Abstract: A thermoplastic polyurethane (I) has: (a) a Shore A hardness of 45-80; (b) a tensile strength (DIN53504) of greater than 15 MPa; (c) a tear strength (DIN53515) of greater than 30 N/mm and an abrasion resistance (DIN 53516) of less than 250 mm . Independent claims are included for: (1) the production of (I) by mixing a thermoplastic polyurethane with a diol having a mol. wt. of 62-700 g/mol, followed by the addition of an isocyanate and optionally an isocyanate reactive compound, having a mol. wt. of 701-8000, diols having a mol. wt. of 62-700, catalyst and/or additive and/or pressing aids; and (2) The production of film, molded articles, rolls, fibers or cladding in automobiles, ducting, cable connectors, bellows, cable sheathing, sealant, or dampening elements containing the thermoplastic polyurethane (I).
-
公开(公告)号:DE50001996D1
公开(公告)日:2003-06-05
申请号:DE50001996
申请日:2000-08-08
Applicant: BASF AG
Inventor: KRECH RUEDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF
Abstract: A thermoplastic polyurethane (I) has: (a) a Shore A hardness of 45-80; (b) a tensile strength (DIN53504) of greater than 15 MPa; (c) a tear strength (DIN53515) of greater than 30 N/mm and an abrasion resistance (DIN 53516) of less than 250 mm . Independent claims are included for: (1) the production of (I) by mixing a thermoplastic polyurethane with a diol having a mol. wt. of 62-700 g/mol, followed by the addition of an isocyanate and optionally an isocyanate reactive compound, having a mol. wt. of 701-8000, diols having a mol. wt. of 62-700, catalyst and/or additive and/or pressing aids; and (2) The production of film, molded articles, rolls, fibers or cladding in automobiles, ducting, cable connectors, bellows, cable sheathing, sealant, or dampening elements containing the thermoplastic polyurethane (I).
-
公开(公告)号:ES2290225T3
公开(公告)日:2008-02-16
申请号:ES02019574
申请日:2000-08-08
Applicant: BASF AG
Inventor: KRECH RUDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF DR
Abstract: Poliuretanos termoplásticos con una dureza Shore de 45 A a 80 A, una resistencia a la tracción según DIN 53504 mayor que 15 MPa, una resistencia al desgarro progresivo según DIN 53515 mayor que 30 N/mm, y una abrasión según DIN 53516 menor que 250 mm3.
-
公开(公告)号:DE19939112A1
公开(公告)日:2001-02-22
申请号:DE19939112
申请日:1999-08-18
Applicant: BASF AG
Inventor: KRECH RUEDIGER , MUELLER JUERGEN , POHLMANN NORBERT , SELLIG PAUL , STEINBERGER ROLF
Abstract: The invention relates to thermoplastic polyurethane with a Shore hardness of 45 A to 80 A, a tensile strength, according to DIN 53504, higher than 5 Mpa, a tear strength, according to DIN 53515 higher than 30 N/mm and an abrasion according to DIN 53516 of less than 250 mm .
-
-
-
-
-
-