公开(公告)号:AU510789B2
公开(公告)日:1980-07-10
申请号:AU3119477
申请日:1977-12-02
Applicant: BASF AG
Inventor: THEYSOHN R , PENZIEN K , SEYDL W , WURMB R , REIMANN H , CORDES C , STERZEL H-J
IPC: C08L77/00 , C08K3/22 , C08K5/03 , C08L1/00 , C08L7/00 , C08L21/00 , C08L27/00 , C08L33/00 , C08L33/02 , C08L51/00 , C08L51/02 , C08L77/06 , C09K3/28
Abstract: A flameproofed nylon molding composition which can be processed by thermoplastic methods and which contains, as the flameproofing agent, from 5 to 30% by weight of brominated styrene oligomers and a synergistic metal oxide. The compositions may be used for the manufacture of injection moldings for the electrical industry.
-
公开(公告)号:SE7800800A
公开(公告)日:1978-07-29
申请号:SE7800800
申请日:1978-01-23
Applicant: BASF AG
IPC: C08L77/00 , C08K3/22 , C08K5/03 , C08L1/00 , C08L7/00 , C08L21/00 , C08L27/00 , C08L33/00 , C08L33/02 , C08L51/00 , C08L51/02
Abstract: A flameproofed nylon molding composition which can be processed by thermoplastic methods and which contains, as the flameproofing agent, from 5 to 30% by weight of brominated styrene oligomers and a synergistic metal oxide. The compositions may be used for the manufacture of injection moldings for the electrical industry.
-
-
公开(公告)号:SE412406B
公开(公告)日:1980-03-03
申请号:SE7602258
申请日:1976-02-24
Applicant: BASF AG
Inventor: HORN P , WURMB R , LEUTNER B , SEYDL W , THEYSOHN R , SCHLIMPER H-U
-
公开(公告)号:SE7800800L
公开(公告)日:1978-07-29
申请号:SE7800800
申请日:1978-01-23
Applicant: BASF AG
IPC: C08L77/00 , C08K3/22 , C08K5/03 , C08L1/00 , C08L7/00 , C08L21/00 , C08L27/00 , C08L33/00 , C08L33/02 , C08L51/00 , C08L51/02
Abstract: A flameproofed nylon molding composition which can be processed by thermoplastic methods and which contains, as the flameproofing agent, from 5 to 30% by weight of brominated styrene oligomers and a synergistic metal oxide. The compositions may be used for the manufacture of injection moldings for the electrical industry.
-
公开(公告)号:SE7501790A
公开(公告)日:1975-08-25
申请号:SE7501790
申请日:1975-02-18
Applicant: BASF AG
CPC classification number: C08K3/34 , C08K3/016 , C08K3/02 , C08K3/40 , C08K5/0066 , C08K13/04 , Y10S260/24 , C08L67/02
Abstract: Glass-fiber-reinforced molding compositions of reduced flammability consisting of (A) a linear saturated polyester resin, (B) from 10 to 60 per cent by weight of glass fibers and (C) from 3 to 30 per cent by weight of a flame retardant. The compositions contain from 2 to 20 per cent by weight, based on the total weight of the molding composition, of a particulate water-insoluble silicate having a bulk density of more than 100 g/l, which prevents dripping of the composition when in contact with an open flame.
-
公开(公告)号:SE7602258L
公开(公告)日:1976-09-22
申请号:SE7602258
申请日:1976-02-24
Applicant: BASF AG
Inventor: HORN P , WURMB P , LEUTNER B , SEYDL W , THEYSOHN R , SCHLIMPER H-U
-
公开(公告)号:SE7602258A
公开(公告)日:1976-09-22
申请号:SE7602258
申请日:1976-02-24
Applicant: BASF AG
Inventor: HORN P , WURMB P , LEUTNER B , SEYDL W , THEYSOHN R , SCHLIMPER H-U
CPC classification number: C08K9/12 , C08K3/22 , C08K5/0066 , C08L77/00
-
公开(公告)号:BR7506976A
公开(公告)日:1976-08-17
申请号:BR7506976
申请日:1975-10-24
Applicant: BASF AG
Inventor: JESERICH W , CORDES C , SEYDL W , WEISS H
Abstract: Process for the continuous manufacture of polymeric starting materials for high-grade transparent thin sheeting, wherein A. epsilon -CAPROLACTAM IS CONTINUOUSLY AGITATED IN A FIRST REACTION ZONE UNDER POLYAMIDE-FORMING CONDITIONS AT TEMPERATURES OF FROM 240 DEG TO 290 DEG C until at least 20% and preferably at least 35% of the epsilon -caprolactam has reacted, B. MAGNESIUM SILICATE HAVING A PARTICLE SIZE OF LESS THAN 30 mu M IS THEN ADDED TO THE MELT TO GIVE MAGNESIUM SILICATE CONCENTRATIONS IN THE REACTION MIXTURE OF FROM 0.0005 TO 0.5% AND PREFERABLY FROM 0.001 TO 0.
-
公开(公告)号:SE7501790L
公开(公告)日:1975-08-25
申请号:SE7501790
申请日:1975-02-18
Applicant: BASF AG
Abstract: Glass-fiber-reinforced molding compositions of reduced flammability consisting of (A) a linear saturated polyester resin, (B) from 10 to 60 per cent by weight of glass fibers and (C) from 3 to 30 per cent by weight of a flame retardant. The compositions contain from 2 to 20 per cent by weight, based on the total weight of the molding composition, of a particulate water-insoluble silicate having a bulk density of more than 100 g/l, which prevents dripping of the composition when in contact with an open flame.
-
-
-
-
-
-
-
-
-