1.
公开(公告)号:DE3001301A1
公开(公告)日:1981-07-23
申请号:DE3001301
申请日:1980-01-16
Applicant: BASF AG
Inventor: FISCHER KARL HEINZ , JOHN GERHARD , ZISSEL ALFRED DIPL CHEM DR
Abstract: Treatment of anionically tanned or retanned leather prior to dyeing with anionic dyes in aq. soln. is carried out by treating the leather with a NH4 salt (I) and an aldehyde or dialdehyde (II) at a pH of 3-8 (pref. 4.5-6). (I) is suitably (NH4)2SO4, NH4Cl or NH4 formate or acetate. (II) is pref. glutaraldehyde. The treatment is pref. effected at 20-70 (esp. 40-50) deg.C for 10-120 (esp. 20-50) min using 50-200%, based on leather wt., of an aq. soln. contg. (I) and (II) in a (I):(II) equiv. ratio of 1-2:1. The amt. of (I) used is pref. equiv. to 1.5-3 wt.% (NH4)2SO4, based on leather wt. The treatment improves the depth of colour achievable with anionic dyes, giving intense even shades with good fastness.
-
公开(公告)号:DE2313063A1
公开(公告)日:1974-09-19
申请号:DE2313063
申请日:1973-03-16
Applicant: BASF AG
IPC: C14C3/18
Abstract: Title prod. obtd. by mixing (a) at least one methylol deriv. of a mononuclear, monohydric phenol of a binuclear phenol (free from condensed rings and contg. one phenolic group on each nucleus), the phenols being free from anionic gps., (b) at least one densation prod. of a naphthalene sulphonic acid with an aldehyde or aldehyde-yielding cpd. and (c) at least one condensation prod. of a phenol-sulphonic acid with urea and formaldehyde (which, if desired, is further condensed with formaldehyde and phenol), in wt. ratio a:b:c = (3-7):(2-6):(0.3-2), dissolving the mixt. in water, subjecting the resulting soln. in mechanical motion for >1 hr. above 30 degrees C and finally removing the water by evaporation.
-