公开(公告)号:DE3039426A1
公开(公告)日:1982-05-27
申请号:DE3039426
申请日:1980-10-18
Applicant: BASF AG
IPC: C08F2/44 , C08F236/04 , C08F236/06 , C08F236/10 , C08F236/12
-
公开(公告)号:DE2911777A1
公开(公告)日:1980-10-09
申请号:DE2911777
申请日:1979-03-26
Applicant: BASF AG
Abstract: In crosslinking profies of C2H4 polymers having density 0.93-0.945 g/cc and melt index 1.5-10 g/10 min., the profiles are heated to 80-120 degrees C before passing under a source of radiation where they are irradiated with electron rays having energy 0.5-3 x 106 e.v. in dosage 50-300 kGy. Electrical charge in profile walls is prevented. Radiation yield is high. Heating increases degree of crosslinking achieved. The hot profiles are pref. quenched with water at 20 degrees C immediately after irradiation.
-