PROCESS FOR MAKING AN AT LEAST PARTIALLY COATED ELECTRODE ACTIVE MATERIAL

    公开(公告)号:CA3145434A1

    公开(公告)日:2021-01-07

    申请号:CA3145434

    申请日:2020-06-17

    Applicant: BASF SE

    Abstract: Process for making an at least partially coated electrode active material wherein said process comprises the following steps: (a) Providing an electrode active material according to general formula Li1+xTM1-xO2, wherein TM is a combination of Ni and Co or Ni and Al and, optionally, Mn, and, optionally, at least one metal selected from Ga, Nb, Ta, Mg, Mo, B, Sn, V, W, Ti and Zr, and x is in the range of from zero to 0.2, (b) treating said electrode active material with at least one carbonyl compound of Co, and (c) treating the material obtained in step (b) with an oxidant.

    PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL

    公开(公告)号:CA3122662A1

    公开(公告)日:2020-07-23

    申请号:CA3122662

    申请日:2020-01-06

    Applicant: BASF SE

    Abstract: Process for making an electrode active material according to general formula Li1+xTM1-xO2, wherein TM is a combination of Ni and Co and Zr and at least one metal selected from Mn and Al, and, optionally, at least one of Mg, Ti, and W, wherein at least 60 mole-% is Ni, referring to the sum of Ni, Co and, if applicable, Mn and Al, and x is in the range of from zero to 0.2, said process comprising the following steps: (a) mixing (A) a mixed oxide or oxyhydroxide of Ni, Co and, if applicable, Mn, (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and (C) at least one oxide or hydroxide or oxyhydroxide of Zr with an average diameter D50 in the range of from 1 to 7 µm, and in compounds (C) that are selected from oxides of Zr, their crystallite size is in the range of from 5 to 20 nm and (b) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000°C.

    10.
    发明专利
    未知

    公开(公告)号:ES3009936T3

    公开(公告)日:2025-03-31

    申请号:ES21778031

    申请日:2021-09-16

    Applicant: BASF SE

    Abstract: Proceso para la fabricación de un material activo de cátodo dopado con fluoruro, en donde dicho proceso comprende los pasos de (a) proporcionar un óxido particulado o (oxi)hidróxido de TM, en donde TM comprende níquel y al menos un metal seleccionado de cobalto y manganeso, en donde dicho óxido particulado o (oxi)hidróxido tiene un diámetro de partícula promedio (D50) en el rango de 3 a 16 μm, (b) proporcionar una fuente de litio que contiene de 0,01 a 2,5 % en peso de fluoruro, uniformemente disperso dentro de dicha fuente de litio, (c) mezclar dicho óxido o (oxi)hidróxido de TM con dicha fuente de litio que contiene fluoruro y, opcionalmente, con una fuente adicional de litio que contiene menos fluoruro, y, opcionalmente, con uno o más dopantes basados en al menos un metal distinto del litio, (d) tratar térmicamente la mezcla obtenida del paso (c). (Traducción automática con Google Translate, sin valor legal)