1.
公开(公告)号:CA3132425A1
公开(公告)日:2020-10-15
申请号:CA3132425
申请日:2020-04-02
Applicant: BASF SE
Inventor: BEIERLING THORSTEN , SCHROEDLE SIMON , SIOSS JAMES , PFISTER DANIELA , KALO BENEDIKT , ERK CHRISTOPH , LONG BRANDON , RIEMANN CHRISTIAN , AMMONS CHRISTINE , TOMOTA YOHKO , HOLZMEISTER PHIL JACK
IPC: C01G51/04 , C01F5/14 , C01G23/04 , C01G25/00 , C01G45/02 , C01G53/00 , C01G53/04 , H01M4/131 , H01M4/1391
Abstract: Process for precipitating a mixed hydroxide of TM wherein TM comprises Ni and at least one of Co and Mn and, optionally, Al, Mg, Zr or Ti, from an aqueous solution of salts of such transition metals or of Al or of Mg, wherein such process is carried out in a stirred vessel and comprises the step of introducing an aqueous solution of alkali metal hydroxide and an aqueous solution of transition metal salts through at least two inlets into said stirred vessel wherein the distance of the locations of introduction of salts of TM and of alkali metal hydroxide is equal or less than 6 times the hydraulic diameter of the tip of the inlet pipe of the alkali metal hydroxide.
-
公开(公告)号:CA3202020A1
公开(公告)日:2022-06-23
申请号:CA3202020
申请日:2021-12-10
Applicant: BASF SE
Inventor: SOMMER HEINO , ERK CHRISTOPH , HAAG JACOB , SIOSS JAMES A , PFISTER DANIELA , MICHEL KATHRIN , GARVE LENNART KARL BERNHARD , BERGNER BENJAMIN JOHANNES HERBERT
Abstract: Process for making an electrode active material wherein said process comprises the follow-ing steps: (a) Providing a hydroxide TM(OH)2 or an oxyhydroxide of TM wherein TM is one or more metals and contains Mn and, optionally, Co, and from 85 to 95 mol% Ni, referring to the sum of Ni, Co and Mn, (b) Drying said hydroxide TM(OH)2 or oxyhydroxide of TM at a temperature in the range of from 400 to 600°C, thereby obtaining an oxide or oxyhydroxide of TM with a residual moisture content of from 200 to 500 ppm, (c) mixing said oxide or oxyhydroxide from step (b) with a source of lithium and with at least one compound of Mg or Al and with at least one compound of Ti or Zr, (d) treating the mixture obtained from step (c) thermally at a temperature in the range of from 550 to 875°C.
-
公开(公告)号:HUE069582T2
公开(公告)日:2025-03-28
申请号:HUE21820288
申请日:2021-12-10
Applicant: BASF SE
-
公开(公告)号:AU2019376818A1
公开(公告)日:2021-05-27
申请号:AU2019376818
申请日:2019-10-30
Applicant: BASF SE
Inventor: BEIERLING THORSTEN , PFISTER DANIELA
IPC: C01G53/00
Abstract: Process for making a nickel composite hydroxide with a mean particle diameter d50 in the range from 3 to 20µm comprising the of combination of (a) an aqueous solution of water-soluble salts of nickel and of at least one of cobalt and manganese, and, optionally, at least one of Al, Mg, B, or transition metals other than nickel, cobalt, and manganese, (b) with an aqueous solution of an alkali metal hydroxide and (c) an aqueous solution of alkali metal (bi)carbonate or ammonium (bi)carbonate in the molar ratio of 0.001 : 1 to 0.04 : 1, and, optionally, (d) an aqueous solution of alkali metal aluminate, in a continuous stirred tank reactor or in a cascade of at least two continuous stirred tank reactors, wherein solutions (b) and (c) are combined first followed by combination with solution (a) and, if applicable, with solution (d), or solutions (a) and (c) are combined first followed by combination with solution (b) and, if applicable, with solution (d), or solutions (a), (b), (c), and, if applicable, (d) are combined simultaneously.
-
公开(公告)号:ES2994047T3
公开(公告)日:2025-01-17
申请号:ES21820288
申请日:2021-12-10
Applicant: BASF SE
Inventor: SOMMER HEINO , ERK CHRISTOPH , HAAG JACOB , SIOSS JAMES A , PFISTER DANIELA , MICHEL KATHRIN , GARVE LENNART KARL BERNHARD , BERGNER BENJAMIN JOHANNES HERBERT
Abstract: 1. Procedimiento para fabricar un material activo de electrodos, en el que dicho procedimiento comprende los siguientes pasos: (a) proporcionar un hidróxido TM(OH)2 o un oxihidróxido de TM, en el que TM es uno o más metales y contiene Mn y, opcionalmente, Co, y de 85 a 95 % en moles de Ni, referido a la suma de Ni, Co y Mn, (b) secar dicho hidróxido TM(OH)2 u oxihidróxido de TM a una temperatura en el intervalo de 400 a 600 °C, obteniendo de este modo un óxido u oxihidróxido de TM con un contenido de humedad residual de 200 a 500 ppm, (c) mezclar dicho óxido u oxihidróxido del paso (b) con una fuente de litio y con al menos un compuesto de Mg o Al y con al menos un compuesto de Ti o Zr, (d) tratar la mezcla obtenida del paso (c) térmicamente a una temperatura en el intervalo de 550 a 875 °C. (Traducción automática con Google Translate, sin valor legal)
-
公开(公告)号:PL4263435T3
公开(公告)日:2025-01-13
申请号:PL21820288
申请日:2021-12-10
Applicant: BASF SE
-
-
-
-
-