1.
公开(公告)号:EP4481856A1
公开(公告)日:2024-12-25
申请号:EP23765789.5
申请日:2023-02-22
Applicant: BYD Company Limited
Inventor: WEN, Xin , GAO, Qingqing , CHEN, Sanzhi , HAO, Rong
IPC: H01M4/58 , H01M10/0525
Abstract: A lithium iron phosphate positive electrode active material, a preparation method thereof, and a lithium-ion battery are provided. The positive electrode active material is formed by mixing a first and a second lithium iron phosphate material. When the volume distribution percentages of the first and second lithium iron phosphate material reach a maximum value, the corresponding particle sizes are D 1 mo µm and D 2 mo µm respectively, and 0.3≤D 1 mo ≤3.2, 1≤D 2 mo ≤5, and D 1 mo 2 mo . The discreteness in particle size distribution of the first and second lithium iron phosphate material is A 1 and A 2 respectively, and 1≤A 1 ≤3, 2≤A 2 ≤4, 4.07 1 x (2.31+D 1 mo ) 2 x (D 2 mo -1.15)
-
2.
公开(公告)号:EP4481854A1
公开(公告)日:2024-12-25
申请号:EP23755708.7
申请日:2023-02-07
Applicant: BYD Company Limited
Inventor: LIU, Jiamin , CHEN, Sanzhi , GAO, Qingqing , HAO, Rong
IPC: H01M4/58 , H01M10/0525
Abstract: A lithium iron phosphate positive electrode active materialand a preparation method thereof are provided. The method includes the following steps: mixing a first lithium iron phosphate material having a particle size D v 50 of 0.3-0.70 µm and a second lithium iron phosphate material having a particle size D v 50 of 0.75-1.5 µm at a certain ratio, such that the particle size of the lithium iron phosphate positive electrode active material meet: 0.95≤0.1 × (D v 90-D v 10)/D v 5+D v 50 × D n 50≤3.3.
-
3.
公开(公告)号:EP4481855A1
公开(公告)日:2024-12-25
申请号:EP23765788.7
申请日:2023-02-22
Applicant: BYD Company Limited
Inventor: WEN, Xin , GAO, Qingqing , CHEN, Sanzhi , HAO, Rong
IPC: H01M4/58 , H01M10/0525
Abstract: A lithium iron phosphate positive electrode active material, a preparation method thereof, and a lithium ion battery are provided. The positive electrode active material is formed by mixing a first and a second lithium iron phosphate material. When the volume distribution percentages of the first and second lithium iron phosphate material reach a maximum value, the corresponding particle sizes are D 1 mo µm and D 2 mo µm respectively; and 0.3≤D 1 mo ≤3.2, 1≤D 2 mo ≤5; and D 1 mo 2 mo . The sphericity of the first and second lithium iron phosphate material are respectively A 1 and A 2 . The first lithium iron phosphate material meets a relation formula below: 0.49 1 mo +0.439A 1 2 mo +2.44A 2 -1.70D 2 mo × A 2
-
-