公开(公告)号:EP4478452A1
公开(公告)日:2024-12-18
申请号:EP23755707.9
申请日:2023-02-07
Applicant: BYD Company Limited
Inventor: LIU, Jiamin , CHEN, Sanzhi , DU, Mengyi , HAO, Rong
IPC: H01M4/136
Abstract: A positive electrode sheet includes a positive electrode current collector and a positive electrode active material layer arranged on at least a surface of the positive electrode current collector. The positive electrode active material layer includes a positive electrode active material, which includes a first lithium iron phosphate material and a second lithium iron phosphate material. When the cumulative volume distribution percentage of the first lithium iron phosphate material is 50%, the particle size is D 1 v 50 µm. When the cumulative volume distribution percentage of the second lithium iron phosphate material is 50%, the particle size is D 2 v 50 µm. where 0.3 ≤ D 1 v 50≤0.95, 1.0≤D 2 v 50≤3.5. When the volume density of the positive electrode active material reaches a maximum value, the particle size is D mo µm, the compaction density of the positive electrode sheet is PD g/cm 3 , and 0.45 ≤ PD x D mo ≤ 12.38.
-
2.
公开(公告)号:EP4481854A1
公开(公告)日:2024-12-25
申请号:EP23755708.7
申请日:2023-02-07
Applicant: BYD Company Limited
Inventor: LIU, Jiamin , CHEN, Sanzhi , GAO, Qingqing , HAO, Rong
IPC: H01M4/58 , H01M10/0525
Abstract: A lithium iron phosphate positive electrode active materialand a preparation method thereof are provided. The method includes the following steps: mixing a first lithium iron phosphate material having a particle size D v 50 of 0.3-0.70 µm and a second lithium iron phosphate material having a particle size D v 50 of 0.75-1.5 µm at a certain ratio, such that the particle size of the lithium iron phosphate positive electrode active material meet: 0.95≤0.1 × (D v 90-D v 10)/D v 5+D v 50 × D n 50≤3.3.
-