公开(公告)号:JP2007161573A
公开(公告)日:2007-06-28
申请号:JP2006329318
申请日:2006-12-06
Applicant: Corning Inc , コーニング インコーポレイテッド
Inventor: DANIEL W HOOTOFU , KELLEY MICHAEL T , ROSETTIE JOHN S , SCHERMERHORN ANDREW P , SHAH KASHYAP H , STONE JOHN III , TANDON PUSHKAR
CPC classification number: C03B19/1423 , C03B19/1453 , C03B19/1476 , C03B2207/66 , C03C3/06 , C03C2201/23 , C03C2201/42
Abstract: PROBLEM TO BE SOLVED: To make doped or undoped pure silica glass material. SOLUTION: (I) At least one stream of glass soot particles comprising silica is provided by a burner 315. (II) At least one stream of the glass soot particles is directed to an essentially planar deposition supporting surface of a deposition substrate 301 rotating about a rotation axis, such that at least one layer of glass soot is deposited on the deposition supporting surface to form a soot preform 303. In the step (II), the burner 315 is allowed to move relative to the deposition supporting surface, and the velocity of the burner 315 relative to the deposition supporting surface is modulated such that in at least half of the area of the layer of glass soot deposited, local soot density variation through at least the center half thickness is low. COPYRIGHT: (C)2007,JPO&INPIT
Abstract translation: 要解决的问题:制备掺杂或未掺杂的纯二氧化硅玻璃材料。 (I)由燃烧器315提供包含二氧化硅的至少一个玻璃烟灰颗粒流。(II)玻璃烟灰颗粒的至少一个流被引导到沉积衬底的基本上平面的沉积支撑表面 301,使得至少一层玻璃烟灰沉积在沉积支撑表面上以形成烟灰预制件303.在步骤(II)中,允许燃烧器315相对于沉积支撑表面移动 并且调节燃烧器315相对于沉积支撑表面的速度,使得在玻璃烟炱层的至少一半区域沉积时,至少中心半部厚度的局部烟灰浓度变化较低。 版权所有(C)2007,JPO&INPIT
-
公开(公告)号:JP2005162610A
公开(公告)日:2005-06-23
申请号:JP2005016570
申请日:2005-01-25
Applicant: Corning Inc , コーニング インコーポレイテッド
Inventor: FOSTER JOHN D , DANIEL W HOOTOFU , LACY CLAUDE L , PENG YING LISA , POWERS DALE R , TARPLEE JENNIFER L , MATTHEWS HAZEL B , MIECZKOWSKI DANIEL , QUINN RICHARD A , WALCZAK WANDA J
IPC: C03B37/12 , C03B37/027 , G02B6/00
CPC classification number: C03B37/02718 , C03B2201/12 , C03B2201/28 , C03B2201/31 , C03B2205/40 , C03B2205/42 , C03B2205/56 , C03B2205/82 , C03B2205/90 , C03B2205/91 , Y02P40/57
Abstract: PROBLEM TO BE SOLVED: To reduce attenuation of a glass optical fiber due to heat aging and Rayleigh scattering in a heat treatment of the fiber. SOLUTION: In the method for forming an optical fiber, the optical fiber is formed by drawing at ≥10 m/sec draw rate from a heated glass source (block 10) and is heat-treated by maintaining the optical fiber within a heated treatment zone for the total resident time of 0.07-0.25 sec, while subjecting the optical fiber to an average cooling rate of 1,200-5,000 °C/sec defined by ä[fiber surface temperature in an inlet zone]-[fiber surface temperature in the outlet zone]}/[the total resident time of the optical fiber in the treatment zone] (block 20). COPYRIGHT: (C)2005,JPO&NCIPI
Abstract translation: 要解决的问题:减少由于热老化引起的玻璃光纤的衰减和在纤维的热处理中的瑞利散射。 解决方案:在形成光纤的方法中,通过从加热的玻璃源(块10)以10m /秒的拉伸速度拉伸而形成光纤,并且通过将光纤维持在 加热处理区,总驻留时间为0.07-0.25秒,同时使光纤的平均冷却速度为ä[进口区的纤维表面温度]定义的1,200-5,000℃/秒 - [纤维表面温度 出口区]} / [处理区中光纤的总驻留时间](方框20)。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:JP2014159369A
公开(公告)日:2014-09-04
申请号:JP2014092417
申请日:2014-04-28
Applicant: Corning Inc , コーニング インコーポレイテッド
Inventor: MICHAEL D BRADY , DANIEL W HOOTOFU
IPC: C03B8/04
CPC classification number: C03B19/1492 , C03B19/1453 , C03B2201/02 , C03B2201/06 , C03B2207/52
Abstract: PROBLEM TO BE SOLVED: To provide a method and an apparatus for producing a thin glass soot sheet which can be taken up and a sintered glass sheet.SOLUTION: Glass soot particles generated from a burner array 105 are deposited on a curved depositional surface 103 of a rotary drum to form a glass soot layer. Then, the glass soot layer is exfoliated from the curved depositional surface 103 to obtain a soot sheet. The soot sheet can be changed into solidified glass by being sintered. The soot sheet and the solidified glass can become sufficiently long and flexible so as to be changed into a roll 117 by being taken up.
Abstract translation: 要解决的问题:提供一种用于生产可被卷取的薄玻璃烟灰板和烧结玻璃板的方法和设备。解决方案:从燃烧器阵列105产生的玻璃烟灰颗粒沉积在弯曲的沉积表面103上 旋转滚筒以形成玻璃烟灰层。 然后,将玻璃烟灰层从弯曲的沉积面103剥离,得到烟灰片。 烟炱片可以通过烧结而变成固化玻璃。 烟炱纸和凝固玻璃可以变得足够长且柔软,以便通过卷取而变成辊117。
-
公开(公告)号:JP2002090568A
公开(公告)日:2002-03-27
申请号:JP2001291920
申请日:2001-09-25
Applicant: CORNING INC
Inventor: ANTOS A JOSEPH , GEORGE E BERKY , DANIEL W HOOTOFU , HOLMES THOMAS G , YANMIN RIU
IPC: G02B6/02 , C03B37/023 , G02B6/036 , H04B10/18 , G02B6/22
Abstract: PROBLEM TO BE SOLVED: To manufacture a dispersion compensation fiber with high negative dispersion value and a large effective area. SOLUTION: A preform to be stretched having a core glass region and a surrounding clad layer is formed and stretched by >=100 g stretching into a waveguide fiber having 125 to 170 μm outer diameter. The waveguide fiber is coated with at least one layer of a polymer material. The coated waveguide fiber is heat treated to substantially remove the residual stress in the coating. The core glass region consists of at least three segments and the surrounding clad layer surrounds the core glass region and has the refractive index nc lower than that of at least a part of the core glass region. The radii r1 and ri and relative refractive index percentages Δ1% and Δi% are selected so as to show negative total dispersion
-
-
-