公开(公告)号:JP2005162610A
公开(公告)日:2005-06-23
申请号:JP2005016570
申请日:2005-01-25
Applicant: Corning Inc , コーニング インコーポレイテッド
Inventor: FOSTER JOHN D , DANIEL W HOOTOFU , LACY CLAUDE L , PENG YING LISA , POWERS DALE R , TARPLEE JENNIFER L , MATTHEWS HAZEL B , MIECZKOWSKI DANIEL , QUINN RICHARD A , WALCZAK WANDA J
IPC: C03B37/12 , C03B37/027 , G02B6/00
CPC classification number: C03B37/02718 , C03B2201/12 , C03B2201/28 , C03B2201/31 , C03B2205/40 , C03B2205/42 , C03B2205/56 , C03B2205/82 , C03B2205/90 , C03B2205/91 , Y02P40/57
Abstract: PROBLEM TO BE SOLVED: To reduce attenuation of a glass optical fiber due to heat aging and Rayleigh scattering in a heat treatment of the fiber. SOLUTION: In the method for forming an optical fiber, the optical fiber is formed by drawing at ≥10 m/sec draw rate from a heated glass source (block 10) and is heat-treated by maintaining the optical fiber within a heated treatment zone for the total resident time of 0.07-0.25 sec, while subjecting the optical fiber to an average cooling rate of 1,200-5,000 °C/sec defined by ä[fiber surface temperature in an inlet zone]-[fiber surface temperature in the outlet zone]}/[the total resident time of the optical fiber in the treatment zone] (block 20). COPYRIGHT: (C)2005,JPO&NCIPI
Abstract translation: 要解决的问题:减少由于热老化引起的玻璃光纤的衰减和在纤维的热处理中的瑞利散射。 解决方案:在形成光纤的方法中,通过从加热的玻璃源(块10)以10m /秒的拉伸速度拉伸而形成光纤,并且通过将光纤维持在 加热处理区,总驻留时间为0.07-0.25秒,同时使光纤的平均冷却速度为ä[进口区的纤维表面温度]定义的1,200-5,000℃/秒 - [纤维表面温度 出口区]} / [处理区中光纤的总驻留时间](方框20)。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:DE60330958D1
公开(公告)日:2010-03-04
申请号:DE60330958
申请日:2003-04-28
Applicant: CORNING INC
Inventor: FOSTER JOHN D , HAWTOF DANIEL W , LACY CLAUDE L , PENG YING LISA , POWERS DALE R , TARPLEE JENNIFER L , MATTHEWS HAZEL B , MIECZKOWSKI DANIEL , QUINN RICHARD A , WALCZAK WANDA J
IPC: C03B37/027 , C03B37/12 , G02B6/00
Abstract: A method for forming a doped optical fiber includes drawing the optical fiber from a doped glass supply at a draw speed and a draw tension sufficient to introduce a heat aging defect in the optical fiber. The optical fiber is treated by maintaining the optical fiber within a treatment temperature range for a treatment time while preferably maintaining the optical fiber within a treatment tension range to reduce the tendency of the optical fiber to increase in attenuation over time following formation of the optical fiber. Apparatus are also provided.
-
公开(公告)号:AU2003231140A1
公开(公告)日:2003-11-17
申请号:AU2003231140
申请日:2003-04-28
Applicant: CORNING INC
Inventor: POWERS DALE R , TARPLEE JENNIFER L , MATTHEWS HAZEL B , MIECZKOWSKI DANIEL , QUINN RICHARD A , WALCZAK WANDA J , FOSTER JOHN D , HAWTOF DANIEL W , LACY CLAUDE L , PENG YING LISA
IPC: C03B37/12 , C03B37/027 , G02B6/00
Abstract: A method for forming a doped optical fiber includes drawing the optical fiber from a doped glass supply at a draw speed and a draw tension sufficient to introduce a heat aging defect in the optical fiber. The optical fiber is treated by maintaining the optical fiber within a treatment temperature range for a treatment time while preferably maintaining the optical fiber within a treatment tension range to reduce the tendency of the optical fiber to increase in attenuation over time following formation of the optical fiber. Apparatus are also provided.
-
-