1.
    发明专利
    未知

    公开(公告)号:DE69725242D1

    公开(公告)日:2003-11-06

    申请号:DE69725242

    申请日:1997-07-29

    Applicant: DAICEL CHEM

    Abstract: Cellulose acetate propionate is a cellulose ester wherein hydroxyl groups of cellulose are substituted with acetyl and propionyl. Cellulose acetate propionate of the present invention has an amorphous index (Am) of not more than 0.4. Cellulose acetate propionate has a degree of acetyl substitution (DSac) and a degree of propionyl substitution (DSpr), which preferably satisfy the formulas (I) to (III), and more preferably satisfy the formulas (I) to (IV). The present invention also provides a solution of cellulose acetate propionate and a cellulose acetate propionate film.

    4.
    发明专利
    未知

    公开(公告)号:DE69725242T2

    公开(公告)日:2004-05-06

    申请号:DE69725242

    申请日:1997-07-29

    Applicant: DAICEL CHEM

    Abstract: Cellulose acetate propionate is a cellulose ester wherein hydroxyl groups of cellulose are substituted with acetyl and propionyl. Cellulose acetate propionate of the present invention has an amorphous index (Am) of not more than 0.4. Cellulose acetate propionate has a degree of acetyl substitution (DSac) and a degree of propionyl substitution (DSpr), which preferably satisfy the formulas (I) to (III), and more preferably satisfy the formulas (I) to (IV). The present invention also provides a solution of cellulose acetate propionate and a cellulose acetate propionate film.

    CELLULOSE ACETATE HAVING EXCELLENT PHYSICAL STRENGTH AND PROCESS FOR PREPARING THE SAME
    8.
    发明公开
    CELLULOSE ACETATE HAVING EXCELLENT PHYSICAL STRENGTH AND PROCESS FOR PREPARING THE SAME 失效
    根据上述制造出色的球技和方法纤维素

    公开(公告)号:EP0769500A4

    公开(公告)日:2001-08-16

    申请号:EP96907721

    申请日:1996-03-29

    Applicant: DAICEL CHEM

    CPC classification number: C08B3/06

    Abstract: Cellulose acetate which can provide moldings improved in the properties, particularly film strength and pliability. The cellulose acetate has an average degree of acetylation of not less than 59 %, a viscosity-average degree of polymerization (DP) of not less than 290, and a viscosity ( eta ), as measured in the form of a concentrated solution thereof by the falling-ball method, satisfying a requirement for the relationship with the viscosity-average degree of polymerization (DP) represented by the following formula (1): 2.814 x 1n(DP) - 11.753