1.
    发明专利
    未知

    公开(公告)号:DE50304190D1

    公开(公告)日:2006-08-24

    申请号:DE50304190

    申请日:2003-05-07

    Applicant: DEGUSSA

    Abstract: Optical cable has a fiber core (1) and fiber cladding (2) adhered with inner and outer external layers (3,4) respectively comprising molding compositions (A and B) having polyamides (I,II). (A) has zero-shear viscosity of 400-6000 Pas at 220 degreesC. (B) further contains flame retardant and impact modifier. Amount of polyamide (II) (a), flame retardant (b) and impact modifier (c) is based on total amount of (a,b,c). An optical cable comprises a polymer optical conductor comprising a fiber core (1) and a single layer or multi-layer fiber cladding (2) which is adhered with inner external layer (3) with a peel force of at least 50 N and an outer external layer (4) adhered to inner external layer with peel force of 30N or less. The inner and outer external layers respectively comprise molding compositions (A and B) containing polyamides (I,II). Polyamide (I) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, and their mixtures, and contains at least 50 micro-eq/g of amino end groups. Composition (A) has zero-shear viscosity of 400-6000 Pas according to ASTM D 4440 at 220 degreesC. The polyamide (II) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, polyetheramide of the above polymers, and their mixtures. Composition (B) further contains 5-45 wt.% of a flame retardant and 0-60 wt.% of an impact modifier. The amount of polyamide (II), flame retardant and impact modifier is based on total amount of polyamide (II), flame retardant and impact modifier.

    Process for the production of a pipe lined with an inliner

    公开(公告)号:AU2014201799A1

    公开(公告)日:2014-10-16

    申请号:AU2014201799

    申请日:2014-03-26

    Abstract: Process for the Production of a Pipe Lined with an Inliner Abstract: A pipe, the interior surface of which has been lined with a thermoplastic layer is produced by a process which comprises the following steps: 5 a) a pipe is provided, b) an inliner made of a thermoplastic material is provided, c) the cross section of the inliner is optionally reduced through exposure to an exterior force, d) the inliner is introduced into the pipe, 10 e) the pipe is heated from outside to a temperature which is higher than the crystallite melting point Tm of the moulding composition, while or after the inliner introduced is expanded radially, so that its exterior surface assumes the internal shape of the pipe, f) the inliner is cooled and is thus fixed. Relative movements between carrier pipe and inliner are thus prevented; the risk of collapse of the inliner is moreover low. The pipe is used for the production of a laid pipeline.

    3.
    发明专利
    未知

    公开(公告)号:AT333102T

    公开(公告)日:2006-08-15

    申请号:AT03010255

    申请日:2003-05-07

    Applicant: DEGUSSA

    Abstract: Optical cable has a fiber core (1) and fiber cladding (2) adhered with inner and outer external layers (3,4) respectively comprising molding compositions (A and B) having polyamides (I,II). (A) has zero-shear viscosity of 400-6000 Pas at 220 degreesC. (B) further contains flame retardant and impact modifier. Amount of polyamide (II) (a), flame retardant (b) and impact modifier (c) is based on total amount of (a,b,c). An optical cable comprises a polymer optical conductor comprising a fiber core (1) and a single layer or multi-layer fiber cladding (2) which is adhered with inner external layer (3) with a peel force of at least 50 N and an outer external layer (4) adhered to inner external layer with peel force of 30N or less. The inner and outer external layers respectively comprise molding compositions (A and B) containing polyamides (I,II). Polyamide (I) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, and their mixtures, and contains at least 50 micro-eq/g of amino end groups. Composition (A) has zero-shear viscosity of 400-6000 Pas according to ASTM D 4440 at 220 degreesC. The polyamide (II) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, polyetheramide of the above polymers, and their mixtures. Composition (B) further contains 5-45 wt.% of a flame retardant and 0-60 wt.% of an impact modifier. The amount of polyamide (II), flame retardant and impact modifier is based on total amount of polyamide (II), flame retardant and impact modifier.

    Polymeric Optical Conductors
    4.
    发明专利

    公开(公告)号:AU2003204916A1

    公开(公告)日:2004-01-22

    申请号:AU2003204916

    申请日:2003-06-24

    Applicant: DEGUSSA

    Abstract: Optical cable has a fiber core (1) and fiber cladding (2) adhered with inner and outer external layers (3,4) respectively comprising molding compositions (A and B) having polyamides (I,II). (A) has zero-shear viscosity of 400-6000 Pas at 220 degreesC. (B) further contains flame retardant and impact modifier. Amount of polyamide (II) (a), flame retardant (b) and impact modifier (c) is based on total amount of (a,b,c). An optical cable comprises a polymer optical conductor comprising a fiber core (1) and a single layer or multi-layer fiber cladding (2) which is adhered with inner external layer (3) with a peel force of at least 50 N and an outer external layer (4) adhered to inner external layer with peel force of 30N or less. The inner and outer external layers respectively comprise molding compositions (A and B) containing polyamides (I,II). Polyamide (I) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, and their mixtures, and contains at least 50 micro-eq/g of amino end groups. Composition (A) has zero-shear viscosity of 400-6000 Pas according to ASTM D 4440 at 220 degreesC. The polyamide (II) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, polyetheramide of the above polymers, and their mixtures. Composition (B) further contains 5-45 wt.% of a flame retardant and 0-60 wt.% of an impact modifier. The amount of polyamide (II), flame retardant and impact modifier is based on total amount of polyamide (II), flame retardant and impact modifier.

    5.
    发明专利
    未知

    公开(公告)号:BR0302122A

    公开(公告)日:2004-08-17

    申请号:BR0302122

    申请日:2003-06-24

    Applicant: DEGUSSA

    Abstract: Optical cable has a fiber core (1) and fiber cladding (2) adhered with inner and outer external layers (3,4) respectively comprising molding compositions (A and B) having polyamides (I,II). (A) has zero-shear viscosity of 400-6000 Pas at 220 degreesC. (B) further contains flame retardant and impact modifier. Amount of polyamide (II) (a), flame retardant (b) and impact modifier (c) is based on total amount of (a,b,c). An optical cable comprises a polymer optical conductor comprising a fiber core (1) and a single layer or multi-layer fiber cladding (2) which is adhered with inner external layer (3) with a peel force of at least 50 N and an outer external layer (4) adhered to inner external layer with peel force of 30N or less. The inner and outer external layers respectively comprise molding compositions (A and B) containing polyamides (I,II). Polyamide (I) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, and their mixtures, and contains at least 50 micro-eq/g of amino end groups. Composition (A) has zero-shear viscosity of 400-6000 Pas according to ASTM D 4440 at 220 degreesC. The polyamide (II) is selected from PA 11, PA 12, PA 1012, PA 1212, copolyamide of at least 2 of PA 11, PA 12, PA 1012, PA 1212 containing not more than 30 mol% of comonomer, polyetheramide of the above polymers, and their mixtures. Composition (B) further contains 5-45 wt.% of a flame retardant and 0-60 wt.% of an impact modifier. The amount of polyamide (II), flame retardant and impact modifier is based on total amount of polyamide (II), flame retardant and impact modifier.