公开(公告)号:ID17539A
公开(公告)日:1998-01-08
申请号:ID972346
申请日:1997-07-07
Applicant: DEGUSSA
Inventor: GORL UDO , LAMBERZ HORST
IPC: C08L19/00 , B60C1/00 , C07F7/08 , C07F7/18 , C08G77/48 , C08K5/548 , C08L7/00 , C08L21/00 , C08L83/08 , C07F , C08L , B60C
Abstract: A mixture (I) of organosilane polysulphides (II) of formula (RO)3Si(CH2)xS-Sz-S(CH2)xSi(OR)3 (1) is new. The mixture contains 20 wt.% or less (1) when z = 2-6 and less than 80 wt.% (1) when z = 0. In (1), R = 1-8C alkyl, preferably 1-3C alkyl; x = 1-8; and z = 0-6. Also claimed are (i) preparation of sulphur, sulphur donor and accelerator vulcanised rubber mixtures containing one or more natural or man-made rubber, silicate, fillers, optionally carbon black and other components, the rubber, fillers, carbon black, optionally plasticiser, anti-oxidants, activators and (I) being mixed at 160-200 degrees C for 3-15 minutes followed by the addition of vulcanisation agents at 60-120 degrees C and mixing for a further 2-10 minutes to yield sheet or strips; (ii) tyre tread compounds with a high silicic acid content containing 4-10 parts weight (pts. wt.) (I) to 100 pts. wt. filler.