Abstract:
PROBLEM TO BE SOLVED: To provide a method for producing a molded product with short-time dimensional stability to heat, and to provide the molded product. SOLUTION: This method for producing the molded product comprises storing the molded product comprising (a) 35-100 wt.% thermoplastic polyester, (b) 0-60 wt.% filler or reinforcing material, (c) 0-20 wt.% elastic rubber for improving an impact strength, (d) 0-30 wt.% flame-retardant agent, (e) 0-20 wt.% synergist and (f) 0-5 wt.% other additives and/or processing aid, for at least 1 hr at 180-250°C. COPYRIGHT: (C)2003,JPO
Abstract:
Preparation of a profiled part having a high degree of short term heat resistance from a molding material containing (wt.%): (a) thermoplastic polyester (35-100); (b) filler or strengthening material (0-60); (c) impact tooth (sic) modified rubber (0-20); (d) flame retarder (0-30); (e) synergists (0-20); and (f) other additives and/or processing aids. The storage of the part for at least one hour at 180-250 degrees C is also new. Independent claims are included for: (1) a profiled part obtained by the process; (2) a profiled part consisting of a plug connection, a spool, a conducting plate, a housing with a conducting plate function, a relay component, a capacitor cup (sic), a cutout, housing components, or capacitor foil.
Abstract:
Preparation of a profiled part having a high degree of short term heat resistance from a molding material containing (wt.%): (a) thermoplastic polyester (35-100); (b) filler or strengthening material (0-60); (c) impact tooth (sic) modified rubber (0-20); (d) flame retarder (0-30); (e) synergists (0-20); and (f) other additives and/or processing aids. The storage of the part for at least one hour at 180-250 degrees C is also new. Independent claims are included for: (1) a profiled part obtained by the process; (2) a profiled part consisting of a plug connection, a spool, a conducting plate, a housing with a conducting plate function, a relay component, a capacitor cup (sic), a cutout, housing components, or capacitor foil.
Abstract:
Preparation of a profiled part having a high degree of short term heat resistance from a molding material containing (wt.%): (a) thermoplastic polyester (35-100); (b) filler or strengthening material (0-60); (c) impact tooth (sic) modified rubber (0-20); (d) flame retarder (0-30); (e) synergists (0-20); and (f) other additives and/or processing aids. The storage of the part for at least one hour at 180-250 degrees C is also new. Independent claims are included for: (1) a profiled part obtained by the process; (2) a profiled part consisting of a plug connection, a spool, a conducting plate, a housing with a conducting plate function, a relay component, a capacitor cup (sic), a cutout, housing components, or capacitor foil.
Abstract:
Preparation of a profiled part having a high degree of short term heat resistance from a molding material containing (wt.%): (a) thermoplastic polyester (35-100); (b) filler or strengthening material (0-60); (c) impact tooth (sic) modified rubber (0-20); (d) flame retarder (0-30); (e) synergists (0-20); and (f) other additives and/or processing aids. The storage of the part for at least one hour at 180-250 degrees C is also new. Independent claims are included for: (1) a profiled part obtained by the process; (2) a profiled part consisting of a plug connection, a spool, a conducting plate, a housing with a conducting plate function, a relay component, a capacitor cup (sic), a cutout, housing components, or capacitor foil.