Abstract:
The present invention relates to a polyethylene resin having a multimodal molecular weight distribution, said resin being further characterized in that it has a density in the range of from about 0.925 g/ccm to about 0.950 g/ccm, a melt index (I 2 ) In the range of from about 0.05 g/10 min to about 5 g/10 min, and in that it comprises at least one high molecular weight (HMW) ethylene interpolymer and at least a low molecular weight (LMW) ethylene polymer, and a composition comprising such resin. Also provided is a shaped article comprising said resin or composition, in particular a pipe.
Abstract translation:本发明涉及具有多峰分子量分布的聚乙烯树脂,所述树脂的特征还在于其密度范围为约0.925g / cm 3至约0.950g / cm 2,熔体指数(I 2)In 约0.05g / 10min至约5g / 10min的范围,其中它包含至少一种高分子量(HMW)乙烯互聚物和至少一种低分子量(LMW)乙烯聚合物,和组合物 包括这种树脂。 还提供了包含所述树脂或组合物,特别是管的成形制品。
Abstract:
Stabilized polyethylene materials which offer an advantageously balanced combination of thermal, mechanical and processing properties, and which maintain their physical properties in chlorinated water environments are disclosed. The materials include an antioxidant system with components to provide extraction resistance in hot water environments and additionally provides oxidation resistance to both chlorine in the water interior of the pipe and oxygen in contact with the pipe's exterior.
Abstract:
The invention provides a composition, comprising at least one high molecular weight ethylene-based interpolymer, and at least one low molecular weight ethylene-based interpolymer, and where the high molecular weight ethylene-based interpolymer has a density less than, or equal to, 0.960 g/cc, and a melt index (I5) less than, or equal to, 1.0 g/10 min; and where the low molecular weight ethylene-based interpolymer has a density less than, or equal to, 0.915 g/cc, and a melt index (I2) greater than, or equal to, 0.4 g/10 min.
Abstract:
Layered, water vapor permeable composite comprise at least one water vapor permeable film layer and at least one substrate layer, the water vapor permeable film (i) comprising at least one film forming polymer and at least one inert porous filler, (ii) having a water vapor transmission rate of at least 1000 g/m 2 /day, and (iii) activated. Representative film forming polymers include ethylene interpolymers, and representative fillers include silica glass beads. One exemplary method of activating the film is to subject it to sufficient pressure such that the glass beads are crushed within the film matrix.
Abstract translation:层状水蒸汽可渗透的复合材料包括至少一个水蒸气可透过膜层和至少一个基底层,该水蒸汽可渗透膜(i)包含至少一种成膜聚合物和至少一种惰性多孔填料,(ii)具有 水蒸汽透过率至少为1000 g / m 2 /天,(iii)活化。 代表性的成膜聚合物包括乙烯互聚物,代表性的填料包括二氧化硅玻璃珠。 激活膜的一个示例性方法是使其受到足够的压力,使得玻璃珠在膜基质内被粉碎。
Abstract:
Stabilized polyethylene materials which offer an advantageously balanced combination of thermal, mechanical and processing properties, and which maintain their physical properties in chlorinated water environments are disclosed. The materials include an antioxidant system with components to provide extraction resistance in hot water environments and additionally provides oxidation resistance to both chlorine in the water interior of the pipe and oxygen in contact with the pipe's exterior.
Abstract:
Layered, water vapor permeable composite comprise at least one water vapor permeable film layer and at least one substrate layer, the water vapor permeable film (i) comprising at least one film forming polymer and at least one inert porous filler, (ii) having a water vapor transmission rate of at least 1000 g/m2/day, and (iii) activated. Representative film forming polymers include ethylene interpolymers, and representative fillers include silica glass beads. One exemplary method of activating the film is to subject it to sufficient pressure such that the glass beads are crushed within the film matrix.
Abstract:
The invention provides a composition, comprising at least one high molecular weight ethylene-based interpolymer, and at least one low molecular weight ethylene-based interpolymer, and where the high molecular weight ethylene-based interpolymer has a density less than, or equal to, 0.960 g/cc, and a melt index (I5) less than, or equal to, 1.0 g/10 min; and where the low molecular weight ethylene-based interpolymer has a density less than, or equal to, 0.915 g/cc, and a melt index (I2) greater than, or equal to, 0.4 g/10 min.
Abstract:
The present invention relates to a polyethylene resin having a multimodal molecular weight distribution, said resin being further characterized in that it has a density in the range of from about 0.925 g/ccm to about 0.950 g/ccm, a melt index (I2) In the range of from about 0.05 g/10 min to about 5 g/10 min, and in that it comprises at least one high molecular weight (HMW) ethylene interpolymer and at least a low molecular weight (LMW) ethylene polymer, and a composition comprising such resin. Also provided is a shaped article comprising said resin or composition, in particular a pipe.