Abstract:
A fire retardant article has a wood-based material with a polyisocyanurate foam article attached thereto, where the polyisocyanurate foam article covers 90% or more of the exposed portion of the wood-based material, has a thickness greater than 1.8 centimeters, a foam core having a density of 28-128 kg/m3, a trimer concentration characterized by at least one of (i) a trimer level in a range of 12-25 weight-percent and (ii) a molar ratio of trimer to sum of urethane and urea in a range of 1-8, a phosphorous concentration of at least 0.3 wt%, a combined concentration of phosphorous and bromine of at least 0.5 wt%, and a vapor permeable and non-combustible facer on at least one primary surface of the foam core.
Abstract:
La invención se refiere a mezclas de interpolímeros o terpolímeros que comprenden residuos de monómero de etileno, residuos de comonómeros que tienen funcionalidad de ácido carboxílico y/o de anhídrido de ácido carboxílico, y residuos de comonómeros que tienen funcionalidad de epóxido. Tales mezclas de interpolímeros o terpolímeros son materiales reticulables adecuados para su uso en aplicaciones de recubrimiento polimérico de cables y requieren poca o ninguna desgasificación después de la reticulación.
Abstract:
Crosslinkable interpolymer blends comprising ethylene monomer residues, residues of comonomers having carboxylic acid and/or carboxylic acid anhydride functionality, and residues of comonomers having epoxide functionality, a peroxide initiator, and optionally a crosslinking catalyst, which, in embodiments, cure to a gel content of greater than (>) 50 wt%within less than 1.5 minutes at 200~C, and require little or no degassing after crosslinking.
Abstract:
A heat-curable structural adhesive includes a non-rubber-modified epoxy resin, a reaction product of a carboxyl- or amine-terminated butadiene polymer or copolymer and a bisphenol F-based epoxy resin, a elastomeric toughener containing capped isocyanate groups, one or more epoxy curing agents a moisture scavenger and a heat activatable catalyst comprising a mixture of a solid or liquid tertiary amine compound that has a boiling temperature of at least 130°C and a novolac resin. The structural adhesive develops excellent bonding properties when cured at moderate temperatures, especially from 120 to 170°C, and in addition performs very well in environmental aging stress testing. The adhesive is particularly good for bonding aluminum to another metal, or bonding aluminum to aluminum.
Abstract:
Interpolymer blends or terpolymers comprising ethylene monomer residues, residues of comonomers having carboxylic acid and/or carboxylic acid anhydride functionality, and residues of comonomers having epoxide functionality. Such interpolymer blends or terpolymers are cross-linkable materials suitable for use in cable polymeric coating applications and require little or no degassing after cross-linking.
Abstract:
composições e métodos para fazer poliolefinas reticuladas com iniciador de peróxido. misturas de interpolímeros reticuláveis compreendendo resíduos de monômeros de etileno, resíduos de comonômeros tendo funcionalidade de ácido carboxílico e/ou anidrido de ácido carboxílico e resíduos de comonômeros tendo funcionalidade epóxido, um iniciador de peróxido e, opcionalmente, um catalisador de reticulação que, em modalidades, cura até um teor de gel superior (>) a 50% em peso em menos de 1,5 minutos a 200 ~c e requer pouca ou nenhuma desgaseificação após reticulação.
Abstract:
An intumescent coating system contains: a polyol component; an isocyanate component; a latent crosslinker having two or more -NACH 2OR groups, where A is selected from a group consisting of H and -CH 2OR, and in each case R is independently selected from a group consisting of hydrocarbons having from one to four carbons, the latent crosslinker being present at a concentration of 30 weight-percent or more based on polyol weight; a boron component at a concentration of one weight-percent or more and 10 weight-percent or less based on total weight of the formulation; and expandable graphite at a concentration of 10 weight-percent or more and 50 weight-percent or less based on the total intumescent system weight; where the polyol and isocyanate are selected so that the reaction product at room temperature of the intumescent coating system components produces a coating having a tensile elongation of 40-percent or more as determined according to ISO 37.
Abstract:
A fire retardant article has a wood-based material with a polyisocyanurate foam article attached thereto, where the polyisocyanurate foam article covers 90% or more of the exposed portion of the wood-based material, has a thickness greater than 1.8 centimeters, a foam core having a density of 28-128 kg/m3, a trimer concentration characterized by at least one of (i) a trimer level in a range of 12-25 weight-percent and (ii) a molar ratio of trimer to sum of urethane and urea in a range of 1-8, a phosphorous concentration of at least 0.3 wt%, a combined concentration of phosphorous and bromine of at least 0.5 wt%, and a vapor permeable and non-combustible facer on at least one primary surface of the foam core.
Abstract:
An article contains a polymeric foam board having a primary surface and an intumescent coating on a primary surface of the polymeric foam board, the intumescent coating containing a polymeric binder, expandable graphite particles, a phosphorous material and a boron-containing compound and wherein the article is free of an object that is in contact with the intumescent coating and that sandwiches the intumescent coating between it and the polymeric foam board and wherein the intumescent coating has a tensile elongation of at least 50 percent and less than 100 percent at 23 degrees Celsius as measured according to ISO 37, has a storage modulus of less than 1 x 106 Pascals at 250 degrees Celsius, is halogen-free, free of sodium silicate, free of polyurea elastomer, and free of formals of pentaerythritol and dipentaerythritol.