公开(公告)号:DE59410124D1
公开(公告)日:2002-07-04
申请号:DE59410124
申请日:1994-11-02
Applicant: ELPATRONIC AG BERGDIETIKON
Inventor: BAESSLER PETER , MAURER URS , MARRIOTT ALAN , OBERHOLZER MARCEL
IPC: B23K9/235 , B23K11/06 , B23K11/08 , B23K11/34 , B23K13/02 , B23K26/00 , B23K26/20 , B23K31/00 , B23K37/04 , B23K37/053 , H05B6/62 , H05B6/80
Abstract: Owing to the fact that sheet edges (3.1, 3.2) to be welded according to the invention are preheated before they are welded, a smaller temperature gradient arises in the material to be welded at the same welding speed during the welding. Consequently, the welding speed can be increased or material which gives poor welding quality at a high temperature gradient can be welded. The preheating is realised, for example, by excitation of the material to be welded at a high frequency.
-
公开(公告)号:DE59712187D1
公开(公告)日:2005-03-03
申请号:DE59712187
申请日:1997-01-24
Applicant: ELPATRONIC AG BERGDIETIKON
Inventor: FREI MATTHIAS , BAESSLER PETER , SCHREIBER PETER , TAIANA PETER
IPC: B65G47/68 , B65G21/20 , B65G47/248 , B65G47/71
Abstract: In order to separate a stream of tin can bodies (8, 9, 10) carried by a conveyor belt (7) at a high speed, a second belt (5) is taken close to the first (7) and there are controlled means (20-26) by which individual tin bodies (11, 13) can be transferred to the second conveyor belt (5). It is thus possible to separate the sequence of tin bodies into two sequences, thus facilitating further processing.
-