公开(公告)号:CH635780A5
公开(公告)日:1983-04-29
申请号:CH701178
申请日:1978-06-27
Applicant: HOECHST AG
Inventor: WORTMANN JOACHIM , SCHOENROGGE BURKHARD , CREMER JOSEPH , DANY FRANZ-JOSEF
-
公开(公告)号:DE4010694A1
公开(公告)日:1991-10-10
申请号:DE4010694
申请日:1990-04-03
Applicant: HOECHST AG , REITEX HYDRAULIK GMBH
-
4.
公开(公告)号:GB2000472B
公开(公告)日:1982-01-20
申请号:GB7828156
申请日:1978-06-28
Applicant: HOECHST AG
Inventor: WORTMANN JOACHIM , SCHOENROGGE BURKHARD , CREMER JOSEPH , DANY FRANZ-JOSEPH
Abstract: Self-extinguishing laminates are made by an improved process, wherein individual layers of a carrier material are impregnated with a thermosetting phenolic resin containing a flame-retardant agent and the impregnated layers are placed one above another and bonded together by compressing them at elevated temperature and under elevated pressure to give a hardened laminate. More specifically, finely pulverulent phosphorus pentanitride as a flame-retarding agent is dispersed in the plasticized or non-plasticized thermosetting phenolic resin, with or without a diluent; the phenolic resin, based on its solid matter content, and the phosphorus pentanitride being used in an approximate ratio by weight of 100:4 to 100:15; and the phenolic resin, based on its solid matter content, and the carrier being used in an approximate ratio by weight of 100:80 to 100:150.
-
公开(公告)号:DE2729527A1
公开(公告)日:1979-01-11
申请号:DE2729527
申请日:1977-06-30
Applicant: HOECHST AG
Inventor: WORTMANN JOACHIM DIPL CHEM DR , SCHOENROGGE BURKHARD , CREMER JOSEPH DIPL CHEM DR , DANY FRANZ-JOSEF DIPL CHEM DR
Abstract: Self-extinguishing laminates are made by an improved process, wherein individual layers of a carrier material are impregnated with a thermosetting phenolic resin containing a flame-retardant agent and the impregnated layers are placed one above another and bonded together by compressing them at elevated temperature and under elevated pressure to give a hardened laminate. More specifically, finely pulverulent phosphorus pentanitride as a flame-retarding agent is dispersed in the plasticized or non-plasticized thermosetting phenolic resin, with or without a diluent; the phenolic resin, based on its solid matter content, and the phosphorus pentanitride being used in an approximate ratio by weight of 100:4 to 100:15; and the phenolic resin, based on its solid matter content, and the carrier being used in an approximate ratio by weight of 100:80 to 100:150.
-
-
公开(公告)号:DE2516119A1
公开(公告)日:1975-11-06
申请号:DE2516119
申请日:1975-04-12
Applicant: HOECHST AG
-
公开(公告)号:DE2436359A1
公开(公告)日:1975-04-10
申请号:DE2436359
申请日:1974-07-27
Applicant: HOECHST AG
-
-
-
-
-
-
-
-