公开(公告)号:ZA824357B
公开(公告)日:1983-04-27
申请号:ZA824357
申请日:1982-06-21
Applicant: HOECHST AG
IPC: C08F30/00 , B41N1/08 , B41N3/03 , C08F30/02 , C08F230/02 , G03F7/004 , C08F , C08L , C09K , D06M , B01F , G03F , B41N
Abstract: The invention relates to a new phosphorus-containing polymer, polyvinylmethylphosphinic acid. It is prepared by polymerization, preferably catalytic, of vinylmethylphosphinic acid or a salt thereof. The new polymer possesses valuable properties and is used, in particular, in the production of offset printing plates which have a light-sensitive layer.
-
-
-
-
-
公开(公告)号:BR7905415A
公开(公告)日:1980-05-20
申请号:BR7905415
申请日:1979-08-22
Applicant: HOECHST AG
Inventor: USBECK G
Abstract: This invention relates to an improvement in the process for anodically oxidizing materials in the form of strips, foils, or sheets composed of aluminum or aluminum alloys in an aqueous electrolyte containing sulfuric acid and phosphoric acid, if appropriate, after a previous mechanical, chemical or electrochemical roughening, the improvement which comprises anodically oxidizing the material in an electrolyte having a concentration of sulfuric acid ranging from about 25 to 150 g per liter, of phosphoric acid ranging from about 10 to 50 g per liter, and of aluminum ions ranging from about 5 to 25 g per liter, at a current density ranging from about 4 to 25 A/dm2, and a temperature ranging from about 25 DEG to 65 DEG C.
-
公开(公告)号:BR7901597A
公开(公告)日:1979-10-16
申请号:BR7901597
申请日:1979-03-15
Applicant: HOECHST AG
Inventor: USBECK G
Abstract: This invention relates to an improvement in the process for anodically oxidizing materials in the form of strips, foils, or plates comprised of aluminum or aluminum alloys in an aqueous electrolyte containing sulfuric acid and aluminum ions, if appropriate, after a foregoing mechanical, chemical, or electrochemical roughening, the improvement comprising anodically oxidizing the material in an electrolyte having a concentration of sulfuric acid in the range of about 25 to 100 g per liter and of aluminum ions in the range of about 10 to 25 g per liter, at a current density in the range of about 4 to 25 A/dm2, and a temperature in the range of about 25 DEG to 65 DEG C.
-
-
公开(公告)号:ZA794419B
公开(公告)日:1980-08-27
申请号:ZA794419
申请日:1979-08-21
Applicant: HOECHST AG
Inventor: USBECK G
Abstract: This invention relates to an improvement in the process for anodically oxidizing materials in the form of strips, foils, or sheets composed of aluminum or aluminum alloys in an aqueous electrolyte containing sulfuric acid and phosphoric acid, if appropriate, after a previous mechanical, chemical or electrochemical roughening, the improvement which comprises anodically oxidizing the material in an electrolyte having a concentration of sulfuric acid ranging from about 25 to 150 g per liter, of phosphoric acid ranging from about 10 to 50 g per liter, and of aluminum ions ranging from about 5 to 25 g per liter, at a current density ranging from about 4 to 25 A/dm2, and a temperature ranging from about 25 DEG to 65 DEG C.
-
-
-
-
-
-
-
-