公开(公告)号:SE7807952L
公开(公告)日:1979-01-20
申请号:SE7807952
申请日:1978-07-18
Applicant: HOECHST AG
Abstract: Aqueous solutions containing an aliphatic amine-N-oxide and a member of a special group of fluorinated surfactants (I) can be used with success as foaming agents for extinguishing liquid hydrocabon fires. (I) has the formula in which RF is a perfluoroalkyl group having from 3 to 16 carbon atoms, R4 is a hydrogen atom, a C1-4 alkyl, cyclohexyl or 2-hydroxyalkyl having from 2 to 6 carbon atoms, R5 is a C1-4 alkyl radical, a cyclohexyl radical or 2-hydroxyalkyl having from 2 to 6 carbon atoms and R6 is a water-solubilizing radical.
-
公开(公告)号:AU513035B2
公开(公告)日:1980-11-06
申请号:AU3375578
申请日:1978-03-02
Applicant: HOECHST AG
Inventor: ADRIAN R , SCHENCK R VON , COX B , WIRTZ P
Abstract: Hardeners of condensed aluminum phosphates for use in water-glass cementing compositions and process for making them. The hardeners consist substantially of a short chain aluminum polyphosphate with a chain length of 3 to 6 and a long chain aluminum polyphosphate with a chain length or more than 40. Quick-setting hardeners contain a high proportion of the short chain component and slow-setting hardeners contain a high porportion of the long chain component.
-
-
-
公开(公告)号:SE7705069A
公开(公告)日:1977-11-04
申请号:SE7705069
申请日:1977-05-02
Applicant: HOECHST AG
Inventor: SCHLEGEL A , WIRTZ P
CPC classification number: A62D1/0078
-
公开(公告)号:AU510222B2
公开(公告)日:1980-06-12
申请号:AU2509177
申请日:1977-05-12
Applicant: HOECHST AG
Inventor: ADRIAN R , SCHENCK R VON , COX B , WIRTZ P
Abstract: Aluminum polyphosphate is made. To this end, solid aluminum hydroxide and polyphosphoric acid which are used in proportions corresponding to an Al:P molar ratio of 1:2.5 to 1:3.5, are introduced separately from, but concurrently with, one another into a reaction zone kept at 150 DEG to 200 DEG C. A moist friable consistency of the starting materials is maintained in the reaction zone by continuously mixing, kneading and comminuting them over substantially the entire period during which they are introduced into the reaction zone. The reaction is continued until a dry sandy powder is formed; and the powder is annealed at 400 DEG to 600 DEG C. over a period sufficient to yield a product undergoing a 0.5 to 1% weight loss on ignition.
-
公开(公告)号:AU509339B2
公开(公告)日:1980-05-08
申请号:AU2477277
申请日:1977-05-02
Applicant: HOECHST AG
Inventor: SCHLEGEL A , WIRTZ P
Abstract: A process is disclosed for deodorizing protein hydrolysates which are used for making air foam. Protein is hydrolyzed by known methods in the absence of heavy metal salts. Then an epoxide is added until blackening occurs when a spot-test is carried out with lead acetate paper.
-
公开(公告)号:ZA781212B
公开(公告)日:1979-03-28
申请号:ZA781212
申请日:1978-03-02
Applicant: HOECHST AG
Abstract: Hardeners of condensed aluminum phosphates for use in water-glass cementing compositions and process for making them. The hardeners consist substantially of a short chain aluminum polyphosphate with a chain length of 3 to 6 and a long chain aluminum polyphosphate with a chain length or more than 40. Quick-setting hardeners contain a high proportion of the short chain component and slow-setting hardeners contain a high porportion of the long chain component.
-
公开(公告)号:BR7801263A
公开(公告)日:1978-11-21
申请号:BR7801263
申请日:1978-03-02
Applicant: HOECHST AG
Abstract: Hardeners of condensed aluminum phosphates for use in water-glass cementing compositions and process for making them. The hardeners consist substantially of a short chain aluminum polyphosphate with a chain length of 3 to 6 and a long chain aluminum polyphosphate with a chain length or more than 40. Quick-setting hardeners contain a high proportion of the short chain component and slow-setting hardeners contain a high porportion of the long chain component.
-
公开(公告)号:SE7705069L
公开(公告)日:1977-11-04
申请号:SE7705069
申请日:1977-05-02
Applicant: HOECHST AG
Inventor: SCHLEGEL A , WIRTZ P
Abstract: A process is disclosed for deodorizing protein hydrolysates which are used for making air foam. Protein is hydrolyzed by known methods in the absence of heavy metal salts. Then an epoxide is added until blackening occurs when a spot-test is carried out with lead acetate paper.
-
-
-
-
-
-
-
-
-