METHOD OF PRODUCING STEEL PIPE
    1.
    发明专利

    公开(公告)号:CA2880661C

    公开(公告)日:2018-05-22

    申请号:CA2880661

    申请日:2012-08-09

    Applicant: JFE STEEL CORP

    Abstract: In a method of producing a steel pipe by shaping a steel plate subjected to edge bending into a cylindrical form through plural times of three-point bending press in widthwise direction and welding a seam thereof to form a non-expanded pipe (1), inserting a pipe expander provided with plural expander tools (2) into an inside of the non-expanded pipe to perform pipe expanding, the expander tools (2) are pushed onto all sites of non-deformation areas (9) in three-point bending press to perform pipe expanding, whereby a steel pipe having an excellent roundness is produced in a high productivity. Moreover, the number of times of the three-point press bending in the above production method is (aN - 1) wherein a is an integer of 1, 2 or the like when the number of the expander tools is N.

    METHOD OF PRODUCING STEEL PIPE
    2.
    发明专利

    公开(公告)号:CA2880661A1

    公开(公告)日:2014-02-13

    申请号:CA2880661

    申请日:2012-08-09

    Applicant: JFE STEEL CORP

    Abstract: In this method for manufacturing a steel pipe, a steel sheet, the edges of which have been bent, is subjected to three-point bending a plurality of times in a widthwise direction so as to form said steel sheet into a cylinder, and after abutting parts are welded together so as to produce a pipe blank (1), a pipe expander provided with a plurality of pieces of expansion hardware (2) is inserted into the pipe blank and the pipe blank is expanded. By expanding the pipe blank with the expansion hardware (2) placed up against each section (9) of the pipe blank that was not deformed by the three-point bending, steel pipes with excellent dimensional precision can be manufactured with high yield. Letting N represent the number of pieces of expansion hardware, the three-point bending is preferably performed aN-1 times (a being an integer, e.g. 1, 2, etc.).

    برامة تشكيل بمكبس ثني

    公开(公告)号:SA516371950B1

    公开(公告)日:2020-12-30

    申请号:SA516371950

    申请日:2016-09-29

    Applicant: JFE STEEL CORP

    Abstract: يتعلّقالاختراعببرامةتشكيل forming punch بمكبسثني bending-press بالكادتتأثربعزمالانثناء bending moment ويمكنالحصولعلىأسطوانةباستدارةٍجيدة. مايتمتوفيرهعبارةعنبرامةتشكيلبمكبسثنيتشتملعلىزوجٍمنالقوالب dies 1 أيسروأيمنيتموضعهماعندفواصلعلىطولاتجاهٍعرضيلمادةصفيحة plate material S لإسنادمادةالصفيحة S عندمكانين؛وبرامة punch 2 متحركةفياتجاهٍللاقترابأوالابتعادعنالقالبين 1 وبشكلٍمتعاقبيكبسمادةالصفيحة S فيالاتجاهالعرضيأثناءإدخالمادةالصفيحةسوياًمعالقالبين 1 لتنفيذالانثناء،حيثتشتملالبرامة 2 علىرأسبرامة punch head 2ألهاسطحمعالجة (تشكيل) K يكونفيتماسٍمعمادةالصفيحة S لكبسمادةالصفيحة S بشكلٍمقعر،ومسندبرامةيتمإمساكهبوصلهبرأسالبرامة 2ألإسنادرأسالبرامة 2أ. علاوةًعلىذلك،يكونلرأسالبرامة 2أسطحمعالجة K لهمركزسطحمعالجة working surface center O يتطابقمعمحورٍ q لمسندالبرامة 2بويتشكلبقوسٍدائريغيرمنتظميكونفيهنصفقطرفيمنطقةمركزيةفيالاتجاهالعرضيهونصفقطرأقصى. شكل 2

    ПУАНСОН ДЛЯ ГИБОЧНОГО ПРЕССОВАНИЯ

    公开(公告)号:RU2650468C2

    公开(公告)日:2018-04-13

    申请号:RU2016138627

    申请日:2015-03-30

    Applicant: JFE STEEL CORP

    Abstract: Изобретениеотноситсяк обработкеметалловдавлением, вчастностик пуансонудлягибкилистовогоматериала. Пуансонвыполненс возможностьюперемещениядляпоследовательногопрессованиялистовогоматериалапоширине. Причемпуансонсодержитголовкус рабочейповерхностью, непосредственноконтактирующейс листовымматериаломдляприданияемувогнутойформы, исоединеннуюс головкойопору. Приэтомрабочаяповерхностьголовкиобразовананеравномернойдугойокружностии максимальнымрадиусомв центральнойобластив направленииширины. Повышаетсяточностьтруббольшогодиаметра. 5 з.п. ф-лы, 9 ил., 1 табл.

    METHOD FOR MANUFACTURING STEEL PIPE

    公开(公告)号:IN990DEN2015A

    公开(公告)日:2015-06-12

    申请号:IN990DEN2015

    申请日:2015-02-06

    Applicant: JFE STEEL CORP

    Abstract: In this method for manufacturing a steel pipe a steel sheet the edges of which have been bent is subjected to three point bending a plurality of times in a widthwise direction so as to form said steel sheet into a cylinder and after abutting parts are welded together so as to produce a pipe blank (1) a pipe expander provided with a plurality of pieces of expansion hardware (2) is inserted into the pipe blank and the pipe blank is expanded. By expanding the pipe blank with the expansion hardware (2) placed up against each section (9) of the pipe blank that was not deformed by the three point bending steel pipes with excellent dimensional precision can be manufactured with high yield. Letting N represent the number of pieces of expansion hardware the three point bending is preferably performed aN-1 times (a being an integer e.g. 1, 2 etc.).

    Uo steel pipe welding bead position detector
    8.
    发明专利
    Uo steel pipe welding bead position detector 有权
    UO钢管焊接钻头位置检测器

    公开(公告)号:JP2011149777A

    公开(公告)日:2011-08-04

    申请号:JP2010010385

    申请日:2010-01-20

    Abstract: PROBLEM TO BE SOLVED: To provide a UO steel pipe welding bead position detector capable of inexpensively and accurately detecting a welding bead position of UO steel pipe.
    SOLUTION: When a UO steel pipe 1 is rotated in a circumferential direction by a turning roll 3 under a condition that a touch roller 6, disposed immediately beneath an axis of the UO steel pipe 1, contacts a circumferential surface of the UO steel pipe 1, an output of a pair of two laser-type displacement gauges 9 changes between before and after a welding bead 2 of the UO steel pipe 1 hurdles the touch roller 6, therefore, the positions of entry and exit sides of the welding bead 2 can be determined from the change of output of the laser-type displacement gauges 9 and the interlevel can be calculated as the position of the welding bead 2. In addition, detection accuracy can be improved by making the position, where an absolute value of the differentiated value of the output in the pair of two laser-type displacement gauges 9 exceeds a predetermined value, at the position of entry or exit side of the welding bead 2.
    COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 要解决的问题:提供能够廉价且准确地检测UO钢管的焊道位置的UO钢管焊道位置检测器。 解决方案:当UO钢管1沿着UO钢管1的轴线正下方设置的接触辊6与UO的圆周表面接触的状态下,通过转动辊3在圆周方向上旋转时, 钢管1中,一对两个激光式位移计量器9的输出在UO钢管1的焊道2之间和之后改变,阻碍了接触辊6,因此,焊接的入射侧和出射侧的位置 可以根据激光型位移计量器9的输出的变化来确定珠子2,并且可以将层叠计算为焊道2的位置。另外,通过使位置可以提高检测精度,其中绝对值 在两个激光位移计量对中的输出的差分值在焊珠2的入口或出口侧的位置超过预定值。(C)2011,JPO&INPIT

    Method of manufacturing steel pipe
    9.
    发明专利
    Method of manufacturing steel pipe 有权
    钢管制造方法

    公开(公告)号:JP2012170977A

    公开(公告)日:2012-09-10

    申请号:JP2011035070

    申请日:2011-02-21

    Abstract: PROBLEM TO BE SOLVED: To provide a method of manufacturing a steel pipe having excellent dimensional accuracy, by which a time required for manufacturing the steel pipe is shortened by reducing the number of times of three point bending, and also the deterioration of characteristics is prevented by performing correction of a shape by cold forming.SOLUTION: After forming the steel plate which is subjected to end bending by performing the three point bending of a plurality of the number of times in the width direction, by inserting a plurality of pipe expanding tools 2 into the inside of the steel pipe 1 the butted part of the steel plate of which is welded, the steel pipe 1 is expanded by bringing the tube expanding tools 2 into contact with all of undeformed parts 9 where deformation caused by the three point bending is not produced.

    Abstract translation: 要解决的问题:提供一种制造具有优异的尺寸精度的钢管的方法,通过减少三点弯曲的次数缩短制造钢管所需的时间,并且还降低了 通过冷成型进行形状修正来防止特性。 解决方案:通过在宽度方向上进行多次多次的三点弯曲来形成经受端部弯曲的钢板之后,通过将多个扩管工具2插入到钢的内部 钢管1的对接部分被焊接,钢管1通过使管膨胀工具2与不产生三点弯曲引起的变形的所有未变形部分9接触而膨胀。 版权所有(C)2012,JPO&INPIT

    O-press die of uoe tube and method for producing uoe tube
    10.
    发明专利
    O-press die of uoe tube and method for producing uoe tube 有权
    U型管的O型压力管和用于生产UOE管的方法

    公开(公告)号:JP2011167765A

    公开(公告)日:2011-09-01

    申请号:JP2011069196

    申请日:2011-03-28

    Inventor: YASUHARA ISAMU

    Abstract: PROBLEM TO BE SOLVED: To provide an O-press die which attains reduction in the production cost of a UOE tube of an intermediate outside diameter and enlargement of a range of produceable diameter of the UOE tube under the conventional expansion condition without degrading work efficiency, in production of the UOE tube of an intermediate outside diameter in a production line of the UOE tube of which the produceable diameter is determined for each size of the O-press die step by step, and to provide a method for producing the UOE tube by using the O-press die.
    SOLUTION: The O-press die for the UOE tube contains upper and lower dies 2A, 2B which are arranged on the upper and lower sides, wherein inner surfaces of the upper and lower dies have a shape formed by cutting a part of upper and lower halves of a transverse oval shape so that the inner surfaces of the upper and lower dies are transverse oval in shape when the gap Go between the upper and lower dies is set to be a predetermined value, and so that the inner surfaces of the upper and lower dies are connected to each other without any step when the upper and lower dies are tightly attached to each other. The UOE tube is produced by using the die.
    COPYRIGHT: (C)2011,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种O型压模,其能够降低中等外径的UOE管的制造成本,并且在常规膨胀条件下扩大UOE管的可产生直径的范围而不降解 在UOE管的生产线中的中间外径的UOE管的生产中,其生产的直径是针对每个O型压模的尺寸逐步确定的,并且提供了一种制造 UOE管采用O型压模。 解决方案:用于UOE管的O形压模包含布置在上侧和下侧上的上模具2A和下模具2B,其中上模具和下模具的内表面具有通过切割一部分 横向椭圆形的上半部和下半部分,使得当上模具和下模具之间的间隙Go设定为预定值时,上模具和下模具的内表面的形状为横向椭圆形,并且使得内表面 当上模具和下模具彼此紧密连接时,上模和下模不间断地连接。 UOE管通过使用模具制造。 版权所有(C)2011,JPO&INPIT