公开(公告)号:US20230332356A1
公开(公告)日:2023-10-19
申请号:US18245596
申请日:2021-09-09
Applicant: KANEKA CORPORATION
Inventor: Asuka FUKUTOME , Yasunori OKADA , Tetsuo OKURA , Kensuke MURASHIMA
Abstract: A laminated article includes a base layer and a coating layer disposed over at least one side of the base layer. The coating layer contains a poly(3-hydroxybutyrate) resin. In a crystalline melting curve obtained by differential scanning calorimetry of the coating layer, the coating layer has at least one peak top temperature (Tma) in the range of 100 to 150° C. and at least one peak top temperature (Tmb) in the range of 150 to 170° C., and the difference between the temperatures Tma and Tmb is 10° C. or more.
-
公开(公告)号:US20240227371A1
公开(公告)日:2024-07-11
申请号:US18561620
申请日:2022-05-16
Applicant: KANEKA CORPORATION
Inventor: Yasunori OKADA , Tetsuo OKURA
CPC classification number: B32B27/10 , B32B27/36 , B32B37/153 , B32B37/156 , B32B2250/03 , B32B2307/31 , B32B2307/7163 , B32B2307/7242 , B32B2367/00 , B32B2439/00
Abstract: A laminated article includes a substrate layer, a gas barrier layer, and a sealant layer. The sealant layer is located on one outermost side of the laminated article. The sealant layer is a resin layer containing poly(3-hydroxybutyrate-co-3-hydroxyhexanoate). In a crystalline melting curve obtained by differential scanning calorimetry of the sealant layer, the sealant layer has at least one top temperature (Tma) in a range of 130 to 160° C.
-
公开(公告)号:US20210301127A1
公开(公告)日:2021-09-30
申请号:US17266676
申请日:2019-08-19
Applicant: KANEKA CORPORATION
Inventor: Tetsuo OKURA
Abstract: Provided is a poly(3-hydroxybutyrate) resin tube including a poly(3-hydroxybutyrate) resin, the tube having a wall thickness of 0.1 to 0.6 mm. The difference between the melting point peak temperature and the melting point peak end temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin is preferably 10° C. or higher. Preferably, production of the tube includes the step of melting a poly(3-hydroxybutyrate) resin in an extruder, then extruding the resin from an annular die, and introducing the resin into water, the annular die temperature being set to a temperature between the melting point peak temperature and the melting point peak end temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin.
-
公开(公告)号:US20230145613A1
公开(公告)日:2023-05-11
申请号:US17907518
申请日:2021-04-09
Applicant: KANEKA CORPORATION
Inventor: Tomoaki HASHIGUCHI , Tetsuo OKURA
CPC classification number: C08L67/04 , F16L11/04 , B29C48/09 , B29C48/919 , B29C48/022 , B29C48/9115 , B29K2105/0088
Abstract: It is an object of an embodiment of the present invention to provide: a poly(3-hydroxybutyrate)-based resin tube which exhibits excellent resistance to repeated bending; and a method for producing the poly(3-hydroxybutyrate)-based resin tube. The object is attained by providing a poly(3-hydroxybutyrate)-based resin tube which contains 95 wt % to 60 wt % of a poly(3-hydroxybutyrate)-based resin and 5 wt % to 40 wt % of an aliphatic-aromatic polyester-based resin and has an elongation at yield point in a tensile test, a tensile elongation of not less than 50% in the tensile test, and a thickness of 0.01 mm to 0.6 mm.
-
公开(公告)号:US20190082719A1
公开(公告)日:2019-03-21
申请号:US16085287
申请日:2017-03-07
Applicant: KANEKA CORPORATION
Inventor: Shunsuke SATO , Tetsuo OKURA
IPC: A23K20/105 , A23K10/30 , A23K50/80
Abstract: Disclosed herein is a feed composition that promotes the growth of zooplankton, enhances the survival rate of zooplankton, is safe, and has little adverse effect on the environment. The feed composition for zooplankton contains PHA.
-
公开(公告)号:US20240001655A1
公开(公告)日:2024-01-04
申请号:US18248015
申请日:2021-10-01
Applicant: KANEKA CORPORATION
Inventor: Wei MIAO , Takeshi SUGIYAMA , Arihiro SAITO , Shun MURASAWA , Tetsuo OKURA
CPC classification number: B32B27/08 , B32B7/02 , B32B27/18 , B32B27/36 , B65D81/051 , B65D65/40 , B32B2250/02 , B32B2307/7376 , B32B2270/00 , B32B2307/31 , B32B2553/00 , B32B2250/244 , C08L67/04
Abstract: A multilayer film includes a first resin layer and a second resin layer. Each of the first and second resin layers contains a poly(3-hydroxyalkanoate) resin. The ratio of the thickness of the first resin layer to the thickness of the second resin layer is from 1.0:0.015 to 1.0:5.0. A heat quantity ΔH of the first resin layer is 30 J/g or more, and a heat quantity ΔH of the second resin layer is 25 J/g or less. The heat quantity ΔH of each of the first and second resin layers is heat of melting over a temperature range of 130 to 190° C.
-
公开(公告)号:US20230235170A1
公开(公告)日:2023-07-27
申请号:US18004557
申请日:2021-06-28
Applicant: KANEKA CORPORATION
Inventor: Tomoaki HASHIGUCHI , Tetsuo OKURA
IPC: C08L67/04
CPC classification number: C08L67/04 , A47G21/18 , C08L2203/18 , C08L2205/025
Abstract: Provided is a resin tube containing a poly(3-hydroxyalkanoate) resin component. The poly(3-hydroxyalkanoate) resin component includes at least two poly(3-hydroxyalkanoate) resins differing in types and/or contents of constituent monomers. A50% fracture energy of the resin tube, as measured by an impact resistance test, is 0.2 J or more.
-
公开(公告)号:US20220267547A1
公开(公告)日:2022-08-25
申请号:US17627356
申请日:2020-07-10
Applicant: KANEKA CORPORATION
Inventor: Asuka FUKUTOME , Tetsuo OKURA , Shunsuke SATO
Abstract: A method for producing a poly(3-hydroxybutyrate) resin-containing composition for melt processing includes: heating a material containing a poly(3-hydroxybutyrate) resin to a temperature equal to or higher than a melting point peak temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin and equal to or lower than a melting point peak end temperature in the differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin, wherein the difference between the melting point peak temperature and the melting point peak end temperature of the poly(3-hydroxybutyrate) resin is 10° C. or more; and extruding the heated material to obtain a composition for melt processing that has a new crystallization peak at a temperature higher than the melting point peak temperature.
-
公开(公告)号:US20250146231A1
公开(公告)日:2025-05-08
申请号:US19014799
申请日:2025-01-09
Applicant: KANEKA CORPORATION
Inventor: Tetsuo OKURA , Shigeru TANAKA , Koki OHTA , Koichi DOHI
Abstract: Impact-cushioning particles contain a poly(3-hydroxybutyrate) resin component. The poly(3-hydroxybutyrate) resin component contains a copolymer component (A), and the copolymer component (A) includes a copolymer (A-1) and/or a copolymer (A-2). The impact-cushioning particles are suitable for use in artificial turf or a paved structure. Copolymer (A-1) is a copolymer of 3-hydroxybutyrate units and other hydroxyalkanoate units, in which the content of the other hydroxyalkanoate units is from 1 to less than 10 mol %. Copolymer (A-2) is a copolymer of 3-hydroxybutyrate units and other hydroxyalkanoate units, in which the content of the other hydroxyalkanoate units is 24 mol % or more.
-
公开(公告)号:US20250066605A1
公开(公告)日:2025-02-27
申请号:US18947386
申请日:2024-11-14
Applicant: KANEKA CORPORATION
Inventor: Tetsuo OKURA
Abstract: Provided is a poly(3-hydroxybutyrate) resin tube including a poly(3-hydroxybutyrate) resin, the tube having a wall thickness of 0.1 to 0.6 mm. The difference between the melting point peak temperature and the melting point peak end temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin is preferably 10° C. or higher. Preferably, production of the tube includes the step of melting a poly(3-hydroxybutyrate) resin in an extruder, then extruding the resin from an annular die, and introducing the resin into water, the annular die temperature being set to a temperature between the melting point peak temperature and the melting point peak end temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin.
-
-
-
-
-
-
-
-
-