Abstract: A biodegradable laminated article includes: a substrate layer; a first thermoplastic resin (A1) layer located on one side of the substrate layer and containing a polyhydroxyalkanoate resin; and a second thermoplastic resin (A2) layer located on the other side of the substrate layer and containing a polyhydroxyalkanoate resin. The weight per unit area of the first thermoplastic resin (A1) layer is from 10 to 200 g/m2, and the weight per unit area of the second thermoplastic resin (A2) layer is from 0.1 to 5 g/m2.
-
公开(公告)号:US20230332356A1
公开(公告)日:2023-10-19
申请号:US18245596
申请日:2021-09-09
Applicant: KANEKA CORPORATION
Inventor: Asuka FUKUTOME , Yasunori OKADA , Tetsuo OKURA , Kensuke MURASHIMA
Abstract: A laminated article includes a base layer and a coating layer disposed over at least one side of the base layer. The coating layer contains a poly(3-hydroxybutyrate) resin. In a crystalline melting curve obtained by differential scanning calorimetry of the coating layer, the coating layer has at least one peak top temperature (Tma) in the range of 100 to 150° C. and at least one peak top temperature (Tmb) in the range of 150 to 170° C., and the difference between the temperatures Tma and Tmb is 10° C. or more.
-
公开(公告)号:US20250144925A1
公开(公告)日:2025-05-08
申请号:US18729994
申请日:2023-01-31
Applicant: KANEKA CORPORATION
Inventor: Kensuke MURASHIMA , Yasunori OKADA
Abstract: A biodegradable laminate includes in order: a layer of a paper substrate (A); a layer of a first thermoplastic resin (B) containing a poly(3-hydroxyalkanoate) resin as a main component; and a layer of a second thermoplastic resin (C) containing a poly(3-hydroxyalkanoate) resin as a main component. The poly(3-hydroxyalkanoate) resin in the first thermoplastic resin (B) has a weight-average molecular weight of 10×104 to less than 35×104, and the poly(3-hydroxyalkanoate) resin in the second thermoplastic resin (C) has a weight-average molecular weight of 45×104 to less than 70×104.
-
公开(公告)号:US20250083426A1
公开(公告)日:2025-03-13
申请号:US18955030
申请日:2024-11-21
Applicant: KANEKA CORPORATION
Inventor: Kensuke MURASHIMA , Itsuki KUSAKABE , Masayuki FUJITA , Yasunori OKADA
Abstract: A laminate includes, in order, a substrate layer (A), a bonding layer (B), and a resin layer (D) containing a poly(3-hydroxyalkanoate) copolymer (C). A glass transition temperature of a total resin material contained in the bonding layer (B) is from 20 to below 90° C., the bonding layer (B) has a weight per square meter of 0.1 to less than 5.0 g/m2, and the resin layer (D) has a thickness of 5 to 100 μm.
-
公开(公告)号:US20240391225A1
公开(公告)日:2024-11-28
申请号:US18707812
申请日:2022-11-10
Applicant: KANEKA CORPORATION
Inventor: Yasunori OKADA , Kensuke MURASHIMA , Tomofumi KUBOTA
Abstract: A laminated article includes at least a substrate layer and a sealant layer. The sealant layer is located on at least one outermost side of the laminated article, and the sealant layer is a resin layer containing a polyhydroxyalkanoate resin component. In differential scanning calorimetry of the polyhydroxyalkanoate resin component, a highest melting peak temperature is 130° C. or higher, and a total crystalline melting enthalpy calculated from all melting peaks is in a range of 20 to 65 J/g.
-
-
-
-