公开(公告)号:JP2005187691A
公开(公告)日:2005-07-14
申请号:JP2003432067
申请日:2003-12-26
Inventor: SHIMOKAWA YOSHIFUMI , MAEDA TOSHIJI , MINOU SEIYA
IPC: C08L101/00 , C08K5/00
Abstract: PROBLEM TO BE SOLVED: To provide a method for manufacturing an amphipatic polymer solution of reduced viscosity and a method for reducing viscosity of the amphipatic polymer solution.
SOLUTION: This method for manufacturing the amphipatic polymer solution of reduced viscosity comprises a step of adding a surfactant in the amphipatic polymer solution with both a hydrophobic group and a hydrophilic group. The method for reducing viscosity of the amphipatic polymer solution comprises an addition of the surfactant in the amphipatic polymer solution with both the hydrophobic group and the hydrophilic group.
COPYRIGHT: (C)2005,JPO&NCIPIAbstract translation: 要解决的问题:提供一种制造具有降低粘度的两亲性聚合物溶液的方法和一种降低两性聚合物溶液粘度的方法。 解决方案:用于制造具有降低粘度的两性聚合物溶液的方法包括在两亲性聚合物溶液中在疏水基团和亲水基团两者之间加入表面活性剂的步骤。 降低两性聚合物溶液粘度的方法包括在具有疏水基团和亲水基团的两亲聚合物溶液中加入表面活性剂。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:JPH11166013A
公开(公告)日:1999-06-22
申请号:JP33545897
申请日:1997-12-05
Applicant: KAO CORP
Inventor: NOJIRI NAOKI , HIRAMATSU SHINOBU , SHIDA JUN , SHIMOKAWA YOSHIFUMI
Abstract: PROBLEM TO BE SOLVED: To provide a method for purifying an ionic polymer efficiently removing low molecular weight impurities containing an ionic residual monomer from an ionic polymer. SOLUTION: Ionic low molecular weight impurities are removed from an aqueous solution containing an ionic polymer and the ionic low molecular weight impurities containing an ionic residual monomer by using a cation exchange resin and/or an anion exchange resin. It is preferable that the weight average molecular weight of the ionic polymer is >=5,000 and the molecular weight of the ionic low molecular weight impurities is
-
公开(公告)号:JPH06124000A
公开(公告)日:1994-05-06
申请号:JP27276292
申请日:1992-10-12
Applicant: KAO CORP
Inventor: NOJIRI NAOKI , YANAGIDA KOICHI , SHIMOKAWA YOSHIFUMI , INATOME HIROSHI , SASAKI MITSUHIRO
IPC: G03G9/087
Abstract: PURPOSE:To prevent aggregation of toner particles in a dispersion medium during polymn., to stabilize the dispersion, and to obtain toner particles having a sharp distribution of particle size. CONSTITUTION:An electrostatic charge image developing toner is obtd. by dispersing a polymerizable monomer compsn. containing a charge controlling agent and a coloring agent in a water-base medium by using a dispersion stabilizer and then effecting suspension polymn. As for the dispersion stabilizer, an inorg. compd. powder which is hardly soluble in water is used. As for a dispersion assistant, a surfactant is used. A part of the inorg. compd. powder which is hardly soluble in water and a part or whole of the surfactant are added when the dispersion is initiated, and the rest of the inorg. compd. powder and surfactant, or the rest of the inorg. compd. powder is added during the dispersion or after the dispersion.
-
公开(公告)号:JP2014012793A
公开(公告)日:2014-01-23
申请号:JP2012151420
申请日:2012-07-05
Inventor: SHIMOKAWA YOSHIFUMI , OKAZAKI FUMIO , FUJINO KEISUKE
Abstract: PROBLEM TO BE SOLVED: To provide a water-insoluble polymer builder having both excellent detergency and anti-resoiling performance, and a method for producing the same.SOLUTION: The water-insoluble polymer builder comprises a copolymer of an organic carboxylic acid monomer and a crosslinkable monomer. The ratio (d2/d1) of a volume-average particle diameter (d2) in a state swollen with water to a volume-average particle diameter (d1) in a dried state of the water-insoluble polymer builder is 5-100.
Abstract translation: 要解决的问题:提供具有优异的去污力和抗回复性能的水不溶性聚合物助洗剂及其制备方法。溶液:水不溶性聚合物助洗剂包括有机羧酸单体和 可交联单体。 在水不溶性聚合物助洗剂的干燥状态下,在水中膨胀的状态下的体积平均粒径(d2)与体积平均粒径(d1)的比率(d2 / d1)为5-100。
-
公开(公告)号:JP2010150444A
公开(公告)日:2010-07-08
申请号:JP2008331783
申请日:2008-12-26
Inventor: NAKA YOSHIHITO , SHIMOKAWA YOSHIFUMI
IPC: C08F20/28 , C04B24/26 , C04B103/30 , C08F8/00
Abstract: PROBLEM TO BE SOLVED: To provide a method for stably producing an aqueous solution containing a polymer comprising a structural unit containing ≥90 wt.% structural unit derived from hydroxyethyl acrylate without generating gel-like materials.
SOLUTION: The method for producing the aqueous solution containing the polymer comprising the structural unit containing ≥90 wt.% structural unit derived from monomers expressed by the following formula (1) is provided. The method for producing the aqueous polymer solution is to polymerize the aqueous solution containing the monomer expressed by formula (1) by using a peroxide-based initiator, subsequently to neutralize the solution by using a particular neutralization agent under agitation by a particular agitation power: H
2 C=CHCOOCH
2 CH
2 OH... formula (1).
COPYRIGHT: (C)2010,JPO&INPITAbstract translation: 要解决的问题:提供一种稳定地制备含有聚合物的水溶液的方法,所述聚合物包含含有≥90重量%的衍生自丙烯酸羟乙酯的结构单元的结构单元,而不产生凝胶状材料。 解决方案:提供含有含有由下式(1)表示的单体衍生的含有≥90重量%结构单元的结构单元的聚合物的水溶液的制备方法。 制备聚合物水溶液的方法是通过使用过氧化物引发剂使含有由式(1)表示的单体的水溶液聚合,然后通过特定的搅拌动力在搅拌下使用特定的中和剂中和溶液: C(CH 2)2 CH 2 OCH 2 CH 2 CH 2 CH 2 OCH 2 CH 2 CH 2 OCH 2 CH 2 CH 2 OCH 2 CH 2 OCH 2 CH 2 CH 2 OH。 版权所有(C)2010,JPO&INPIT
-
6.
公开(公告)号:JP2010138278A
公开(公告)日:2010-06-24
申请号:JP2008315657
申请日:2008-12-11
Inventor: KURATA MINORU , SHIMOKAWA YOSHIFUMI
Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a water-absorbing resin composite material having excellent performance by easily and uniformly treating a surface in the case of adding inorganic particles to a water-absorbing resin. SOLUTION: The method for producing the water-absorbing resin composite material comprises addition of the inorganic particles to the water-absorbing resin by using a mechanical stirring mixer, wherein mixing is carried out by setting the product of circumferential velocity (m/sec) of tip end of the stirring blade of the mixer and the mixing time (second) to 25-480 m. COPYRIGHT: (C)2010,JPO&INPIT
Abstract translation: 解决问题:提供一种在将无机颗粒添加到吸水性树脂的情况下,通过容易且均匀地处理表面来制造具有优异性能的吸水性树脂复合材料的方法。 解决方案:制造吸水性树脂复合材料的方法包括通过使用机械搅拌混合器将无机颗粒添加到吸水性树脂中,其中通过将圆周速度乘积(m / 秒),搅拌时间(秒)为25-480米。 版权所有(C)2010,JPO&INPIT
-
公开(公告)号:JP2007176806A
公开(公告)日:2007-07-12
申请号:JP2005373952
申请日:2005-12-27
Inventor: KURATA MINORU , SHIMOKAWA YOSHIFUMI , MAEDA TOSHIJI , KUBO MAKOTO
IPC: C07F9/09
Abstract: PROBLEM TO BE SOLVED: To provide a method by which side reactions are suppressed and a polymerizable phosphoric ester with a high content of an active ingredient is produced.
SOLUTION: The method for producing at least one kind selected from polymerizable phosphoric esters comprises adding phosphoric acid anhydride to an alcohol containing an unsaturated group. The temperature when adding the phosphoric acid anhydride is within the range of 40-90°C. The phosphoric acid anhydride is added for a time not longer than t
max represented by the following formula (V) t
max =1.835×10
-7 exp[5864/(T+273.15)] (V) (wherein, t
max represents the maximum value of addition time h of the phosphoric acid anhydride; and T represents the temperature °C when the phosphoric acid anhydride is added).
COPYRIGHT: (C)2007,JPO&INPITAbstract translation: 要解决的问题:提供抑制副反应的方法,并且产生具有高含量活性成分的可聚合磷酸酯。 解决方案:选自可聚合磷酸酯中的至少一种的制备方法包括向含有不饱和基团的醇中加入磷酸酐。 加入磷酸酐时的温度在40〜90℃的范围内。 加入磷酸酐一段时间不超过由下式(V)表示的t SB S = 1.835×10 SP = -7 / SP > exp [5864 /(T + 273.15)](V)(其中,t
max SB>表示磷酸酐的添加时间h的最大值; T表示当磷酸 加入酸酐)。 版权所有(C)2007,JPO&INPIT -
公开(公告)号:JP2005187692A
公开(公告)日:2005-07-14
申请号:JP2003432068
申请日:2003-12-26
Inventor: SHIMOKAWA YOSHIFUMI , MAEDA TOSHIJI , MINOU SEIYA
IPC: C08F6/10
Abstract: PROBLEM TO BE SOLVED: To provide a method for producing an amphiphatic polymer solution having reduced organic solvent content from a polymer solution having high viscosity and foaming property and provide a method for decreasing the organic solvent content of the amphiphatic polymer solution.
SOLUTION: The method for producing an amphiphatic polymer solution having decreased organic solvent content comprises the addition of water before and/or during the removal of the organic solvent by distillation from the amphiphatic polymer solution containing the organic solvent. The distillation of the organic solvent in the amphiphatic polymer solution containing the organic solvent is carried out by adding water before and/or during the removal of the organic solvent by distillation and continuously evaporating the solvent with a thin-film evaporator under a condition to keep the viscosity of the amphiphatic polymer solution to ≤8,000 mPas.
COPYRIGHT: (C)2005,JPO&NCIPIAbstract translation: 要解决的问题:提供一种由具有高粘度和起泡性的聚合物溶液制备具有降低的有机溶剂含量的二脂族聚合物溶液的方法,并且提供了降低所述两亲性聚合物溶液的有机溶剂含量的方法。 解决方案:生产具有降低的有机溶剂含量的亲水性聚合物溶液的方法包括在从含有机溶剂的两性聚合物溶液中蒸馏除去有机溶剂之前和/或期间添加水。 有机溶剂在含有有机溶剂的两性聚合物溶液中的蒸馏通过在蒸馏除去有机溶剂之前和/或期间通过加入水进行,并在薄膜蒸发器下在保持条件下连续蒸发溶剂 两亲性聚合物溶液的粘度为≤8,000mPas。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:JP2003300931A
公开(公告)日:2003-10-21
申请号:JP2002109255
申请日:2002-04-11
Inventor: SHIMOKAWA YOSHIFUMI , MINOU SEIYA , UKIANA TOSHINAO , SATO HARUYUKI , KOYANAGI KOJI
Abstract: PROBLEM TO BE SOLVED: To provide a method for stably producing an unsaturated carboxylic acid ester by effectively suppressing gel formation. SOLUTION: This method for producing the unsaturated carboxylic acid by performing an esterification reaction of an unsaturated carboxylic acid with an alcohol is provided by introducing oxygen gas into the reaction system so as to satisfy a specific relationship of the water content of stock raw materials with a flowing amount of oxygen gas. COPYRIGHT: (C)2004,JPO
Abstract translation: 待解决的问题:提供通过有效抑制凝胶形成来稳定生产不饱和羧酸酯的方法。 解决方案:通过将不饱和羧酸与醇的酯化反应进行制备不饱和羧酸的方法是通过将氧气引入反应体系中以满足原料的水含量的具体关系 具有流动量的氧气的材料。 版权所有(C)2004,JPO
-
公开(公告)号:JPH09255704A
公开(公告)日:1997-09-30
申请号:JP9761796
申请日:1996-03-26
Applicant: KAO CORP
Inventor: NAKAO MASAKAZU , MATSUYAMA KAZUO , SHIMOKAWA YOSHIFUMI , SHIDA JUN
IPC: C08F2/00 , C08F2/34 , C08F4/40 , C08F20/06 , C08F20/10 , C08F20/34 , C08F20/56 , C08F28/00 , C08F28/02 , C08F30/02 , C08F120/04
Abstract: PROBLEM TO BE SOLVED: To prevent the polymn. in a spraying machine in a process for producing a polymer by the spray polymn. of a monomer soln. using a redox polymn. initiator, to provide a process for producing a polymer enabling long-time continuous running and quality uniformization, and provide a nozzle for spray polymn. SOLUTION: In this process for producing a polymer wherein a mixture of a monomer component and a redox polymn. initiator is sprayed with a nozzle to be subjected to polymn. in a gas phase, a nozzle having two or more feed supply ports, two or more mixing zones, and two or more spray gas supply ports is used to supply the reducing and oxidizing agents constituting the initiator through respective supply ports; and the monomer component and the initiator are mixed in the mixing zone and sprayed to be subjected to polymn. in a gas phase.
-
-
-
-
-
-
-
-
-