Abstract:
PROBLEM TO BE SOLVED: To provide a method for manufacturing a surface reformed particle where the surface reforming ratio is highly maintained and the necessary time is shortened. SOLUTION: The method includes (1) process to obtain an inorganic particle water-sol containing a dispersant by dispersing a dispersant in the inorganic particle water-sol, (2) process to obtain a dried powder by drying the inorganic particle water-sol using freeze-drying or the like, (3) process to obtain an organic solvent sol by dispersing the dried powder in an organic solvent, and (4) surface reforming agent treatment process to disperse a surface reforming agent in the organic solvent sol. COPYRIGHT: (C)2010,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a resin composite material which has high mechanical characteristics such as high modulus, impact resistance and surface smoothness, and also has a low linear expansion coefficient. SOLUTION: The particle composite resin composition comprises: an aluminum oxide particle which is surface-treated with an organic acid having sulfonic group and phosphate group or silane coupling agent and has an aspect ratio of 5 to 500; a condensation polymer; a non-condensation polymer composed of main chains of carbon-carbon bonding; and a polymer having at least one selected from a group including carboxylic acid anhydride group and carboxyl group in the molecular structure. COPYRIGHT: (C)2009,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a resin composition excellent both in mechanical properties and in transparency. SOLUTION: The resin composition is obtained by compounding at least two kinds of metal oxides with different aspect ratios with a thermoplastic resin. In at least two kinds of the metal oxides, the length of the long axis of the metal oxide having the longest long axis is 20-700 nm and the length of the short axis of it is 1-10 nm. Its aspect ratio is 5-100. COPYRIGHT: (C)2007,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To obtain inorganic particulates of a nanoorder level whose dispersibility into a resin is excellent, and to provide a resin composite having a high elastic modulus and a low linear expansion coefficient using the same. SOLUTION: In the metal oxide particle composite, phosphoric acid or phosphoric acid ester and aromatic sulfonic acids are chemically bonded to metal oxide particles. The resin composite is composed of the metal oxide particle composite and a resin. COPYRIGHT: (C)2007,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a resin composition having excellent mechanical strength while holding transparency. SOLUTION: The resin composition is obtained as follows. The surfaces of metal oxide particles are treated with an acid or a base and the surfaces of the metal oxide particles are then treated with a surface treating agent to provide a metal oxide particle composite. The resultant metal oxide particle composite is then compounded with a resin. COPYRIGHT: (C)2007,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a polymer nano-composite containing a surface modified nano-filler excluding bad influences of dysfunction such as filler aggregation, deterioration of molecular weight and discoloring by a surface modifier such as a coupling agent which cannot chemically be combined with the nano-filler, a condensate, etc., formed by mutually combining the surface modifier. SOLUTION: The polymer nano-composite is produced as follows. The nano-filler is dispersed in a solvent and a prescribed modifier is added to modify the surface. The solvent containing the nano-filler is directly washed and the free modifier present as a residual component of the modifier in the solvent is removed to afford a surface modified nano-filler. The resultant surface modified nano-filler is compounded and dispersed in a prescribed organic polymer. COPYRIGHT: (C)2007,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide a thermoplastic resin containing surface coated oxide particles, allowing improvement in impact resistance, elastic modulus and heat dimensional stability. SOLUTION: It is achieved by a resin composition consisting of: oxide particles; a long chain compound having a plurality of chemical binding capacities for the surfaces of the oxide particles; and the thermoplastic resin. COPYRIGHT: (C)2009,JPO&INPIT
Abstract:
PROBLEM TO BE SOLVED: To provide alumina particles usable as a filler for a thermoplastic resin, and to provide a thermoplastic resin composition having various improved properties such as strength, modulus of elasticity and heat resistance. SOLUTION: When the alumina particles are modified by bringing the alumina particle into contact with an organic compound, the alumina particles are brought into contact with the organic compound within a temperature range of 100-400°C, whereby the surface active groups of the alumina particles are satisfactorily deactivated so as to exert the effect as a filler when it is compounded in the predetermined thermoplastic resin, and thus a thermoplastic resin composition having various improved properties such as strength, modulus of elasticity and heat resistance can be obtained. COPYRIGHT: (C)2008,JPO&INPIT