Process for hot briqueting granular sponge iron

    公开(公告)号:AU1191097A

    公开(公告)日:1997-07-03

    申请号:AU1191097

    申请日:1996-12-05

    Applicant: OUTOTEC OYJ

    Abstract: PCT No. PCT/EP96/05446 Sec. 371 Date Dec. 21, 1998 Sec. 102(e) Date Dec. 21, 1998 PCT Filed Dec. 5, 1996 PCT Pub. No. WO97/21840 PCT Pub. Date Jun. 19, 1997The granular sponge iron is supplied to a roller press at temperatures of 600 to 850 DEG C. for molding the hot briquets. There is produced a strip structure of sponge iron containing formed hot briquets, which are arranged at a distance from each other. By smashing the strip structure, the hot briquets are separated from each other, so that fragments of the strip structure are obtained. The hot briquets and at least part of the fragments are cooled to temperatures in the range from 20 to 400 DEG C., and the cooled briquets and fragments are passed through a rotary drum. In the rotary drum, fine-grained fines of the briquets and fragments are produced. Subsequently, these fines are separated from the briquets and fragments, as they exhibit a pyrophoric behavior.

    Method for producing iron carbide from granulated sponge iron

    公开(公告)号:AU7212398A

    公开(公告)日:1998-11-13

    申请号:AU7212398

    申请日:1998-03-28

    Applicant: OUTOTEC OYJ

    Abstract: Process for producing Iron carbide wherein, in a first stage, Iron ore is reduced to sponge iron using a reducing gas containing at least 90% hydrogen, on a nitrogen-free basis, to produce a sponge iron having a carbon content of less than 1% wt.; then in a second stage the sponge iron is fluidized at a temperature of 500 to 800° C. with a methane-containing fluidizing gas in a fluidized bed reactor wherein the water content of the gas in the reactor is not more than 1.5% wt., to produce a product wherein at least 85% of the iron content is in the form of Fe3C.

    УСТАНОВКА ДЛЯ ПРОИЗВОДСТВА НИЗКОТЕМПЕРАТУРНОГО КОКСА

    公开(公告)号:EA013087B1

    公开(公告)日:2010-02-26

    申请号:EA200800694

    申请日:2003-12-01

    Applicant: OUTOTEC OYJ

    Abstract: Настоящееизобретениеотноситсяк установкедляпроизводстванизкотемпературногококса, вкоторойгранулированныйугольи, возможно, другиетвердыематериалынагреваютдотемпературыот 700 до 1050°Св реакторес псевдоожиженнымслоем (2) спомощьюкислородсодержащегогаза. Сцельюулучшенияиспользованияэнергиипредлагаетсявводитьпервыйгазилигазовуюсмесьснизупоменьшеймеречерезоднугазоподводящуютрубу (3) взонусмесительногопространства (8) реактора (2), причемэтагазоподводяющаятруба (3), покрайнеймере, частичноокруженастационарнымкольцевымпсевдоожиженнымслоем (6), которыйпсевдоожижаетсяподводимымпсевдоожижающимгазом. Объемныескоростипервогогазаилигазовойсмесии псевдоожижающегогазадлякольцевогопсевдоожиженногослоя (6) регулируютсятакимобразом, чтобычислаФрудадлячастицв газоподводящейтрубе (3) составлялиот 1 до 100, вкольцевомпсевдоожиженномслое (6) - от 0,02 до 2 ив смесительномпространстве (8) - от 0,3 до 30 (фиг. 1).

    Method and plant for the heat treatment of solids containing iron oxide

    公开(公告)号:AU2003292233B2

    公开(公告)日:2009-07-09

    申请号:AU2003292233

    申请日:2003-12-12

    Applicant: OUTOTEC OYJ

    Abstract: A plant for the heat treatment of solids containing iron oxide includes a fluidized bed reactor. The reactor includes at least one gas supply tube at least partly surrounded by an annular chamber in which a stationary annular fluidized bed is located, and a mixing chamber being located above the upper orifice region of the at least one gas supply tube. The gas flowing through the at least one gas supply tube entrains solids from the stationary annular fluidized bed-into the mixing chamber when passing through the upper orifice region of the at least one gas supply tube.

    УСТАНОВКА ДЛЯ ТЕРМИЧЕСКОЙ ОБРАБОТКИ ТВЕРДЫХ МАТЕРИАЛОВ, СОДЕРЖАЩИХ ОКСИД ЖЕЛЕЗА, С ИСПОЛЬЗОВАНИЕМ РЕАКТОРА С ПСЕВДООЖИЖЕННЫМ СЛОЕМ

    公开(公告)号:EA013278B1

    公开(公告)日:2010-04-30

    申请号:EA200800690

    申请日:2003-12-01

    Applicant: OUTOTEC OYJ

    Abstract: Настоящееизобретениеотноситсяк установкедлятермическойобработкитвердыхматериалов, содержащихоксиджелеза, накотороймелкозернистыетвердыематериалынагреваютсядотемпературыот 700 до 1150°Св реакторес псевдоожиженнымслоем (8). Сцельюулучшенияиспользованияэнергиипредлагаетсявводитьпервыйгазилигазовуюсмесьснизучерезпоменьшеймереоднугазоподводящуютрубу (9) вобластьсмесительногопространства (15) реактора (8), причемгазоподводящаятруба (9), покрайнеймере, частичноокруженастационарнымкольцевымпсевдоожиженнымслоем (12), которыйпсевдоожижаетсяподаваемымпсевдоожижающимгазом. Объемныескоростипервогогазаилигазовойсмесии псевдоожижающегогазадлякольцевогопсевдоожиженногослоярегулируюттакимобразом, чтобычислоФрудадлячастицв газоподводящейтрубе (9) былов пределахот 1 до 100, вкольцевомпсевдоожиженномслое (12) от 0,02 до 2 ив смесительномпространстве (15) от 0,3 до 30.