Abstract:
Provided is an electrical steel sheet comprising: a groove formed in a surface of a steel sheet, wherein the groove includes a bottom surface, a first side surface extending from the bottom surface, and a second side surface extending from the bottom surface in opposite to the first side surface, wherein the groove has a depth from the surface to the bottom surface, a width in a rolling direction of the steel sheet, and a length in a width direction of the steel sheet, and wherein the groove is formed through laser-irradiation and removal of melt produced by the laser-irradiation; an opening defined by the bottom surface, the first side surface and the second side surface; and a first solidification portion formed on the first side surface of the groove. The first solidification portion is formed by a solidification of part of the melt produced from the laser-irradiation.
Abstract:
A method for manufacturing an electrical steel sheet is provided. The method for manufacturing an electrical steel sheet includes forming a groove having first and second side surfaces and a bottom surface by melting a surface of a steel sheet by laser irradiation, and forming an opening by removing melted byproducts of the steel sheet formed on the first and second side surfaces and the bottom surface through air blowing or suctioning to expose at least one surface of the first side surface, the second side surface, and the bottom surface in the forming of the groove.
Abstract:
An oriented electrical steel sheet and a method of manufacturing the same are provided, and in a method of manufacturing an oriented electrical steel sheet including processes of producing a hot rolled plate by hot rolling a steel slab, performing or omitting hot rolled plate annealing, performing cold rolling, performing decarburization and nitride annealing, and performing final high temperature annealing, the decarburization and nitride annealing process is performed in a dew point range of 35-55° C., and in the final annealing process, a glassless additive including MgO is applied.
Abstract:
Provided is a grain-oriented electric steel sheet having superior magnetic property and to a grain-oriented electric steel sheet including 2.0 to 4.5 weight % of Si, 0.001 to 0.10 weight % of C, 0.010 weight % or lower of Al, 0.08 weight % or lower of Mn, 0.005 weight % or lower of N, 0.002 to 0.050 weight % of S, the remainder being Fe and other unavoidable impurities. The steel sheet having been subjected to secondary recrystallization using at least any one of grain boundary-segregated elementary S and an FeS precipitate as a grain growth inhibitor.
Abstract:
Provided is a grain-oriented electric steel sheet having superior magnetic property and to a grain-oriented electric steel sheet including 2.0 to 4.5 weight % of Si, 0.001 to 0.10 weight % of C, 0.010 weight % or lower of Al, 0.08 weight % or lower of Mn, 0.005 weight % or lower of N, 0.002 to 0.050 weight % of S, the remainder being Fe and other unavoidable impurities. The steel sheet having been subjected to secondary recrystallization using at least any one of grain boundary-segregated elementary S and an FeS precipitate as a grain growth inhibitor.