TI02 SLURRY STABILIZATION
    2.
    发明专利

    公开(公告)号:CA2206162A1

    公开(公告)日:1997-11-28

    申请号:CA2206162

    申请日:1997-05-26

    Abstract: A stable aqueous pigment slurry and a process for preparing same. The slurry contains about 50 to 90 wt.%, based on the weight of the slurry, of a pigment such as titanium dioxide and about 0.2 to 3.0 wt.%, based on the weight of the slurry, of a smectite clay such as bentonite, hectorite or montmorillonite. Preferably, the pigment slurry also contains about 0.1 to 2.0 wt.%, based on the weight of the slurry, of a dispersant. The process involves admixing a pigment slurry and a smectite clay slurry and preferably also the dispersant by milling the three components together under high shear conditions.

    TI02 SLURRY STABILIZATION
    3.
    发明专利

    公开(公告)号:CA2206162C

    公开(公告)日:2002-03-12

    申请号:CA2206162

    申请日:1997-05-26

    Abstract: A stable aqueous pigment slurry and a process for preparing same. The slurry contains about 50 to 90 wt.%, based on the weight of the slurry, of a pigment such as titanium dioxide and about 0.2 to 3.0 wt.%, based on the weight of the slurry, of a smectite clay such as bentonite, hectorite or montmorillonite. Preferably, the pigment slurry also contains about 0.1 to 2.0 wt.%, based on the weight of the slurry, of a dispersant. The process involves admixing a pigment slurry and a smectite clay slurry and preferably also the dispersant by milling the three components together under high shear conditions.

    5.
    发明专利
    未知

    公开(公告)号:BR9610674A

    公开(公告)日:1999-07-06

    申请号:BR9610674

    申请日:1996-09-27

    Abstract: Unusually high loading levels of smectite minerals are found to provide excellent pigment spacing in aqueous-based coatings, as will enable desired improved hiding, thereby extending the pigment. The level of smectite used in accordance with the invention is sufficiently high that the high gelling efficiency smectites previously used as thixotropes would be inappropriate, and would yield viscosities so high as to render the aqueous coating composition lacking in desired flowability properties. Thus in accordance with the present invention, there is mixed with the aqueous carrier and pigment at least 0.5% by weight of the total composition, of a particulate water swellable smectite which has a gelling efficiency such as to display a 20 rpm Brookfield viscosity of less than 900 cps when subjected to the standard gelling test herein, with the amount of the smectite in the composition not exceeding that which would raise the viscosity of the composition above 110 Krebs Units (KU).

    7.
    发明专利
    未知

    公开(公告)号:BR9807432A

    公开(公告)日:2000-03-21

    申请号:BR9807432

    申请日:1998-02-18

    Abstract: An improved process for preparing an aqueous clay slurry having superior gellation properties. The process involves the bead milling of the clay in an aqueous medium for a period of about 0.5 to 20 minutes at an energy input level of about 44 to 146 kilowatt-hours per metric ton of dry clay. The milling may carried out using any suitable horizontal or vertical sand mill or ball mill such as the "Morehouse Cowles Sandmill" or the "Polymill" containing a grinding medium such as zirconium silicate or zirconium oxide. The clay is preferably a smectite clay such as montmorillonite and is present in the slurry in the range of about 3 to 30 wt. %, based on the total weight of the slurry. The aqueous clay slurry is useful as a rheological additive in water-based coating formulations.

    METHOD FOR EXTENDING PIGMENTS
    8.
    发明专利

    公开(公告)号:CA2232824A1

    公开(公告)日:1997-04-03

    申请号:CA2232824

    申请日:1996-09-27

    Abstract: Unusually high loading levels of smectite minerals are found to provide excellent pigment spacing in aqueous-based coatings, as will enable desired improved hiding, thereby extending the pigment. The level of smectite used in accordance with the invention is sufficiently high that the high gelling efficiency smectites previously used as thixotropes would be inappropriate, and would yield viscosities so high as to render the aqueous coating composition lacking in desired flowability properties. Thus in accordance with the present invention, there is mixed with the aqueous carrier and pigment at least 0.5 % by weight of the total composition, of a particulate water swellable smectite which has a gelling efficiency such as to display a 20 rpm Brookfield viscosity of less than 900 cps when subjected to the standard gelling test herein, with the amount of the smectite in the composition not exceeding that which would raise the viscosity of the composition above 110 Krebs Units (KU).