MASTERBATCH COMPOSITION
    1.
    发明申请

    公开(公告)号:WO2018117271A1

    公开(公告)日:2018-06-28

    申请号:PCT/JP2017/046271

    申请日:2017-12-18

    Abstract: A masterbatch composition is provided which provides a polypropylene resin composition having good surface appearance and excellent fluidity. A masterbatch composition containing: 65 to 85 wt% of a propylene (co) polymer as component (1) containing 0 to 3 wt% of ethylene or one or more C4-C10-α-olefin-derived units; and 15 to 35 wt% of a propylene-ethylene copolymer as component (2) containing 25 to 35 wt% of ethylene-derived units, wherein the masterbatch composition satisfies the following requirements: 1) the composition has a melt flow rate (230°C, load: 21.18 N) of 5 to 30 g/10 minutes; 2) xylene insolubles of the composition have an Mw of 10 x 10 4 to 30 x 10 4 and an Mw/Mn of 6 to 20 as measured by GPC; and 3) xylene solubles of the composition have an intrinsic viscosity of 5.5 to 9.0 dl/g.

    POLYPROPYLENE COMPOSITIONS
    2.
    发明申请
    POLYPROPYLENE COMPOSITIONS 审中-公开
    聚丙烯组合物

    公开(公告)号:WO2016000910A1

    公开(公告)日:2016-01-07

    申请号:PCT/EP2015/062713

    申请日:2015-06-08

    Abstract: The invention relates to a heterophasic polypropylene compositions comprising 68-76 % by weight of a propylene homopolymer or copolymer matrix, 24-32 % by weight of an ethylene-propylene copolymer and a nucleating agent. The composition has an intrinsic viscosity of the xylene soluble fraction at room temperature up to 1.3 dl/g and a melt flow rate (230 °C, 2.16 kg) of 30 to 70 g/10 min. The compositions disclosed herein can be used to prepare molded articles, particularly by thin wall injection molding, that are endowed with excellent impact behaviour.

    Abstract translation: 本发明涉及包含68-76重量%的丙烯均聚物或共聚物基质,24-32重量%的乙烯 - 丙烯共聚物和成核剂的多相聚丙烯组合物。 该组合物在室温下的二甲苯可溶级分的特性粘度高达1.3dl / g,熔体流动速率(230℃,2.16kg)为30-70g / 10min。 本文公开的组合物可用于制备具有优异冲击性能的模制品,特别是通过薄壁注射成型。

    POLYPROPYLENE COMPOSITION AND MOLDED ARTICLE

    公开(公告)号:WO2019245058A1

    公开(公告)日:2019-12-26

    申请号:PCT/JP2019/025266

    申请日:2019-06-19

    Abstract: Provided is a polypropylene composition having an excellent balance between stiffness and low temperature impact resistance as well as having high flowability and gloss. A polypropylene composition comprising: as component (1), a propylene (co)polymer containing 0 to 0.5% by weight of an ethylene-derived unit; as component (2), an ethylene/propylene copolymer containing 15 to 30% by weight of an ethylene-derived unit; and 0.01 to 1.0 parts by weight of a crystal nucleating agent based on a total of 100 parts by weight of component (1) and component (2); wherein the polypropylene composition satisfies the following requirements: 1) the Mw/Mn value of xylene insolubles (XI) of the composition as measured by GPC is in the range of 6 to 20, 2) the weight ratio of component (1) to component (2) is in the range of 82:18 to 90:10, 3) the intrinsic viscosity of xylene solubles (XSIV) of the composition is in the range of 2.5 to 3.4 dl/g, 4) the MFR (at 230°C under a load of 2.16 kg) of the composition is in the range of 3 to 10 g/10 min.

    POLYPROPYLENE COMPOSITION AND MOLDED ARTICLE

    公开(公告)号:WO2020080555A1

    公开(公告)日:2020-04-23

    申请号:PCT/JP2019/041813

    申请日:2019-10-17

    Abstract: Provided is a polypropylene composition that is capable of giving an injection- molded article having high gloss and excellent balance between stiffness and low temperature impact resistance by maintaining flowability. A polypropylene composition comprising: as component (1), a propylene (co)polymer containing 0 to 0.5% by weight of an ethylene-derived unit; and as component (2), an ethylene/propylene copolymer containing 65 to 85% by weight of an ethylene-derived unit; wherein the polypropylene composition satisfies the following requirements: 1) the Mw/Mn value of xylene insolubles (XI) of the composition as measured by GPC is in the range of 6 to 20, 2) the weight ratio of component (1) to component (2) is in the range of 70:30 to 85:15, 3) the intrinsic viscosity of xylene solubles (XSIV) of the composition is in the range of 1.0to 3.0 dl/g, 4) the MFR (at 230°C under a load of 2.16 kg) of the composition is in the range of 3 to 15 g/10 min.

    POLYPROPYLENE COMPOSITION AND MOLDED ARTICLE

    公开(公告)号:WO2019177180A8

    公开(公告)日:2019-09-19

    申请号:PCT/JP2019/012288

    申请日:2019-03-15

    Abstract: The present invention provides a polypropylene composition having an excellent balance between transparency and flexibility. A polypropylene composition comprising: as component (1), a propylene/ethylene copolymer containing 2 to 4% by weight of an ethylene-derived unit; and as component (2), an ethylene/propylene copolymer containing 65 to 87% by weight of an ethylene-derived unit; wherein the polypropylene composition satisfies the following requirements: 1) the weight ratio of component (1) to component (2) is in the range of 65:35 to 77:23, 2) the intrinsic viscosity of xylene solubles (XSIV) of the composition is in the range of 0.8 to 1.4 dl/g, 3) the MFR (at 230°C under a load of 2.16 kg) of the composition is in the range of 15 to 40 g/10 min., 4) no crystal nucleating agent is contained.