公开(公告)号:KR20200139129A
公开(公告)日:2020-12-11
申请号:KR20207018846
申请日:2019-01-25
Applicant: TORAY INDUSTRIES
Inventor: KOGAWA TAISUKE , FUJITA MASAKI , KOYAMATSU YUICHI , TANAHASHI KAZUHIRO , KIDOBA KAZUYUKI
Abstract: 본발명은높은추종성과우수한분해성을구비한생분해성을갖는블록공중합체를제공하는것을목적으로하고있다. 본발명은폴리알킬렌글리콜블록과, 폴리히드록시알칸산블록으로이루어지며, 전체질량에대한폴리알킬렌글리콜블록의질량비율이 10~60%이며, 카르보닐탄소의탄소핵완화시간 T1ρ가 20ms 이하이며, 하기식 1을충족하는블록공중합체를제공한다. χ=χ1×χ2≥20 …식 1 χ1: 폴리알킬렌글리콜블록의결정화율χ2: 폴리히드록시알칸산블록에포함되는반복단위중 단일의반복단위로이루어지는호모폴리머의결정화율이가장높은반복단위를 A라고했을때의폴리 A 블록의결정화율
-
公开(公告)号:CA3039448A1
公开(公告)日:2018-04-12
申请号:CA3039448
申请日:2017-09-29
Applicant: TORAY INDUSTRIES
Inventor: TANAKA NOBUAKI , TSUCHIKURA HIROSHI , YAMADA SATOSHI , KOYAMATSU YUICHI , KOGAWA TAISUKE , SAKAGUCHI YUKA , TANAHASHI KAZUHIRO
Abstract: The present invention relates to a tubular fabric useful for hoses used to transfer fluid and powder and protect wire-like materials such as wires, cables, and electric wire tubing, tubular filters, base materials for artificial blood vessels, and the like. Provided is a tubular fabric that is woven by interlacing warp yarn and weft yarn and has a difference in outer diameter of 10% or less in the warp direction of the tubular fabric, wherein the following formula is satisfied: (L2 - L1)/L1 = 0.1 wherein L1 is a distance between marked lines when compressive stress of 0.01 cN/dtex is applied in the warp direction of the tubular fabric with the marked lines drawn on the outer circumference of the tubular fabric at a distance five times the maximum value for the fabric outer diameter measured in a state where stress is not applied to the tubular fabric, and L2 is the distance between the marked lines during elongation at a stress of 0.01 cN/dtex in the warp direction of the tubular fabric with the marked lines drawn on the outer circumference of the tubular fabric at a distance five times the maximum value for the fabric outer diameter measured in a state where stress is not applied to the tubular fabric.
-
公开(公告)号:CA3092567A1
公开(公告)日:2019-10-03
申请号:CA3092567
申请日:2019-01-25
Applicant: TORAY INDUSTRIES
Inventor: KOGAWA TAISUKE , FUJITA MASAKI , KOYAMATSU YUICHI , TANAHASHI KAZUHIRO , KIDOBA KAZUYUKI
Abstract: The purpose of the present invention is to provide a biodegradable block copolymer which combines high conformability with excellent degradability. The present invention provides a block copolymer which comprises a poly(alkylene glycol) block and a poly(hydroxyalkanoic acid) block, wherein the proportion by mass of the poly(alkylene glycol) block to the whole mass is 10-60%, the block copolymer having a carbon-nucleus relaxation time T1? regarding the carbonyl carbon atom of 20 ms or less and satisfying expression 1. ?=?1×?2=20 (expression 1) ?1 is the degree of crystallization of the poly(alkylene glycol) block. ?2 is the degree of crystallization of a poly-A block, where A is a repeating unit, among the repeating units contained in the poly(hydroxyalkanoic acid) block, that is the highest in the degree of crystallization of the homopolymer made up of the same repeating units alone.
-
公开(公告)号:AU2017340701A1
公开(公告)日:2019-04-04
申请号:AU2017340701
申请日:2017-09-29
Applicant: TORAY INDUSTRIES
Inventor: TANAKA NOBUAKI , TSUCHIKURA HIROSHI , YAMADA SATOSHI , KOYAMATSU YUICHI , KOGAWA TAISUKE , SAKAGUCHI YUKA , TANAHASHI KAZUHIRO
Abstract: The present invention relates to a tubular fabric useful for hoses used to transfer fluid and powder and protect wire-like materials such as wires, cables, and electric wire tubing, tubular filters, base materials for artificial blood vessels, and the like. Provided is a tubular fabric that is woven by interlacing warp yarn and weft yarn and has a difference in outer diameter of 10% or less in the warp direction of the tubular fabric, wherein the following formula is satisfied: (L2 − L1)/L1 ≥ 0.1 wherein L1 is a distance between marked lines when compressive stress of 0.01 cN/dtex is applied in the warp direction of the tubular fabric with the marked lines drawn on the outer circumference of the tubular fabric at a distance five times the maximum value for the fabric outer diameter measured in a state where stress is not applied to the tubular fabric, and L2 is the distance between the marked lines during elongation at a stress of 0.01 cN/dtex in the warp direction of the tubular fabric with the marked lines drawn on the outer circumference of the tubular fabric at a distance five times the maximum value for the fabric outer diameter measured in a state where stress is not applied to the tubular fabric.
-
公开(公告)号:EP2108698A4
公开(公告)日:2010-03-17
申请号:EP07851046
申请日:2007-12-21
Applicant: TORAY INDUSTRIES
Inventor: KOYAMATSU YUICHI , MICALLEF MARK , IDA NOBUO , KOIWA MASAKAZU , KAKIZAWA YOSHINORI
-
-
-
-