公开(公告)号:AU3405389A
公开(公告)日:1989-11-09
申请号:AU3405389
申请日:1989-05-04
Applicant: TORAY INDUSTRIES
Inventor: SHINDO TAKESHI , SANO MASUKI , OKA KEN-ICHIRO
Abstract: Disclosed is a polyethylene terephthalate untwisted multifilament which satisfies the following requirements (A), (B), (C) and (D); (A) the intrinsic viscosity [IV] is 0.97 to 1.15; (B) the amorphous orientation function [fa] is not larger than 0.55; (C) the tenacity [T] (g/d), the shrinkage [ DELTA S] (%) as measured after standing in dry air at 150 DEG C for 30 minutes, the medium elongation [ME] (%) under a load of 4.5 g/d, and the dimensional stability index [Y] expressed by the formula: Y= ME + DELTA S + 1.32 are within ranges defined by the following formulae (a), (b), (c), (d) and (e): and and (d) the elongation at break is at least 11% and the product of the tenacity and elongation, which is defined by: [tenacity (g/d) at break] x 2ROOT elongation (%) at break, is 30 to 36.
-
公开(公告)号:CA1327685C
公开(公告)日:1994-03-15
申请号:CA598456
申请日:1989-05-02
Applicant: TORAY INDUSTRIES
Inventor: SHINDO TAKESHI , SANO MASUKI , OKA KEN-ICHIRO
Abstract: POLYESTER FIBER FOR INDUSTRIAL USE AND PROCESS FOR PREPARATION THEREOF Disclosed is a polyethylene terephthalate untwisted multifilament which satisfies the following requirements (A), (B), (C) and (D); (A) the intrinsic viscosity ¢IV! is 0.97 to 1.15; (B) the amorphous orientation function ¢fa! is not larger than 0.55; (C) the tenacity ¢T! (g/d), the shrinkage ¢.DELTA.S! (%) as measured after standing in dry air at 150.degree.C for 30 minutes, the medium elongation ¢ME! (%) under a load of 4.5 g/d, and the dimensional stability index ¢y! expressed by the formula: Y= ME0-81 + .DELTA.S + 1.32 are within ranges defined by the following formulae (a), (b), (c), (d) and (e): 0.33Y + 5.55 ? T ? 0.33Y + 6.50 (a), 8.0 ? T ? 9.5 (b), 8.5 ? Y ? 10.5 (c), 5 ? ME ? 10 (d), and 2 ? .DELTA.S ? 6 (e); and (d) the elongation at break is at least 11% and the product of the tenacity and elongation, which is defined by: , is 30 to 36.
-
公开(公告)号:AU629546B2
公开(公告)日:1992-10-08
申请号:AU3405389
申请日:1989-05-04
Applicant: TORAY INDUSTRIES
Inventor: SHINDO TAKESHI , SANO MASUKI , OKA KEN-ICHIRO
Abstract: Disclosed is a polyethylene terephthalate untwisted multifilament which satisfies the following requirements (A), (B), (C) and (D); (A) the intrinsic viscosity [IV] is 0.97 to 1.15; (B) the amorphous orientation function [fa] is not larger than 0.55; (C) the tenacity [T] (g/d), the shrinkage [ DELTA S] (%) as measured after standing in dry air at 150 DEG C for 30 minutes, the medium elongation [ME] (%) under a load of 4.5 g/d, and the dimensional stability index [Y] expressed by the formula: Y= ME + DELTA S + 1.32 are within ranges defined by the following formulae (a), (b), (c), (d) and (e): and and (d) the elongation at break is at least 11% and the product of the tenacity and elongation, which is defined by: [tenacity (g/d) at break] x 2ROOT elongation (%) at break, is 30 to 36.
-
公开(公告)号:ZA8903434B
公开(公告)日:1990-01-31
申请号:ZA8903434
申请日:1989-05-09
Applicant: TORAY INDUSTRIES
Inventor: SHINDO TAKESHI , TAKESHI SHINDO , SANO MASUKI , MASUKI SANO , OKA KEN-ICHIRO , KEN-ICHIRO OKA
CPC classification number: D01D5/084 , D01F6/62 , Y10S57/902 , Y10T428/2913 , Y10T428/2929 , Y10T428/2933 , Y10T428/2969
-
公开(公告)号:ZA893434B
公开(公告)日:1990-01-31
申请号:ZA893434
申请日:1989-05-09
Applicant: TORAY INDUSTRIES
Inventor: KEN-ICHIRO OKA , SHINDO TAKESHI , TAKESHI SHINDO , SANO MASUKI , MASUKI SANO , OKA KEN-ICHIRO
Abstract: Disclosed is a polyethylene terephthalate untwisted multifilament which satisfies the following requirements (A), (B), (C) and (D); (A) the intrinsic viscosity [IV] is 0.97 to 1.15; (B) the amorphous orientation function [fa] is not larger than 0.55; (C) the tenacity [T] (g/d), the shrinkage [ DELTA S] (%) as measured after standing in dry air at 150 DEG C for 30 minutes, the medium elongation [ME] (%) under a load of 4.5 g/d, and the dimensional stability index [Y] expressed by the formula: Y= ME + DELTA S + 1.32 are within ranges defined by the following formulae (a), (b), (c), (d) and (e): and and (d) the elongation at break is at least 11% and the product of the tenacity and elongation, which is defined by: [tenacity (g/d) at break] x 2ROOT elongation (%) at break, is 30 to 36.
-
公开(公告)号:DE2716106A1
公开(公告)日:1977-10-27
申请号:DE2716106
申请日:1977-04-12
Applicant: TORAY INDUSTRIES
Inventor: OTAKI YUKIO , OKA KEN-ICHIRO , KOIDE KAZUYOSHI , NAKAGAWA KIYOSHI
Abstract: This invention relates to a method and apparatus for imparting false twists to two yarns simultaneously. The significance of the invention resides in that an industrially utilizable method for false twisting yarns by frictional contact of two yarns with 4 rotating frictional discs has been provided. The apparatus of the present invention for practising the false twisting method is characterized in that the angle of contact of yarns with the frictional discs is maintained within a specific range and the frictional discs are attached to four shafts in specific order at specific heights. Various processes for preparing a variety of false twist yarns by utilizing the false twisting method and apparatus of the present invention have been established.
-
-
-
-
-