RUBBER-REINFORCING POLYESTER FIBER AND PROCESS FOR PREPARATION THEREOF

    公开(公告)号:AU6642690A

    公开(公告)日:1991-06-13

    申请号:AU6642690

    申请日:1990-11-15

    Abstract: PCT No. PCT/JP90/01491 Sec. 371 Date Sep. 13, 1991 Sec. 102(e) Date Sep. 13, 1991 PCT Filed Nov. 15, 1990 PCT Pub. No. WO91/07529 PCT Pub. Date May 30, 1991.A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T 2ROOT E) is at least (2S+5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.

    RUBBER-REINFORCING POLYESTER FIBER AND PROCESS FOR PREPARATION THEREOF

    公开(公告)号:CA2045134A1

    公开(公告)日:1991-05-16

    申请号:CA2045134

    申请日:1990-11-15

    Abstract: A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T~E) is at least (2S + 5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.

    5.
    发明专利
    未知

    公开(公告)号:DE3889282D1

    公开(公告)日:1994-06-01

    申请号:DE3889282

    申请日:1988-10-06

    Abstract: A conjugated fiber having a sheath-core conjugated structure comprising a polyester core component composed mainly of polyethylene terephthalate and a polyamide sheath component composed mainly of polyhexamethylene adipamide, is disclosed, which has excellent mechanical properties such as a high tenacity, a high modulus, and an improved dimensional stability, and an improved adhesion to a rubber, especially a high-temperature adhesion, an improved heat resistance in a rubber, and a high fatigue resistance, and thus is useful as an industrial material. By adopting a high-speed spinning procedure in the fiber preparing process, the peel resistance in the interface of the sheath-core conjugated structure is greatly improved, and the following valuable characteristics not possessed by conventional conjugated yarns can be obtained: (1) Excellent adhesion and high-temperature adhesion comparable to those of a polyamide, which cannot be obtained in a polyester. (2) High modulus and dimensional stability comparable to those of a polyester, which cannot be obtained in a polyamide. (3) A heat resistance in a rubber and a fatigue resistance superior to those of a polyester. p

    RUBBER-REINFORCING POLYESTER FIBER AND PROCESS FOR PREPARATION THEREOF

    公开(公告)号:CA2045134C

    公开(公告)日:1999-03-16

    申请号:CA2045134

    申请日:1990-11-15

    Abstract: A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T~E) is at least (2S + 5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.

    7.
    发明专利
    未知

    公开(公告)号:DE69028693D1

    公开(公告)日:1996-10-31

    申请号:DE69028693

    申请日:1990-11-15

    Abstract: PCT No. PCT/JP90/01491 Sec. 371 Date Sep. 13, 1991 Sec. 102(e) Date Sep. 13, 1991 PCT Filed Nov. 15, 1990 PCT Pub. No. WO91/07529 PCT Pub. Date May 30, 1991.A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T 2ROOT E) is at least (2S+5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.

    HIGH-TENACITY CONJUGATED FIBER AND PROCESS FOR PREPARATION THEREOF

    公开(公告)号:CA1314673C

    公开(公告)日:1993-03-23

    申请号:CA579481

    申请日:1988-10-06

    Abstract: HIGH-TENACITY CONJUGATED FIBER AND PROCESS FOR PREPARATION THEREOF A conjugated fiber having a sheath-core conjugated structure-comprising a polyester core component composed mainly of polyethylene terephthalate and a polyamide sheath component composed mainly of polyhexamethylene adipamide, is disclosed, which has excellent mechanical properties such as a high tenacity, a high modulus, and an improved dimensional stability, and an improved adhesion to a rubber, especially a high-temperature adhesion, an improved heat resistance in a rubber, and a high fatigue resistance, and thus is useful as an industrial material. By adopting a high-speed spinning procedure in the fiber preparing process, the peel resistance in the interface of the sheath-core conjugated structure is greatly improved, and the following valuable characteristics not possessed by conventional conjugated yarns can be obtained: (1) Excellent adhesion and high-temperature adhesion comparable to those of a polyamide, which cannot be obtained in a polyester. (2) High modulus and dimensional stability comparable to those of a polyester, which cannot be obtained in a polyamide. (3) A heat resistance in a rubber and a fatigue resistance superior to those of a polyester.

    HIGH-TENACITY CONJUGATED FIBRE
    10.
    发明专利

    公开(公告)号:AU606462B2

    公开(公告)日:1991-02-07

    申请号:AU2343588

    申请日:1988-10-05

    Abstract: A conjugated fiber having a sheath-core conjugated structure comprising a polyester core component composed mainly of polyethylene terephthalate and a polyamide sheath component composed mainly of polyhexamethylene adipamide, is disclosed, which has excellent mechanical properties such as a high tenacity, a high modulus, and an improved dimensional stability, and an improved adhesion to a rubber, especially a high-temperature adhesion, an improved heat resistance in a rubber, and a high fatigue resistance, and thus is useful as an industrial material. By adopting a high-speed spinning procedure in the fiber preparing process, the peel resistance in the interface of the sheath-core conjugated structure is greatly improved, and the following valuable characteristics not possessed by conventional conjugated yarns can be obtained: (1) Excellent adhesion and high-temperature adhesion comparable to those of a polyamide, which cannot be obtained in a polyester. (2) High modulus and dimensional stability comparable to those of a polyester, which cannot be obtained in a polyamide. (3) A heat resistance in a rubber and a fatigue resistance superior to those of a polyester. p