公开(公告)号:DE69627229D1
公开(公告)日:2003-05-15
申请号:DE69627229
申请日:1996-01-25
Applicant: TORAY INDUSTRIES
Inventor: MATSUMURA YOSHITAKA , HARASHINA YUKO , HIGUCHI TETSUNORI , SASAMOTO TAI
IPC: C08G63/668 , D01F6/86 , D01F8/14
Abstract: A hygroscopic polyester copolymer contains copolymerized units derived from (1) a hydrophilic compound and (2) a cross-linking agent and has a release parameter DELTA MR of at least 12% so as to be controlled in its moisture absorbing and releasing property. Fibers containing the polyester copolymer may be formed and these may be utilized in materials for underwear, sports wear, interlinings, etc. as highly hygroscopic woven and knitted fabrics, etc.
-
公开(公告)号:AT356847T
公开(公告)日:2007-04-15
申请号:AT02001273
申请日:2002-01-17
Applicant: TORAY INDUSTRIES
Inventor: OHKURA MASATOSHI , SASAMOTO TAI , SHINNUMADATE HIROSHI
IPC: B65D65/40 , B29C55/02 , B32B27/22 , B65D65/46 , C08J3/18 , C08J7/04 , C08K5/00 , C08L67/04 , C08L101/16 , C08J5/18
Abstract: Disclosed is a biodegradable oriented film of a plasticizer-containing biodegradable resin, of which the both surfaces are coated with at least one thin layer and of which the loop stiffness change ( DELTA R) after heat treatment at 130 DEG C for 30 minutes is at most 20 %. This is favorable for wrapping films.
-
公开(公告)号:DE69627229T2
公开(公告)日:2004-02-05
申请号:DE69627229
申请日:1996-01-25
Applicant: TORAY INDUSTRIES
Inventor: MATSUMURA YOSHITAKA , HARASHINA YUKO , HIGUCHI TETSUNORI , SASAMOTO TAI
IPC: C08G63/668 , D01F6/86 , D01F8/14
Abstract: A hygroscopic polyester copolymer contains copolymerized units derived from (1) a hydrophilic compound and (2) a cross-linking agent and has a release parameter DELTA MR of at least 12% so as to be controlled in its moisture absorbing and releasing property. Fibers containing the polyester copolymer may be formed and these may be utilized in materials for underwear, sports wear, interlinings, etc. as highly hygroscopic woven and knitted fabrics, etc.
-
公开(公告)号:DE69028693T2
公开(公告)日:1997-02-20
申请号:DE69028693
申请日:1990-11-15
Applicant: TORAY INDUSTRIES
Inventor: SASAMOTO TAI , MIYOSHI TAKEHIKO , SATO TAKUJI
Abstract: PCT No. PCT/JP90/01491 Sec. 371 Date Sep. 13, 1991 Sec. 102(e) Date Sep. 13, 1991 PCT Filed Nov. 15, 1990 PCT Pub. No. WO91/07529 PCT Pub. Date May 30, 1991.A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T 2ROOT E) is at least (2S+5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.
-
公开(公告)号:ZA909179B
公开(公告)日:1991-09-25
申请号:ZA909179
申请日:1990-11-15
Applicant: TORAY INDUSTRIES
Inventor: SASAMOTO TAI , TAI SASAMOTO , MIYOSHI TAKEHIKO , TAKEHIKO MIYOSHI , SATO TAKUJI , TAKUJI SATO
IPC: C08G63/183 , C08G63/181 , C08G63/86 , D01F20060101 , D01F6/62 , D01F
-
公开(公告)号:DE60218764D1
公开(公告)日:2007-04-26
申请号:DE60218764
申请日:2002-01-17
Applicant: TORAY INDUSTRIES
Inventor: OHKURA MASATOSHI , SASAMOTO TAI , SHINNUMADATE HIROSHI
IPC: B65D65/40 , C08J5/18 , B29C55/02 , B32B27/22 , B65D65/46 , C08J3/18 , C08J7/04 , C08K5/00 , C08L67/04 , C08L101/16
Abstract: Disclosed is a biodegradable oriented film of a plasticizer-containing biodegradable resin, of which the both surfaces are coated with at least one thin layer and of which the loop stiffness change ( DELTA R) after heat treatment at 130 DEG C for 30 minutes is at most 20 %. This is favorable for wrapping films.
-
公开(公告)号:DE60015935T2
公开(公告)日:2005-12-01
申请号:DE60015935
申请日:2000-08-02
Applicant: TORAY INDUSTRIES
Inventor: MORIMOTO TSUTOMU , TSUZUKI TOSHIHIRO , SASAMOTO TAI
-
公开(公告)号:CA2426662A1
公开(公告)日:2003-04-22
申请号:CA2426662
申请日:2002-05-08
Applicant: TORAY INDUSTRIES
Inventor: TANAKA SHIGERU , SASAMOTO TAI , OHKURA MASATOSHI , MASUDA JUN ICHI
Abstract: A biaxially oriented polypropylene film exhibiting a high rigidity in the machine direction can be produced according to a general lengthwise-widthwis e sequential biaxial stretching process either by specifying the additive contained in the film, the melt-tensile strength (MS) and melt flow rate (MF R) of the polypropylene as determined at 230 ~C, or the Trouton ratio of the polypropylene or by making specified longitudinal fibrils present in the fil m.
-
公开(公告)号:CA2167989A1
公开(公告)日:1996-07-26
申请号:CA2167989
申请日:1996-01-24
Applicant: TORAY INDUSTRIES
Inventor: MATSUMURA YOSHITAKA , HARASHINA YUKO , HIGUCHI TETSUNORI , SASAMOTO TAI
IPC: C08G63/668 , D01F6/86 , D01F8/14 , D02G3/04 , C08G63/91
Abstract: Disclosed are a hygroscopic polyester copolymer containing a hydrophilic compound copolymerized and a crosslinking agent and having controlled moisture absorbing and releasing property, and a fiber produced using the polyester copolymer. The fiber can be used as a comfortable material for underwear, sports wear, interlinings, etc. as highly hygroscopic woven and knitted fabrics, etc. of high quality.
-
公开(公告)号:AU6642690A
公开(公告)日:1991-06-13
申请号:AU6642690
申请日:1990-11-15
Applicant: TORAY INDUSTRIES
Inventor: SASAMOTO TAI , MIYOSHI TAKEHIKO , SATO TAKUJI
Abstract: PCT No. PCT/JP90/01491 Sec. 371 Date Sep. 13, 1991 Sec. 102(e) Date Sep. 13, 1991 PCT Filed Nov. 15, 1990 PCT Pub. No. WO91/07529 PCT Pub. Date May 30, 1991.A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T 2ROOT E) is at least (2S+5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.
-
-
-
-
-
-
-
-
-