A METHOD FOR CONTINUOUSLY PRODUCING A CYCLIC FORMAL

    公开(公告)号:MY120444A

    公开(公告)日:2005-10-31

    申请号:MYPI9800379

    申请日:1998-01-27

    Abstract: CYCLIC FORMAL IS MANUFACTURED BY CYCLIC REACTION OF AN ALKYLENE GLYCOL AND AN ALDEHYDE IN A REACTOR, PRODUCING FORMAL MIXED WITH UNREACTED ALDEHYDE AS AN IMPURITY, WHICH IS REDUCED IN AMOUNT BY CONNECTING THE REACTOR TO A DISTILLATION TOWER AND CONTINUOUSLY SUPPLYING A RAW ALKYLENE GLYCOL TO THE DISTILLATION TOWER FROM WHICH UNREACTED FORMALDEHYDE AND A CYCLIC FORMAL ARE BEING DISTILLED, AND CONTINUOUSLY REACTING THEM WITH SUPPLIED RAW FORMALDEHYDE BY COUNTERCURRENT FLOW DURING DISTILLATION. WATER CONTENT IS AZEOTROPIC ADMIXTURE WITH CYCLIC FORMAL CAN BE REMOVED BY AZEOTROPIC DISTILLATION WITH A HYDROCARBON AZEOTROPIC ADMIXTURE WITH WATER, DISTILLING WATER FROM THE CYCLIC FORMAL.

    POLYOXYMETHYLENE MULTI-COPOLYMER AND ITS RESIN COMPOSITION

    公开(公告)号:CA2022837C

    公开(公告)日:2001-12-04

    申请号:CA2022837

    申请日:1990-08-08

    Abstract: A polyoxymethylene multi-copolymer obtainable by copolymerizing (a) trioxane, (b) at least one cyclic ether or formal compound chosen from the group of ethylene oxide, 1,3-dioxolane, 1,3-dioxepane, 1,3,5-trioxepane and 1,3,6-trioxocane, and (c) at least one compound chosen from the group of glycidyl phenyl ether, styrene oxide and glycidyl naphthyl ether, and characterized in that the number average molecular weight of said polyoxymethylene multi-copolymer is from 10,000 to 100,000, that the melting point (Tm) and crystallization temperature (Tc) there of are in a relationship of Tm - Tc

    4.
    发明专利
    未知

    公开(公告)号:DE3750887D1

    公开(公告)日:1995-02-02

    申请号:DE3750887

    申请日:1987-04-30

    Abstract: A process for producing an oxymethylene copolymer comprises the steps of polymerizing trioxane and cyclic ether in the presence of a boron trifluoride catalyst, adding a hindered amine compound to the polymer obtained by said polymerization, and stabilizing unstable chain ends of the polymer. The oxymethylene copolymer thus obtained provides excellent heat resistance and superior mechanical properties.

    6.
    发明专利
    未知

    公开(公告)号:DE69029078T2

    公开(公告)日:1997-04-03

    申请号:DE69029078

    申请日:1990-05-17

    Abstract: An elastic polyester is continuously produced by continuously feeding an aromatic polyester and a lactone to an extruder (6), which is provided with a cylinder having an aspect ratio (L/D) ranging from 3 to 50 (wherein L represents the cylinder length of a reactor and D the inner diameter of the cylinder) and at least one screw and wherein the space in the cylinder provided with the screw accounts for 70 % or less of the internal volume of the cylinder, and reacting the lactone with the aromatic polyester while conducting the melting, carrying and kneading of the feed material in the extruder (6). Since the screw can be turned with a high speed, the effect of kneading can be enhanced and the reaction time can be shortened. Since the obtained elastic polyester is excellent in durability represented by thermal and weathering resistances, rubber elasticity, and mechanical properties, it has a wide range of uses such as automotive parts, electric and electronics components and machine parts.

    7.
    发明专利
    未知

    公开(公告)号:DE69023571D1

    公开(公告)日:1995-12-21

    申请号:DE69023571

    申请日:1990-08-07

    Abstract: A polyoxymethylene multi-copolymer having spherulites and obtainable by copolymerizing (a) trioxane, (b) at least one cyclic ether or formal compound chosen from ethylene oxide, 1,3-dioxolane, 1,3-dioxepane, 1,3,5-trioxepane and 1,3,6-trioxocane, and (c) at least one compound chosen from glycidyl phenyl ether, styrene oxide and glycidyl naphthyl ether, is characterised in that the number average molecular weight of said polyoxymethylene multi-copolymer is from 10,000 to 100,000, that the melting point (Tm) and crystallization temperature (Tc) thereof are governed by the relationship, Tm - Tc

    PROCESS FOR CONTINUOUS PRODUCTION OF ELASTIC POLYESTERS

    公开(公告)号:CA2033095A1

    公开(公告)日:1990-11-18

    申请号:CA2033095

    申请日:1990-05-17

    Abstract: An elastic polyester is continuously produced by continuously feeding an aromatic polyester and a lactone to an extruder (6), which is provided with a cylinder having an aspect ratio (L/D) ranging from 3 to 50 (wherein L represents the cylinder length of a reactor and D the inner diameter of the cylinder) and at least one screw and wherein the space in the cylinder provided with the screw accounts for 70 % or less of the internal volume of the cylinder, and reacting the lactone with the aromatic polyester while conducting the melting, carrying and kneading of the feed material in the extruder (6). Since the screw can be turned with a high speed, the effect of kneading can be enhanced and the reaction time can be shortened. Since the obtained elastic polyester is excellent in durability represented by thermal and weathering resistances, rubber elasticity, and mechanical properties, it has a wide range of uses such as automotive parts, electric and electronics components and machine parts.

    9.
    发明专利
    未知

    公开(公告)号:DE60115342D1

    公开(公告)日:2006-01-05

    申请号:DE60115342

    申请日:2001-07-24

    Abstract: A rubber-reinforced styrene transparent resin composition contains a styrene copolymer reinforced with a rubber polymer, wherein the monomer composition of an acetone soluble resin component contained in the resin composition contains 5 to 70% by weight of aromatic vinyl monomer (a1), 30 to 95% by weight of unsaturated carboxylic acid alkyl ester monomer (a2), 0 to 50% by weight of vinyl cyanide monomer (a3), and 0 to 50% by weight of another monomer copolymerizable with these monomers, and the acid value of the acetone soluble resin component is 0.01 to 1 mgKOH/g.

    10.
    发明专利
    未知

    公开(公告)号:DE69807135D1

    公开(公告)日:2002-09-19

    申请号:DE69807135

    申请日:1998-01-29

    Abstract: Cyclic formal is manufactured by cyclic reaction of an alkylene glycol and an aldehyde in a reactor, producing formal mixed with unreacted aldehyde as an impurity, which is reduced in amount by connecting the reactor to a distillation tower and continuously supplying a raw alkylene glycol to the distillation tower from which unreacted formaldehyde and a cyclic formal are being distilled, and continuously reacting them with supplied raw formaldehyde by countercurrent flow during distillation. Water content in azeotropic admixture with cyclic formal can be removed by azeotropic distillation with a hydrocarbon azeotropic admixture with water, distilling water from the cyclic formal.