Abstract:
A gas phase polymerization process comprising: (1) preparing a solution of a catalyst precursor comprising a mixture of magnesium and titanium compounds, an electron donor and a solvent; (2) adding a filler to the solution from step (1) to form a slurry; (3) spray drying the slurry from step (2) at a temperature of 100 to 140 °C to form a spray dried precursor; (4) slurring the spray dried precursor from step (3) in mineral oil, (5) partially or fully pre-activating the catalyst precursor by contacting the slurry of (4) with one or more Lewis Acids, and (6) transferring the partially or fully activated precursor from step (5) into a gas phase reactor in which an olefin polymerization reaction is in progress.
Abstract:
A Ziegler-Natta procatalyst composition in the form of solid particles and comprising magnesium, halide and transition metal moieties, said particles having an average size (D50) of from 10 to 70 μm, characterized in that at least 5 percent of the particles have internal void volume substantially or fully enclosed by a monolithic surface layer (shell), said layer being characterized by an average shell thickness/particle size ratio (Thickness Ratio) determined by SEM techniques for particles having particle size greater than 30 μm of greater than 0.2.
Abstract:
Se describe una composicion de procatalizador de ZieglerNatta en forma de Particulas Solidas y que comprende fracciones de magnesio, haluro y metal de transicion, tales particulas tienen un tamano promedio (D50) de 10 a 70 mum, caracterizada por un indice de tamano de particula D95/D5 menor de o igual a 10.
Abstract:
Se describe una composicion de procatalizador de Ziegler-Natta en la forma de particulas solidas y que comprende magnesio, haluro y porciones de metales de transicion, tales particulas tienen un tamano promedio (D50) desde 10 hasta 70 ?m, caracterizada porque al menos 5 por ciento de las particulas tienen volumen hueco interno sustancial o completamente encerrado por una capa de superficie monolitica (coraza), caracterizandose la capa por una proporcion de espesor de coraza/tamano de particula promedio (Proporcion de espesor) determinada mediante tecnicas de SEM para particulas con un tamano de `particula mayor que 30 ?m de mas de 0.2.
Abstract:
A Ziegler-Natta procatalyst composition in the form of solid particles and comprising magnesium, halide and transition metal moieties, said particles having an average size (D50) of from 10 to 70 μm, characterized in that at least 5 percent of the particles have internal void volume substantially or fully enclosed by a monolithic surface layer (shell), said layer being characterized by an average shell thickness/particle size ratio (Thickness Ratio) determined by SEM techniques for particles having particle size greater than 30 μm of greater than 0.2.
Abstract:
Un método para la producción de una composición de procatalizador Ziegler-Natta en forma de partículas sólidas y que comprende fracciones de magnesio, haluro y metales de transición, teniendo dichas partículas un tamaño medio (D50) de entre 10 y 70 μm, y que comprende al menos un 5 por ciento de partículas que tienen un volumen interno hueco, sustancial o completamente encerrado por una capa superficial monolítica (recubrimiento), teniendo dicha capa una relación media grosor de recubrimiento / tamaño de partícula (relación de grosor), determinada por medio de técnicas de micrografía electrónica de barrido (SEM) para partículas que tienen un tamaño de partícula mayor que 30 μm, de más de 0,2, comprendiendo las etapas del método: a) proporcionar una composición líquida que comprenda i) un compuesto de haluro de magnesio, ii) un disolvente o diluyente, iii) un compuesto de metal de transición, en el que el compuesto de metal de transición es un haluro de titanio o un haloalcoholato de titanio que tiene de 1 a 8 átomos de carbono por cada grupo alcoholato, iv) opcionalmente un donador de electrones interno, y v) opcionalmente además un elemento de relleno; b) secar por pulverización la composición para formar una partícula secada por pulverización; y c) recoger las partículas sólidas resultantes, caracterizado por que la concentración del compuesto de haluro de magnesio está presente en una cantidad que es al menos el 90 por ciento de la concentración de saturación en el disolvente o diluyente.
Abstract:
A Ziegler-Natta procatalyst composition in the form of solid particles and comprising magnesium, halide and transition metal moieties, said particles having an average size (D50) of from 10 to 70 µm, characterized in that at least 5 percent of the particles have internal void volume substantially or fully enclosed by a monolithic surface layer (shell), said layer being characterized by an average shell thickness/ particle size ratio (Thickness Ratio) determined by SEM techniques for particles having particle size greater than 30 µm of greater than 0.2.