Abstract:
Provided are a polyamide-based film having superior thickness uniformity as well as comparatively little variation in properties in four directions formed of the 0 degree direction, 45 degree direction, 90 degree direction and 135 degree direction, and a method for producing the same. The present invention relates to a polyamide-based film, wherein (1) the difference between the maximum value and minimum value of the respective stress at 5% elongation as determined by a uniaxial tensile test is 35 MPa or less in four directions formed of a specific direction from an arbitrary point in the film that is designated as 0 degrees and directions at 45 degrees, 90 degrees and 135 degrees relative to the specific direction in the clockwise direction, and (2) the difference between the maximum value and the minimum value of the respective stress at 15% elongation as determined by the uniaxial tensile test in the four directions is 40 MPa or less.
Abstract:
Disclosed is an adhesive for packaging materials being in a form of an aqueous dispersion including an acid-modified polyolefin resin containing a (meth)acrylic acid ester component, polyvinyl alcohol and an aqueous medium, wherein the content of polyvinyl alcohol is 0.1 to 10 parts by mass in relation to 100 parts by mass of the acid-modified polyolefin resin. Also disclosed is a packaging material using the adhesive wherein a barrier layer, an adhesive layer formed of a coating film obtained from the adhesive, and a sealant layer are laminated in this order.
Abstract:
The present invention provides a mold release film including a resin layer provided on one surface of a polyester film, wherein the resin layer includes 100 parts by mass of a polypropylene-based modified polyolefin resin with the proportion of a modifying component of 1 to 10% by mass and 1 to 50 parts by mass of a cross-linking agent; the peel strength between the resin layer and a pressure-sensitive adhesive measured by bonding a rubber-based pressure-sensitive adhesive to the resin layer exceeds 3.0 N/cm; and the residual adhesion rate of a pressure-sensitive adhesive after bonding an acrylic pressure-sensitive adhesive to the resin layer is 80% or more.
Abstract:
Disclosed is an aqueous polyolefin resin dispersion including a polyolefin resin and an aqueous medium, wherein the polyolefin resin includes an olefin component and an unsaturated carboxylic acid component as copolymer components; the olefin component includes propylene (A) and an olefin(s) (B) other than propylene; the mass ratio (A/B) between the propylene (A) and the olefin(s) (B) other than propylene is 60/40 to 95/5; the content of the unsaturated carboxylic acid component as the copolymer component is 1 part by mass or more in relation to 100 parts by mass of the total mass of (A) and (B); and the content of the unsaturated carboxylic acid monomer in the dry residue of the aqueous dispersion is 10,000 ppm or less.
Abstract:
The present invention provides fibrous copper microparticles suppressed in the occurrence of irregularities on the surface thereof and the aggregates of the fibrous copper microparticles having an average crystallite diameter controlled so as to fall within a specific range. In the fibrous copper microparticles of the present invention, the number of fibrous copper microparticles each including one or more irregularities each having a dimensional difference of 0.02 μm or more, in a range of 1 μm in the lengthwise direction of a fibrous body, between the maximum diameter portion of the fibrous body and the minimum diameter portion of the fibrous body falling in a diameter dimension range of 0.01 to 0.5 μm, and each having a length of 1 μm or more is 10 or less per 100 of the fibrous copper microparticles.
Abstract:
Disclosed is a semiaromatic polyamide resin composition including a semiaromatic polyamide (A), a phosphorus-based flame retardant (B) and an inorganic aluminum compound (C), wherein the mass ratio (A/B) between (A) and (B) is 50/50 to 95/5; the amount of the inorganic aluminum compound (C) is 0.1 to 20 parts by mass in relation to 100 parts by mass of the total amount of (A) and (B); (A) is constituted with an aromatic dicarboxylic acid component, an aliphatic diamine component and a monocarboxylic acid component; and the content of the monocarboxylic acid component is 0.3 to 4.0 mol % in relation to the whole monomer components constituting (A).
Abstract:
The present invention provides a mold release film including a resin layer provided on one surface of a polyester film, wherein the resin layer includes 100 parts by mass of a polypropylene-based modified polyolefin resin with the proportion of a modifying component of 1 to 10% by mass and 1 to 50 parts by mass of a cross-linking agent; the peel strength between the resin layer and a pressure-sensitive adhesive measured by bonding a rubber-based pressure-sensitive adhesive to the resin layer exceeds 3.0 N/cm; and the residual adhesion rate of a pressure-sensitive adhesive after bonding an acrylic pressure-sensitive adhesive to the resin layer is 80% or more.
Abstract:
The polylactic acid resin composition of the present invention includes a polylactic acid resin (A) having a D-isomer content of 0 to 2.0 mol % or 98.0 to 100 mol %. The polylactic acid resin composition of the present invention further includes tin oxide (B) in an amount of 0.005 to 10 parts by mass in relation to 100 parts by mass of the polylactic acid resin (A). By using the polylactic acid resin composition of the present invention, a molded body being excellent in crystallinity and heat resistance, and at the same time, having sufficiently excellent moisture-heat durability can be obtained.
Abstract:
The present invention provides a mold release film including a resin layer provided on one surface of a polyester film, wherein the resin layer includes an acid-modified polyolefin resin with a proportion of an acid-modifying component of 1 to 10% by mass, polyvinyl alcohol and a cross-linking agent; the content of polyvinyl alcohol exceeds 200 parts by mass and is 1000 parts by mass or less, and the content of the cross-linking agent is 1 to 20 parts by mass in relation to 100 parts by mass of the acid-modified polyolefin resin; and the peel force between the resin layer and a rubber-based adherend measured by bonding the rubber-based adherend to the resin layer is 0.5 N/cm or less.
Abstract:
The polyarylate resin of the present invention includes a bisphenol residue represented by the general formula (1) and an aromatic dicarboxylic acid residue represented by the general formula (2). In formula (1), R1 and R2 each independently represent a hydrocarbon group having 1 to 6 carbon atoms, a halogenated alkyl group or a halogen atom, p and q each independently represent an integer of 0 to 4, and X represents a fluorine atom-containing divalent group. In formula (2), R3 and R4 each independently represent a hydrocarbon group having 1 to 6 carbon atoms, a halogenated alkyl group or a halogen atom, and r and s each independently represent an integer of 0 to 4.